An adhesive blend is described that can include a semi-crystalline copolymer of propylene and at least one comonomer selected from the group consisting of ethylene and at least one C4 to C20 &agr;-olefin, the copolymer having a weight average molecular weight (Mw) from about 15,000 to about 200,000; an melt index (MI) from about 7 dg/min to about 3000 dg/min as measured by ASTM D 1238(B), and a (Mw/Mn) of approximately 2. Various production processes are also described. Also described are adhesive compositions and methods for making adhesive compositions having polymers or polymer blends with melt flow rates (MFRs) equal to and above 250° dg/min. at 230° C. Certain specific embodiments of the invention involve the use of a free radical initiator, e.g., a peroxide.
摘要:
An adhesive blend is described that can include a semi-crystalline copolymer of propylene and at least one comonomer selected from the group consisting of ethylene and at least one C4 to C20 α-olefin, the copolymer having a weight average molecular weight (Mw) from about 15,000 to about 200,000; an melt index (MI) from about 7 dg/min to about 3000 dg/min as measured by ASTM D 1238 (B), and a (Mw/Mn) of approximately 2. Various production processes are also described. Also described are adhesive compositions and methods for making adhesive compositions having polymers or polymer blends with melt flow rates (MFRS) equal to and above 250 dg/min. at 230°C. Certain specific embodiments of the invention involve the use of a free radical initiator, e.g., a peroxide.
摘要:
An adhesive blend is described that can include a semi-crystalline copolymer of propylene and at least one comonomer selected from the group consisting of ethylene and at least one C4 to C20 α-olefin, the copolymer having a weight average molecular weight (Mw) from about 15,000 to about 200,000; an melt index (MI) from about 7 dg/min to about 3000 dg/min as measured by ASTM D 1238(B), and a (Mw/Mn) of approximately 2. Various production processes are also described. Also described are adhesive compositions and methods for making adhesive compositions having polymers or polymer blends with melt flow rates (MFRs) equal to and above 250 dg/min. at 230° C. Certain specific embodiments of the invention involve the use of a free radical initiator, e.g., a peroxide.
摘要:
An adhesive blend is described that can include a semi-crystalline copolymer of propylene and at least one comonomer selected from the group consisting of ethylene and at least one C4 to C20 α-olefin, the copolymer having a weight average molecular weight (Mw) from about 15,000 to about 200,000; an melt index (MI) from about 7 dg/min to about 3000 dg/min as measured by ASTM D 1238(B), and a (Mw/Mn) of approximately 2. Various production processes are also described. Also described are adhesive compositions and methods for making adhesive compositions having polymers or polymer blends with melt flow rates (MFRs) equal to and above 250 dg/min. at 230 NC. Certain specific embodiments of the invention involve the use of a free radical initiator, e.g., a peroxide.
摘要:
The invention relates to novel adhesive alpha-olefin inter-polymers which are largely amorphous and have a rheological behavior that makes them suitable for adhesive use, both without and with minimized amounts of tackifying resins. Specifically, the invention poly-alpha olefin inter-polymer may be composed of A) from 60 to 94 mol % of units derived from one alpha mono-olefin having from 3 to 6 carbon atoms and B) from 6 to 40 mol % of units derived from one or more other mono-olefins having from 4 to 10 carbon atoms and at least one carbon atom more than A); and C) optionally from 0 to 10 mol % of units derived from another copolymerizable unsaturated hydrocarbon, different from A) and B); the diad distribution of component A in the polymer as determined by 13C NMR as described herein showing a ratio of experimentally determined diad distribution over the calculated Bernoullian diad distribution of less than 1.07; and the storage modulus G′ of said polymer, determined upon cooling as described herein, intersecting a value of 3.105 Pa at a temperature of less than 85° C. The invention also describes polymerization processes suitable for the manufacture of these adhesive alpha-olefin inter-polymers.
摘要:
The invention relates to novel adhesive alpha-olefin inter-polymers which are largely amorphous and have a rheological behavior that makes them suitable for adhesive use, both without and with minimzed amounts of tackifying resins. Specifically, the invention poly-alpha olefin inter-polymer may be composed of A) from 60 to 94% of units derived from one alpha mono-olefin having from 3 to 6 carbon atoms and B) from 6 to 40 mol % of units derived from one or more other mono-olefins having from 4 to 10 carbon atoms and at least one carbon atom more than A); and C) optionally from 0 to 10 mol % of units derived from another copolymerizable unsaturated hydrocarbon, different from A) and B); the diad distribution of component A in the polymer as determined by 13C NMR as described herein showing a ratio of experimentally determined diad distribution over the calculated Bernoullian diad distribution of less than 1.07; and the storage modulus G′ of said polymer, determined upon cooling as described herein, intersecting a value of 3.105 Pa at a temperature of less than 85° C. The invention also describes polymerization processes suitable for the manufacture of these adhesive alpha-olefin inter-polymers.
摘要翻译:本发明涉及新型粘合剂α-烯烃聚合物,其主要是无定形的并且具有使其适合于粘合剂使用的流变行为,不含和最少量的增粘树脂。 具体地说,本发明的聚α-烯烃聚合物可以由A)60-94%的衍生自一个具有3至6个碳原子的α-单烯烃的单元组成,B)6-40摩尔%衍生的单元 来自一种或多种其它具有4至10个碳原子和至少一个碳原子的单烯烃,比A)多; 和C)任选地0至10mol%衍生自不同于A)和B)的另一种可共聚不饱和烃的单元; 通过本文所述的13 C NMR确定的聚合物中组分A的二元分布显示出计算的伯努利二元分布的实验测定的二单元分布的比率小于1.07; 并且在本文所述的冷却下测定的所述聚合物的储能模量G'在小于85℃的温度下与3.10Pa的值相交。本发明还描述了适合于 制造这些粘合的α-烯烃聚合物。
摘要:
Embodiments of the present invention relate to article comprising 1) a functionalized component, 2) tackifier, and 3) an olefin polymer comprising one or more C3 to C40 olefins, optionally one or more diolefins, and less than 5 mole % of ethylene having a Dot T-Peel of 1 Newton or more, a branching index (g′) of 0.95 or less measured at the Mz of the polymer; and an Mw of 100,000 or less; where the functional component is selected from the group consisting of functionalized polymers, functionalized oligomers and beta nucleating agents; and where the Gardner color of the adhesive does not change by more than 7 Gardner units when the adhesive has been heat aged at 180° C. for 48 hours as compared to the Gardner color of the unaged composition.
摘要:
A composition suitable for an air barrier such as an automotive tire innertube, innerliner, and aircraft tire innertube or innerliner, curing bladders, and other pneumatic devices is disclosed. The composition comprises an elastomer, a processing oil, and a grafted resin component.
摘要:
Improved adhesives are provided through the use of styrenic tetrablock or pentablock copolymers which have a reduced elastomeric behavior under the die-cutting conditions used in label production.
摘要:
Adhesive compositions and a method for selecting adhesive compositions are disclosed herein. Preferred adhesives generally have small domains and/or a homogeneous domain distribution. The method of selecting adhesives is based on size and distribution of the domains.