公开(公告)号:US20240279769A1
公开(公告)日:2024-08-22
申请号:US18443862
申请日:2024-02-16
Applicant: CORNING INCORPORATED
Inventor: Deqiu Fan , Qiang Fu , Yuhui Jin , Grace MaryAlice Yu Leahy , Cedrick Alexander O’Shaughnessy
Abstract: A process for recovering lithium from lithium-containing glass based materials includes providing lithium-containing particles comprising the lithium-containing glass-based materials; contacting the lithium-containing particles with calcium salts in water, wherein the contacting causes leaching of at least a portion of lithium ions from the lithium-containing particles into a first leachate of the first mixture; separating the first mixture into the first leachate and a first residue; and recovering lithium from the first leachate.
-
公开(公告)号:US20250051219A1
公开(公告)日:2025-02-13
申请号:US18797619
申请日:2024-08-08
Applicant: CORNING INCORPORATED
Inventor: Qiang Fu , Kayla Nicole Horton , Cedrick Alexander O’Shaughnessy , Charisse Marye Spier , Alana Marie Whittier
Abstract: A glass composition includes: greater than or equal to about 70 mol % and less than or equal to about 90 mol % SiO2; greater than or equal to about 2 mol % and less than or equal to about 9 mol % Al2O3; greater than or equal to about 5 mol % and less than or equal to about 15 mol % Li2O; greater than or equal to about 0 mol % and less than or equal to about 10 mol % Y2O3; greater than or equal to about 0 mol % and less than or equal to about 9 mol % Ta2O5; greater than or equal to about 0 mol % and less than or equal to about 10 mol % La2O3; and greater than or equal to about 0.05 mol % and less than or equal to about 1 mol % SnO2. The sum of Y2O3, Ta2O5, and La2O3 may be greater than or equal to about 2 mol % and less than or equal to about 15 mol %.
-
公开(公告)号:US20240286913A1
公开(公告)日:2024-08-29
申请号:US18443962
申请日:2024-02-16
Applicant: CORNING INCORPORATED
Inventor: Bavani Balakrisnan , Deqiu Fan , Qiang Fu , Yuhui Jin , Grace MaryAlice Yu Leahy , Cedrick Alexander O’Shaughnessy
Abstract: Methods of recovering lithium from glass include crushing the glass to produce glass particles and contacting the glass particles with an aqueous leaching solution at a leaching temperature greater than ambient temperature and less than the boiling temperature of the aqueous leaching solution to produce a leachate slurry. The glass particles include lithium. The aqueous leaching solution includes sulfuric acid in water or sodium hydroxide in water. Contacting the glass particles with the aqueous leaching solution leaches greater than or equal to about 50% of the lithium out of the glass particles. The methods further comprise separating the leachate slurry to produce a solid residue and a leachate, the leachate comprising the lithium leached from the glass particles. The method further include recovering the lithium from the leachate through precipitation.
-
公开(公告)号:US20250121351A1
公开(公告)日:2025-04-17
申请号:US18893022
申请日:2024-09-23
Applicant: CORNING INCORPORATED
Abstract: A method for forming fluorite from a F−-containing aqueous fluid, the method comprising: contacting a bioactive glass comprising calcium with the F−-containing aqueous fluid; and forming the fluorite. A filter media, and filter containing the filter media, for forming fluorite from a F−-containing aqueous fluid, the filter media comprising: a bioactive glass comprising calcium; and at least one of sand, gravel, charcoal, polymer particles, and ceramic particles.
-
公开(公告)号:US20240287648A1
公开(公告)日:2024-08-29
申请号:US18582791
申请日:2024-02-21
Applicant: CORNING INCORPORATED
Inventor: David Eugene Baker , Deqiu Fan , Qiang Fu , Yuhui Jin , Grace MaryAlice Yu Leahy , William James McKendrick , Cedrick Alexander O’Shaughnessy
Abstract: A method for extracting lithium metal ions from glass includes contacting the glass with a molten salt bath for a duration of time, wherein the glass includes lithium and the contacting the glass with the molten salt bath for the duration of time extracts at least 40% of the lithium metal ions from the glass. The method further includes removing residual solids from the molten salt bath, wherein the residual solids include residual glass having a reduced concentration of lithium. The method further includes precipitating lithium metal ions from the molten salt bath to produce a solid precipitated lithium salt and separating the precipitated lithium salt from the molten salt bath.
-
6.
公开(公告)号:US20240182352A1
公开(公告)日:2024-06-06
申请号:US18386292
申请日:2023-11-02
Applicant: CORNING INCORPORATED
Inventor: Qiang Fu , Yuhui Jin , William James McKendrick , Cedrick Alexander O’Shaughnessy , Wei Sun
IPC: C03C3/085
CPC classification number: C03C3/085 , C03C21/002
Abstract: A method of regenerating a lithium-poisoned molten salt bath is provided. The method includes contacting glass particulates with the molten salt bath such that poisoning ions are exchanged from the bath into the glass. The glass compositions utilized in the method are also provided.
-
-
-
-
-