    IPC分类号: B32B3/00 B32B7/02 B32B27/00

    摘要: An antireflective film is provided, the antireflective film including: a transparent support; and at least one low refractive index layer, wherein the low refractive index layer is formed from a composition containing at least following (A) to (C): (A) a fluorine-containing antifouling agent having at least one polymerizable unsaturated group; (B) a fluorine-containing copolymer having at least one polymerizable unsaturated group; and (C) inorganic fine particles.

    摘要翻译: 提供一种抗反射膜,该防反射膜包括:透明支撑体; 和至少一个低折射率层,其中所述低折射率层由至少含有以下(A)至(C)的组合物形成:(A)具有至少一个可聚合不饱和基团的含氟防污剂; (B)具有至少一个可聚合不饱和基团的含氟共聚物; 和(C)无机细颗粒。

    ANTISTATIC HARD COAT LAYER FORMING COMPOSITION, OPTICAL FILM, OPTICAL FILM MANUFACTURING METHOD, POLARIZATION PLATE, AND IMAGE DISPLAY DEVICE
    2.
    发明申请
    ANTISTATIC HARD COAT LAYER FORMING COMPOSITION, OPTICAL FILM, OPTICAL FILM MANUFACTURING METHOD, POLARIZATION PLATE, AND IMAGE DISPLAY DEVICE 审中-公开
    防静电硬层成型组合物,光学膜,光学膜制造方法,极化板和图像显示装置

    公开(公告)号:US20130052434A1

    公开(公告)日:2013-02-28

    申请号:US13600026

    申请日:2012-08-30

    摘要: Providing is an antistatic hard-coat-layer forming composition including a nonvolatile component containing a conductive polymer (a) a compound (b) and a photo-polymerization initiator (c); and a volatile component containing a solvent (d) having a hydroxyl group, and a solvent (e) having no hydroxyl group where the boiling point is 120° C. or less, wherein the solvent (d) contains a solvent (d2) with 4 or more carbon atoms having a hydroxyl group where the boiling point is 90° C. or more and the SP value is 22.0 to 35.0, the proportion of the polymer (a) in the nonvolatile component is 1 to 20 mass %, the proportion of the solvent (d) in the volatile component is 0.5 to 25 mass %, and the proportion of the component (d2) in the component (d) is 80 to 100 mass %.

    摘要翻译: 提供一种抗静电硬涂层形成组合物,其包含含有导电聚合物(a)化合物(b)和光聚合引发剂(c)的非挥发性组分; 和含有羟基的溶剂(d)的挥发性成分和沸点为120℃以下的不含羟基的溶剂(e),其中溶剂(d)含有溶剂(d 2)与 具有沸点为90℃以上且SP值为22.0〜35.0的羟基的4个以上的碳原子,非挥发成分中的聚合物(a)的比例为1〜20质量%,比例 挥发性成分中的溶剂(d)的比例为0.5〜25质量%,成分(d)的成分(d 2)的比例为80〜100质量%。

    ANTIREFLECTIVE FILM, POLARIZING PLATE, IMAGE DISPLAY DEVICE AND COATING COMPOSITION FOR FORMING LOW REFRACTIVE INDEX LAYER
    3.
    发明申请
    ANTIREFLECTIVE FILM, POLARIZING PLATE, IMAGE DISPLAY DEVICE AND COATING COMPOSITION FOR FORMING LOW REFRACTIVE INDEX LAYER 审中-公开
    抗反射膜,极化板,图像显示装置和涂层组合物,用于形成低折射率指数层

    公开(公告)号:US20100246014A1

    公开(公告)日:2010-09-30

    申请号:US12750804

    申请日:2010-03-31

    IPC分类号: G02B1/11 B32B27/00 C09D4/00

    摘要: An antireflective film includes: a transparent substrate film; and at least one low refractive index layer, the low refractive index layer is formed with a composition containing: a fluorine-containing antifouling agent having a weight average molecular weight of less than 10,000 and a structure represented by the following formula (F); a polyfunctional monomer having a polymerizable unsaturated group; and (C) an inorganic particle, and a content of the fluorine-containing antifouling agent is 1% by weight or more and less than 25% by weight based on a total solid content of the coating composition: (Rf)-[(W)-(RA)n]m  Formula (F) wherein, Rf represents a (per)fluoroalkyl group or a (per)fluoropolyether group, W represents a connecting group, RA represents a functional group having a polymerizable unsaturated group, n represents an integer of from 1 to 3, and m represents an integer of from 1 to 3.

