Abstract:
A zeolitic material having framework type CHA, comprising a transition metal M and an alkali metal A, and having a framework structure comprising a tetravalent element Y, a trivalent element X and O, wherein the transition metal M is a transition I metal of groups 7 to 12 of the periodic table, A is one or more of K and Cs, Y is one or more of Si, Ge, Ti, Sn and Zr, and X is one or more of Al, B, Ga and In. A process for preparing such a zeolitic material. Use of such a zeolitic material.
Abstract:
The present invention relates to a process for the preparation of a zeolitic material SiO2 and X2O3 in its framework structure, wherein X stands for a trivalent element, wherein said process comprises interzeolitic conversion of a first zeolitic material comprising SiO2 and X2O3 in its framework structure, wherein the first zeolitic material has an FER-, TON-, MTT-, BEA-, MEL-, MWW-, MFS-, and/or MFI-type framework structure to a second zeolitic material comprising SiO2 and X2O3 in its framework structure, wherein the second zeolitic material obtained in (2) has a different type of framework structure than the first zeolitic material. Furthermore, the present invention relates to a zeolitic material per se as obtainable and/or obtained according to the inventive process and to its use, in particular as a molecular sieve, as an adsorbent, for ion-exchange, or as a catalyst and/or as a catalyst support.
Abstract:
The present invention relates to a method for the preparation of a treated zeolitic material having a BEA framework structure comprising the steps of: (i) providing a zeolitic material having a BEA framework structure, wherein the BEA framework structure comprises YO2 and X2O3, wherein Y is a tetravalent element, and X is a trivalent element, and wherein the zeolitic material having a BEA framework structure is obtainable and/or obtained from an organotemplate-free synthetic process; (ii) calcining the zeolitic material provided in step (i) at a temperature of 650° C. or more; and (iii) treating the calcined zeolitic material obtained from step (ii) with an aqueous solution having a pH of 5 or less, as well as to zeolitic materials per se preferably obtainable according to the inventive method and to their use, and to a process for converting oxygenates to olefins employing the inventive zeolitic materials.
Abstract:
The present invention relates to a rare earth element containing zeolitic material having a framework structure selected from the group consisting of AEI, AFT, AFV, AFX, AVL, CHA, EMT, GME, KFI, LEV, LTN, and SFW, including mixtures of two or more thereof, the framework structure of the zeolitic material comprising SiO2 and X2O3, wherein X stands for a trivalent element, wherein the zeolitic material displays an SiO2:X2O molar ratio in the range of from 2 to 20, and wherein the zeolitic material contains one or more rare earth elements as counter-ions at the ion exchange sites of the framework structure. Furthermore, the present invention relates to a process for the production of the inventive rare earth element containing zeolitic material as well as to the use of the inventive rare earth element containing zeolitic material.
Abstract:
The present invention relates to a process for the production of a zeolitic material having a BEA-type framework structure comprising YO2 and X2O3, wherein said process comprises the steps of (1) preparing a mixture comprising one or more sources for YO2 and one or more sources for X2O3; (2) crystallizing the mixture obtained in step (1); (3) subjecting the zeolitic material having a BEA-type framework structure obtained in step (2) to an ion-exchange procedure with Cu; and (4) subjecting the Cu ion-exchanged zeolitic material obtained in step (3) to an ion-exchange procedure with Fe; wherein Y is a tetravalent element, and X is a trivalent element, wherein the mixture provided in step (1) and crystallized in step (2) further comprises seed crystals comprising one or more zeolitic materials having a BEA-type framework structure, and wherein the mixture provided in step (1) and crystallized in step (2) does not contain an organotemplate as a structure-directing agent, as well as to the zeolitic material having a BEA framework structure per se, and to its use, in particular in a method for the treatment of NOx by selective catalytic reduction (SCR).
Abstract:
The present invention relates to a method for the preparation of a treated zeolitic material having a BEA framework structure including the steps of: (i) providing a zeolitic material having a BEA framework structure, wherein the BEA framework structure includes YO2 and X2O3, wherein Y is a tetravalent element, and X is a trivalent element, and wherein the zeolitic material having a BEA framework structure is obtainable and/or obtained from an organotemplate-free synthetic process; (ii) calcining the zeolitic material provided in step (i) at a temperature of 650° C. or more; and (iii) treating the calcined zeolitic material obtained from step (ii) with an aqueous solution having a pH of 5 or less, as well as to zeolitic materials per se preferably obtainable according to the inventive method and to their use, and to a process for converting oxygenates to olefins employing the inventive zeolitic materials.
Abstract:
The present invention relates to a process for preparing at least one sheet silicate comprising Ga and/or Zn, and based thereon, a framework silicate, preferably of the RRO structure type, to the sheet silicate and framework silicate themselves and to the uses of the silicates, especially of the framework silicate, preferably as catalysts.
Abstract:
Described is a process for the production of a pillared silicate. The process comprises (i) providing a layered silicate; (ii) interlayer expanding the layered silicate provided in step (i) comprising a step of treating the layered silicate with one or more swelling agents; (iii) treating the interlayer expanded silicate obtained in step (ii) with one or more hydrolyzable silicon containing compounds; (iv) treating the interlayer expanded compound obtained in step (iii) with an aqueous solution to obtain a pillared silicate; (v) removing at least a portion of the one or more swelling agents from the pillared silicate obtained in step (iv); and (vi) impregnating the pillared silicate obtained in step (v) with one or more elements selected from the group consisting of Fe, Ru, Ir, and combinations of two or more thereof. Also described is a pillared silicate optionally obtainable from said process and its use, in particular, in a process for the production of one or more olefins according to the invention.