摘要:
The present invention relates to a process for applying integrated pretreatment layers having a thickness of 1 to 25 μm to metallic surfaces, particularly the surfaces of coil metals, by treatment with a composition comprising at least one binder, crosslinker, a finely divided inorganic filler, and a dicarboxylic acid-olefin copolymer. It also relates to shaped metallic articles provided with an integrated pretreatment layer of this kind, and to a formulation for implementing the process.
摘要:
The present invention relates to a composition for coating metallic surfaces, comprising a binder component; a corrosion inhibitor polymer based on an ethylenically monocarboxylic and dicarboxylic acid and, if appropriate, further ethylenical monomers, a solvent component, and, if appropriate, crosslinkable components, and also pigment/filler components. The invention further relates to processes for its preparation and also to methods of coating a metallic surface using the composition, to coated metallic surfaces thus obtained, and to the use of the composition as a primer, particularly in coil coating or in atmospheric corrosion control. After drying, the applied layer preferably has a thickness of at least 3.1 μm and is therefore thicker than a typical pretreatment layer.
摘要:
Copolymers which comprise dicarboxylic acid units modified with —SR, —CSNR2 and/or —CN units, and also at least one further comonomer. Processes for preparing them by polymer-analogous reaction, and their use as corrosion inhibitors.
摘要:
Method of applying corrosion control coats, especially integrated pretreatment layers or coats for atmospheric corrosion control, to metallic surfaces, using copolymers comprising as monomeric building blocks 20% to 70% by weight of monomers containing nitrogen heterocycles, 10% to 50% by weight of monomers containing acidic groups, 10% to 50% by weight of vinylaromatic monomers, and optionally 0% to 25% by weight of further monomers. Copolymers of the stated composition, and also preparations for applying corrosion control coats.
摘要:
Process for applying integrated pretreatment layers to metallic surfaces, particularly the surfaces of coil metals, by treatment with a composition comprising at least one binder, crosslinker, a finely divided inorganic filler, and compounds containing at least two thioamide groups or containing one thioamide group and at least one functional group. Integrated pretreatment layer obtainable by the process.
摘要:
A process for passivating a metallic surface by treating it with an acidic aqueous preparation comprising at least one itaconic acid homo- or copolymer. Passivating layers and metallic surfaces obtainable by means of the process.
摘要:
Process for the passivation of metallic surfaces, in particular of strip metals, by treatment of the surface with an acidic, aqueous preparation which comprises at least one water-soluble acid group-containing polymer and at least one wax.
摘要:
Partially neutralized carboxylate-rich copolymers, processes for their preparation and methods of using the same are disclosed, the copolymers comprising: monomers (A), (B), and (C); wherein monomer (A) comprises at least one monoethylenically unsaturated monocarboxylic acid, and is present in an amount of 30% to 79.99% by weight; wherein monomer (B) comprises at least one monoethylenically unsaturated dicarboxylic acid selected from the group consisting of acids corresponding to general formula I, acids corresponding to general formula II, anhydrides thereof, and other hydrolyzable derivatives thereof, and is present in an amount of 20.01% to 70% by weight: (HOOC)R1C═CR2(COOH) (I) R1R2C═C(—(CH2)n-COOH)(COOH) (II) wherein R1 and R2 each independently represent H or a straight-chain or branched, optionally substituted alkyl radical having 1 to 20 carbon atoms, or, in the case of (I), R1 and R2 together being an optionally substituted alkylene radical having 3 to 20 carbon atoms, and n represents an integer from 0 to 5; wherein monomer (C) comprises at least one additional ethylenically unsaturated comonomer, and is present in an amount of 0% to 40% by weight; wherein the carboxylate-rich copolymer is partially neutralized with at least one amine and the carboxylate-rich copolymer has a degree of neutralization of 2 to 18 mol %, based on the total amount of all COOH groups of the monocarboxylic and dicarboxylic acids; and wherein the carboxylate-rich copolymer has an average molecular weight Mw of at least 3000 g/mol.
摘要:
Flat shaped bodies which comprise at least one metallic layer, a conversion coat applied thereto, and at least one paint coat, and methods for producing such bodies starting from flat, metallic, semifinished products.