摘要:
Moldable-foam moldings whose density is in the range from 10 to 100 g/l, obtainable via the fusion of prefoamed foam beads composed of expandable, pelletized thermoplastic polymer materials, comprising from 5 to 100% by weight of a styrene copolymer A), from 0 to 95% by weight of polystyrene B), and from 0 to 95% by weight of a thermoplastic polymer C) other than A) and B), and a process for producing the expandable pelletized thermoplastic polymer materials.
摘要:
A power washer is provided with a transport frame, a wash unit and a gun. The wash unit and the gun may be separated from the transport frame to be used in multiple modes. Possible modes include a walk-behind mode, a spray mode and hand wash modes. A quick connection is also provided to make it easier to disconnect and reconnect various components of the power washer.
摘要:
A process prepares expandable propylene polymer beads by mixing propylene polymer melt with a volatile organic blowing agent and with a nucleating agent in an extruder, whereupon the extrusion and pelletization of the extruded takes place in a water bath under conditions of temperature and pressure at which practically no foaming of the pellets takes place.
摘要:
The invention relates to expanded polypropylene beads having a density of from 5 to 200 g/l and a bead diameter of from 1 to 10 mm which comprise from 0.002 to 20% by weight of graphite particles.
摘要:
Open-cell moldable foams are based on a thermoplastic matrix which comprises A. from 99 to 50% by weight of a styrene polymer and B. from 1 to 50% by weight of a polymer of low compatibility with the styrene polymer.
摘要:
The invention relates to expandable olefin bead polymers which comprise a blowing agent with a boiling point of from −5 to 150° C., selected from the group consisting of alkanes, alkanols, ketones, ethers and esters. The particles are unfoamed and have a bulk density above 500 g/l, and can be foamed to a bulk density below 200 g/l after storage for one hour at room temperature in free contact with the atmosphere. They are prepared by impregnating polyolefin pellets in suspension in a pressure vessel with the blowing agent, cooling the batch below 100° C., reducing the pressure and isolating the particles.
摘要:
Flame-retardant foam slabs are based on styrene polymers wherein from 1 to 12% by weight of expanded graphite and also, if desired, from 1 to 12% by weight of a phosphorus compound are present as flame retardants.
摘要:
Expandable, rubber-modified styrene polymers for elastic polystyrene foams comprisea) a continuous phase comprising polystyrene or a styrene copolymer containing at most 50% of copolymerized comonomers andb) from 5 to 30% by weight of a butadiene-styrene block copolymer dispersed therein,and also a low-boiling blowing agent. The rubber particles have a compact lamellar structure without polystyrene inclusions. The expandable styrene polymers are prepared by polymerization of styrene in the presence of the block copolymer and impregnation with the blowing agent.
摘要:
A process for the preparation of bead-form expandable styrene polymers by polymerizing styrene, if desired in the presence of further comonomers, in aqueous suspension in the presence of organic molecular colloids as suspension stabilizers and conventional styrene-soluble polymerization catalysts and with addition of a blowing agent and, if desired, conventional additives in effective amounts, wherein the aqueous suspension contains at least one olefinically unsaturated carboxylic acid or a water-soluble salt thereof in an amount, based on the organic phase, of from 0.002 to 0.3% by weight of carboxylate anions.
摘要:
A process for the preparation of expandable thermoplastic polymers by post-impregnation with a blowing agent in aqueous suspension in the presence of a mixture of magnesium pyrophosphate and a sulfonate group-containing extender as suspension stabilizer, in a reactor comprisesa) preparing the magnesium pyrophosphate in the same reactor at below 50.degree. C. by adding a solid magnesium salt in an amount corresponding to an at least 3% stoichiometric excess, based on pyrophosphate, to an aqueous solution of the pyrophosphate,b) heating the suspension medium to from 70.degree. to 140.degree. C. andc) adding the blowing agent in this temperature range.