Method of forming foam moldings having varied density regions
    5.
    发明授权
    Method of forming foam moldings having varied density regions 失效
    形成具有不同密度区域的泡沫塑料模制品的方法

    公开(公告)号:US5252270A

    公开(公告)日:1993-10-12

    申请号:US879431

    申请日:1992-05-06

    CPC classification number: C08J9/232 B29C44/0469 B29C44/445 C08J2323/02

    Abstract: Moldings made from polyolefin particle foams having a mean density of from 0.015 to 0.100 g/cm.sup.3 and having at least two different regions whose densities differ by from 0.005 to 0.030 g/cm.sup.3 have a transition zone between the different density regions having a thickness of not more than 25 mm. A method of forming the moldings, using removable mold dividing walls, is described.

    Abstract translation: 平均密度为0.015〜0.100g / cm 3,具有至少两个密度为0.005〜0.030g / cm 3的不同区域的聚烯烃颗粒泡沫制成的模制品在不同密度区域之间的过渡区域的厚度不为 超过25毫米。 描述了使用可拆卸模具分隔壁形成模制件的方法。

    Expansion of shrunk foam particles of propylene polymers
    6.
    发明授权
    Expansion of shrunk foam particles of propylene polymers 失效
    膨胀丙烯聚合物的收缩泡沫颗粒

    公开(公告)号:US5045256A

    公开(公告)日:1991-09-03

    申请号:US549164

    申请日:1990-07-06

    CPC classification number: C08J9/22 C08J2323/10 Y10S521/918

    Abstract: Foam particles of propylene polymers which have shrunk from 40 to 95% of their original volume and have a bulk density of from 10 to 30 g/1 can be expanded if they are treated with air or nitrogen under superatmospheric pressure, subsequently decompressed. If desired post-foamed by heating and, after aging, re-treated with air or nitrogen under superatmospheric pressure, subsequently decompressed and aged under atmospheric pressure until the pressure in the cells has dissipated.

    Abstract translation: 如果在超大气压下用空气或氮气处理,则其膨胀的丙烯聚合物的泡沫颗粒已经收缩了其原始体积的40至95%并且具有10至30g / l的堆积密度,随后减压。 如果需要通过加热发泡,并且在老化之后,在空气或氮气中在超大气压下再次处理,随后在大气压下减压和老化,直到电池中的压力消散。

    Shock-absorbing propylene polymer composite moldings
    8.
    发明授权
    Shock-absorbing propylene polymer composite moldings 失效
    阻聚丙烯聚合物复合材料

    公开(公告)号:US5180628A

    公开(公告)日:1993-01-19

    申请号:US822263

    申请日:1992-01-17

    Abstract: A shock-absorbing propylene polymer composite molding containsa. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130.degree. to 165.degree. C.,b. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90.degree. to 140.degree. C.,c. a foam layer with a thickness of from 3 to 200 mm and a density of from 0.015 to 0.1 g/cm.sup.3 based on a propylene copolymer having a melting point of from 125.degree. to 155.degree. C.,d. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90.degree. to 140.degree. C.,e. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130.degree. to 165.degree. C.

    Abstract translation: 减震丙烯聚合物复合成型体包含a。 b。厚度为0.5至10毫米的层,其含有熔点为130至165℃的丙烯聚合物,b。 c)厚度为0.05至0.5mm的中间层,包括基于熔点为90-140℃的烯烃共聚物的热熔粘合剂,c。 d。基于熔点为125-155℃的丙烯共聚物,厚度为3至200mm,密度为0.015至0.1g / cm 3的泡沫层。 厚度为0.05至0.5mm的中间层,包括基于熔点为90°至140℃的烯烃共聚物的热熔粘合剂, 厚度为0.5〜10mm的层,其含有熔点为130〜165℃的丙烯聚合物。