摘要:
Expandable, rubber-modified styrene polymers for elastic polystyrene foams comprisea) a continuous phase comprising polystyrene or a styrene copolymer containing at most 50% of copolymerized comonomers andb) from 5 to 30% by weight of a butadiene-styrene block copolymer dispersed therein,and also a low-boiling blowing agent. The rubber particles have a compact lamellar structure without polystyrene inclusions. The expandable styrene polymers are prepared by polymerization of styrene in the presence of the block copolymer and impregnation with the blowing agent.
摘要:
The invention relates to expandable styrene polymers for elastic polystyrene foams, comprisinga) from 50 to 75% by weight of polystyrene and/or a styrene copolymer containing at least 50% by weight of copolymerized styrene,b) from 5 to 30% by weight of a styrene-soluble elastomer,c) from 5 to 20% by weight of at least one block copolymer containing styrene as one component,d) from 15 to 50% by weight of at least one polyolefin,e) from 1 to 15% by weight, based on the sum of a) and b), of a low-boiling blowing agent, and, if desired,f) conventional additives in effective amounts,and to foams produced therefrom.
摘要:
The invention relates to expandable styrene polymers for elastic polystyrene foams, comprisinga) from 75 to 98% by weight of polystyrene and/or a styrene copolymer containing at least 50% by weight of copolymerized styrene,b) from 2 to 25% by weight of at least one styrene-soluble elastomer,c) from 1 to 15% by weight, based on the sum of a) and b), of a low-boiling blowing agent, and, if desired,d) conventional additives in effective amounts,where the unfoamed beads have a structure in which the elastomer phase is dispersed in the polystyrene phase in the form of cell particles, and to foams and foam moldings produced therefrom.
摘要:
In a process for preparing expandable styrene polymers containing graphite particles, styrene is polymerized in aqueous suspension in the presence of graphite particles.
摘要:
Expandable styrene bead polymers having improved expandability contain from 1 to 20% by weight of a liquid oligomeric aliphatic olefin having 2 to 20 carbon atoms and a degree of polymerization of from 2 to 200.
摘要:
Rigid polyurethane foams having a low thermal conductivity are produced by reactinga) organic and/or modified organic polyisocyanates withb) at least one compound containing at least 2 reactive hydrogen atoms in the presence ofc) blowing agents,d) catalysts and, if desired,e) auxiliaries and/or additives,wherein graphite is added to the component a) and/or b).
摘要:
In a process for producing expandable styrene polymers containing graphite particles by polymerization of styrene in aqueous suspension in the presence of two peroxides which decompose at different temperatures, the peroxide which decomposes at lower temperature is multifunctional and on decomposition forms two or more linked polymer chains.
摘要:
Expandable styrene polymers (EPS) comprising, in each case based on the styrene polymer, a) from 0.05 to 5% by weight of an organic bromine compound whose bromine content is at least 50% by weight, as flame retardant, b) from 0.05 to 2% by weight of a flame retardant synergist, c) from 0.1 to 5% by weight of a metal salt as acid scavenger, and process for their production.
摘要:
Expandable styrene polymers (EPS) comprising, in each case based on the styrene polymer, a) from 0.05 to 5% by weight of an organic bromine compound whose bromine content is at least 50% by weight, as flame retardant, b) from 0.05 to 2% by weight of a flame retardant synergist, c) from 0.1 to 5% by weight of a metal salt as acid scavenger, and process for their production.
摘要:
Expandable, thermoplastic polymer bead material, comprising A) from 45 to 98.8 percent by weight of a styrene polymer, B1) from 1 to 45 percent by weight of a polyolefin whose melting point is in the range from 105 to 140° C., B2) from 0 to 25 percent by weight of a polyolefin whose melting point is below 105° C., C1) from 0.1 to 9.9 percent by weight of a styrene-butadiene block copolymer, C2) from 0.1 to 9.9 percent by weight of a styrene-ethylene-butylene block copolymer, D) from 1 to 15 percent by weight of a blowing agent, E) from 0 to 5 percent by weight of a nucleating agent where the entirety of A) to E) gives 100% by weight, and also processes for production of the same, and use for the production of elastic molded-foam moldings.