    摘要翻译: 防反射膜包括:透明基板膜; 和至少一个低折射率层,低折射率层由含有重均分子量小于10,000的含氟防污剂和由下式(F)表示的结构的组合物形成; 具有聚合性不饱和基团的多官能单体; 和(C)无机颗粒,并且含氟防污剂的含量相对于涂料组合物的总固体含量为1重量%以上且小于25重量%:(Rf) - [(W ) - (RA)n] m式(F)其中,Rf表示(全)氟烷基或(全)氟聚醚基,W表示连接基,RA表示具有可聚合不饱和基的官能团,n表示 1〜3的整数,m表示1〜3的整数。

    OPTICAL FILM, POLARIZING PLATE AND IMAGE DISPLAY APPARATUS
    4.
    发明申请
    OPTICAL FILM, POLARIZING PLATE AND IMAGE DISPLAY APPARATUS 有权
    光学膜,偏光板和图像显示装置

    公开(公告)号:US20100079867A1

    公开(公告)日:2010-04-01

    申请号:US12566712

    申请日:2009-09-25

    IPC分类号: G02B1/11

    摘要: An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°

    摘要翻译: 提供一种光学膜,所述光学膜包括:支撑体; 以及至少一个具有凹凸表面的防眩光层,其中,所述至少一个防眩光层包含至少一种透光性颗粒,所述至少一种透光性颗粒包含基于总固体含量为0.01〜1质量%的第一透光性颗粒 防眩光层,第一透光性颗粒的平均粒径比防眩光层的平均厚度大0.1〜4.0μm,区域&gt;(0.5)倾斜角度&amp; 防眩光层表面的粗糙度在0°的范围内; <0.5°构成防眩光层表面的40%至98%。

    OPTICAL FILM, POLARIZING PLATE, AND IMAGE DISPLAY APPARATUS
    5.
    发明申请
    OPTICAL FILM, POLARIZING PLATE, AND IMAGE DISPLAY APPARATUS 有权
    光学膜,偏光板和图像显示装置

    公开(公告)号:US20090091835A1

    公开(公告)日:2009-04-09

    申请号:US12239372

    申请日:2008-09-26

    IPC分类号: G02B1/11 B32B5/16

    摘要: An optical film includes, in the following order, a support; an antiglare layer having an uneven surface; a high refractive index layer; and a low refractive index layer, wherein an arithmetic average roughness (Ra) of the optical film is: 0.03 μm

    摘要翻译: 光学薄膜按以下顺序包括支撑体; 具有不平坦表面的防眩层; 高折射率层; 和低折射率层,其中光学膜的算术平均粗糙度(Ra)为0.03μm(Ra <0.4μm),光学膜的平均不平均距离(Sm)为:80μm

    OPTICAL FILM, POLARIZING PLATE AND IMAGE DISPLAY DEVICE
    6.
    发明申请
    OPTICAL FILM, POLARIZING PLATE AND IMAGE DISPLAY DEVICE 有权
    光学薄膜,偏光板和图像显示装置

    公开(公告)号:US20090081447A1

    公开(公告)日:2009-03-26

    申请号:US12238261

    申请日:2008-09-25

    IPC分类号: B32B5/16 C08L67/00

    摘要: An optical film, includes: a transparent support; and at least one low refractive index layer, wherein the at least one low refractive index layer is a layer formed from a coating composition containing: (A) an inorganic fine particle; (B) a fluorine-containing copolymer; and (C) a polyfunctional fluorine-containing acrylate, and the polyfunctional fluorine-containing acrylate (C) is represented by the following structural formula: wherein Rf represents a (p+q)-valent perfluoro saturated hydrocarbon group having a carbon number of 1 to 20, which may have an ether bond; p represents an integer of 2 to 10; q represents an integer of 0 to 8, provided that (p+q) represents an integer of 2 to 10; r represents an integer of 0 to 100; and R represents a hydrogen atom, a methyl group, a fluorine atom or a trifluoromethyl group.

