1.
公开(公告)号:US20180223092A1
公开(公告)日:2018-08-09
申请号:US15747917
申请日:2016-07-21
Applicant: DOW GLOBAL TECHNOLOGIES LLC
Inventor: Jacquelyn A. Degroot , Thor E. Gardarsson , Lisa S. Madenjian
CPC classification number: C08L53/00 , B29C48/0018 , B29K2023/08 , B29K2096/04 , B29K2105/0085 , B29K2995/0053 , B29L2031/4878 , B32B5/022 , B32B7/12 , B32B27/08 , B32B27/12 , B32B27/28 , B32B27/32 , B32B37/153 , B32B38/0008 , B32B2262/00 , B32B2262/02 , B32B2307/30 , B32B2307/51 , B32B2307/514 , B32B2307/518 , B32B2307/732 , B32B2307/738 , B32B2555/00 , B32B2555/02 , C08L2203/16 , C08L2205/02 , C08L2205/025
Abstract: Disclosed herein is a film comprising a polymer blend, the polymer blend comprising a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C. Disclosed herein too is a method of manufacturing a film comprising blending a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole to form a polymer blend; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C.; and forming the polymer blend into a film.
-
公开(公告)号:US11230641B2
公开(公告)日:2022-01-25
申请号:US15747917
申请日:2016-07-21
Applicant: DOW GLOBAL TECHNOLOGIES LLC
Inventor: Jacquelyn A. Degroot , Thor E. Gardarsson , Lisa S. Madenjian
IPC: C08L53/00 , B32B5/02 , B32B27/08 , B32B27/12 , B32B27/32 , B32B27/28 , B32B7/12 , B32B37/15 , B29C48/00 , B29K23/00 , B29K96/04 , B29K105/00 , B29L31/48 , B32B38/00
Abstract: Disclosed herein is a film comprising a polymer blend, the polymer blend comprising a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C. Disclosed herein too is a method of manufacturing a film comprising blending a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole to form a polymer blend; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C.; and forming the polymer blend into a film.
-