Abstract:
The invention provides a composition comprising the following components: A) a first composition, wherein the first composition comprises a first ethylene-based polymer and a second ethylene-based polymer, and wherein the ratio of the “high load melt index (I21) of the first composition” to the “high load melt index (I21) of the first ethylene-based polymer” is greater than, or equal to, 40, and B) one or more azide compounds present in an amount greater than, or equal to, 50 ppm, based on the weight of the first composition.
Abstract:
The instant invention provides a polyethylene composition suitable for film applications and film made therefrom. The linear low density polyethylene composition suitable for film applications according to the present invention comprises: less than or equal to 100 percent by weight of the units derived from ethylene; and less than 35 percent by weight of units derived from one or more α-olefin comonomers; wherein said linear low density polyethylene composition has a density in the range of from 0.890 to 0.915 g/cm3, a molecular weight distribution (Mw/Mn) in the range of from 2.5 to 4.5, a melt index (12) in the range of from 2 to 10 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of from 2.2 to 3, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition, and a zero shear viscosity ratio (ZSVR) in the range from 1 to 1.2.
Abstract:
The instant invention provides a polyethylene composition suitable for stretch film applications and, method of producing the same, and cast film made therefrom. The linear low density polyethylene composition suitable for stretch film applications according to the present invention comprises: less than or equal to 100 percent by weight of the units derived from ethylene; and less than 35 percent by weight of units derived from one or more α-olefin comonomers; wherein said linear low density polyethylene composition has a density in the range of from 0.900 to 0.930 g/cm3, a molecular weight distribution (Mw/Mn) in the range of from 2.5 to 4.5, a melt index (I2) in the range of from 0.3 to 10 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of from 2.2 to 3, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition, and a zero shear viscosity ratio (ZSVR) in the range from 1 to 1.2.
Abstract:
A linear low density polyethylene composition suitable for injection molding applications comprising less than or equal to 100 percent by weight of the units derived from ethylene, less than 35 percent by weight of units derived from one or more α-olefin comonomers, and characterized by its density, molecular weight distribution (Mw/Mn), a melt index (I2), a molecular weight distribution (Mz/Mw), vinyl unsaturation, and zero shear viscosity ratio (ZSVR). The linear low density polyethylene composition exhibits low hexane extractable levels.
Abstract:
The instant invention provides a linear low density polyethylene composition suitable for film applications, and films made therefrom. The linear low density polyethylene composition suitable for film applications comprises: (a) less than or equal to 100 percent by weight of the units derived from ethylene; and (b) less than 35 percent by weight of units derived from one or more α-olefin comonomers; wherein said linear low density polyethylene composition has a density in the range of 0.905 to 0.925 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 2.5 to 4.5, a melt index (I2) in the range of 0.1 to 3 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of from 2.2 to 3, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition, and a zero shear viscosity ratio (ZSVR) in the range from 1 to 1.2.
Abstract:
The invention provides a composition comprising a first composition, wherein the first composition comprises a first ethylene-based polymer and a second ethylene-based polymer, and wherein the first composition has a high load melt index (I21) less than 17, a density greater than, or equal to, 0.952 g/cm3, a molecular weight distribution MWD (conv), defined as the ratio of the weight average molecular weight to the number average molecular weight (Mw (conv)/Mn (conv)), greater than, or equal to, 11; and a viscosity ratio, η(0.01 s−1)/η(100 s−1) at 190° C., greater than, or equal to, 60.
Abstract:
A linear low density polyethylene composition suitable for injection molding applications comprising less than or equal to 100 percent by weight of the units derived from ethylene, less than 35 percent by weight of units derived from one or more α-olefin comonomers, and characterized by its density, molecular weight distribution (Mw/Mn), a melt index (I2), a molecular weight distribution (Mz/Mw), vinyl unsaturation, and zero shear viscosity ratio (ZSVR). The linear low density polyethylene composition exhibits low hexane extractable levels.
Abstract:
The invention provides a composition comprising the following components: A) a first composition, wherein the first composition comprises a first ethylene-based polymer and a second ethylene-based polymer, and wherein the ratio of the “high load melt index (I21) of the first composition” to the “high load melt index (I21) of the first ethylene-based polymer” is greater than, or equal to, 40, and B) one or more azide compounds present in an amount greater than, or equal to, 50 ppm, based on the weight of the first composition.
Abstract:
The instant invention provides a sealant composition, method of producing the same, film layers and multilayer structures made therefrom. The linear low density polyethylene composition suitable for sealant applications according to the present invention comprises: less than or equal to 100 percent by weight of the units derived from ethylene; less than 35 percent by weight of units derived from one or more α-olefin comonomers; wherein said linear low density polyethylene composition has a density in the range of 0.900 to 0.920 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 2.5 to 4.5, a melt index (I2) in the range of 0.5 to 3 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of from 2.2 to 3, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition, and a zero shear viscosity ratio (ZSVR) in the range from 1.0 to 1.2.
Abstract:
The invention provides a composition comprising a first composition, wherein the first composition comprises a first ethylene-based polymer and a second ethylene-based polymer, and wherein the first composition has a high load melt index (I21) less than 17, a density greater than, or equal to, 0.952 g/cm3, a molecular weight distribution MWD (conv), defined as the ratio of the weight average molecular weight to the number average molecular weight (Mw(conv)/Mn(conv)), greater than, or equal to, 11; and a viscosity ratio, η(0.01 s−1)/η(100 s−1) at 190° C., greater than, or equal to, 60.