摘要:
To offer a timepiece faceplate having exceptional transmission of light as well as exceptional aesthetic appearance, and to offer a timepiece provided with the timepiece faceplate. A timepiece faceplate 1 of the invention is provided with a first plate member 11 comprising a material having an optical transmission property, and a second plate member 12 comprising a material having an optical transmission property.
摘要:
A decorative article 1 includes a substrate 2 formed mainly of plastic material, an oxide coating 3 formed mainly of metal oxide material provided on the substrate 2, and a metal coating 4 formed mainly of metal material provided on a surface of the oxide coating 3 on a side opposite the surface of the oxide coating 3 that is adjacent the substrate 2. It is desirable that the oxide coating 3 is formed of a material including at least one material selected from among TiO2 and CrO. It is further desirable that the metal coating 4 is formed of a material including at least one material selected from among Ag, Cr, Au, Al, Ti, Sn, and In. It is still further desirable that the sum of the average thickness of the oxide coating 3 and the average thickness of the metal coating 4 is 0.02 to 2.5 μm.
摘要:
A decorative article 1A for a timepiece or the like is provided having a superior aesthetic appearance that can be maintained over a long period of time. The decorative article 1A has a substrate 2 wherein at least part of the surface vicinity is primarily configured from Ti and/or stainless steel, a first coat 3 formed on the substrate 2, and a second coat 4 formed on the first coat 3. The first coat 3 is configured primarily from TiCN, and the combined C content and N content in the first coat 3 is 5 to 30 wt %. The second coat 4 is configured primarily from M (where M is one or more elements selected from Ti, Pt, Pd, and In). The average thickness of the first coat 3 is 1.6 to 5 μm. The average thickness of the second coat 4 is 0.15 to 0.5 μm.
摘要:
A decorative article 1A for a timepiece or the like is provided having a superior aesthetic appearance that can be maintained over a long period of time. The decorative article 1A has a substrate 2 wherein at least part of the surface vicinity is primarily configured from Ti and/or stainless steel, a first coat 3 formed on the substrate 2, and a second coat 4 formed on the first coat 3. The first coat 3 is configured primarily from TiCN, and the combined C content and N content in the first coat 3 is 5 to 30 wt %. The second coat 4 is configured primarily from M (where M is one or more elements selected from Ti, Pt, Pd, and In). The average thickness of the first coat 3 is 1.6 to 5 μm. The average thickness of the second coat 4 is 0.15 to 0.5 μm.
摘要:
To offer a timepiece faceplate having exceptional transmission of light as well as exceptional aesthetic appearance, and to offer a timepiece provided with the timepiece faceplate, a timepiece faceplate of the invention is provided with a first plate member including a material having an optical transmission property, and a second plate member including a material having an optical transmission property.
摘要:
A method of manufacturing a decorative article, including a first coating formation step of forming a first coating of primarily TiN on a base member, and a second coating formation step of forming a second coating on the first coating by means of a dry plating method using an Au—Pd—Ag—In alloy of primarily Au and containing 6.0-9.0 wt % Pd, 6.0-8.0 wt % Ag, and 7.0-9.0 wt % In as a target.
摘要:
An ornamental article 1 has: a plastic material substrate 2; a first film 3 on the substrate 2 and made of a made of a material containing at least one substance selected from the group made of Cr, Ti, compounds of Cr, and compounds of Ti; and a second film provided adjacent to the surface of the first film that is on the opposite side of the side that faces the substrate and made of a material containing at least one metal selected from the group made of Ag and Al. It is preferred that the first film 3 contain at least one substance selected from the group made of Cr, Ti oxide, and Cr oxide. It is also preferred that the sum of the average thicknesses of the first film 3 and second film 4 be from 0.02 to 2.5 micrometers.