    摘要翻译: 一种光学膜,包括:透明支撑体; 和至少一个低折射率层,其中所述至少一个低折射率层是由包含以下物质的涂料组合物形成的层:(A)无机细颗粒; (B)含氟共聚物; 和(C)多官能含氟丙烯酸酯,多官能含氟丙烯酸酯(C)由以下结构式表示:其中,Rf表示碳数为1的(p + q)价全氟饱和烃基 至20,其可具有醚键; p表示2〜10的整数, q表示0〜8的整数,条件是(p + q)表示2〜10的整数。 r表示0〜100的整数, R表示氢原子,甲基,氟原子或三氟甲基。

    PRODUCTION METHOD OF ANTIREFLECTION FILM, ANTIREFLECTION FILM AND COATING COMPOSITION
    7.
    发明申请
    PRODUCTION METHOD OF ANTIREFLECTION FILM, ANTIREFLECTION FILM AND COATING COMPOSITION 审中-公开
    抗反射膜的制备方法,抗反射膜和涂层组合物

    公开(公告)号:US20120207992A1

    公开(公告)日:2012-08-16

    申请号:US13396195

    申请日:2012-02-14

    摘要: A production method of an antireflection film comprises, in order, a step of applying a coating composition obtained by mixing the following components (A) to (D) on a base material to form a coating film, a step of drying the coating film to volatilize the solvent therefrom, and a step of curing the coating film to form a cured layer, wherein a multilayer structure having different refractive indexes is formed from the coating composition: (A) a compound having at least one structure selected from a fluorine-containing hydrocarbon structure and a polysiloxane structure and at least one basic functional group, (B) an inorganic fine particle, (C) a curable binder containing no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.

    摘要翻译: 防反射膜的制造方法依次包括将通过将下列组分(A)至(D)混合在基材上而获得的涂料组合物涂覆在基材上以形成涂膜的步骤,将涂膜干燥至 使溶剂挥发,并且使涂膜固化形成固化层的步骤,其中由涂料组合物形成具有不同折射率的多层结构体:(A)具有至少一种选自氟 烃结构和聚硅氧烷结构和至少一个碱性官能团,(B)无机细颗粒,(C)分子中不含氟原子的可固化粘合剂和(D)溶剂,条件是质量比[ 组分(A)+组分(B)] / [组分(C)]为1/199至60/40。

    METHOD FOR PRODUCING ANTIREFLECTION FILM, ANTIREFLECTION FILM, AND COATING COMPOSITION
    8.
    发明申请
    METHOD FOR PRODUCING ANTIREFLECTION FILM, ANTIREFLECTION FILM, AND COATING COMPOSITION 有权
    生产抗反射膜,抗反射膜和涂层组合物的方法

    公开(公告)号:US20160187540A2

    公开(公告)日:2016-06-30

    申请号:US13451214

    申请日:2012-04-19

    摘要: The method for producing an antireflection film is provided. The method includes, a step of coating a coating composition including the following components (A) to (D) on a base material to form a coating film, a step of volatilizing the solvent from the coating film for drying the coating film, and a step of curing the coating film to form a cured layer, in which a multilayer structure having different refractive indices from the coating composition is formed: (A) a fluorine-containing polymer with a specific structure, having a polyalkylene oxide group in the molecule, (B) non-surface-modified inorganic fine particles, or inorganic fine particles that are surface-treated with a silane coupling agent having a molecular weight of 600 or less, (C) a curable binder having no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.

    摘要翻译: 提供了制造抗反射膜的方法。 该方法包括:将下述成分(A)〜(D)的涂料组合物涂布在基材上形成涂膜的工序,使涂膜干燥后的溶剂挥发的工序,以及 固化涂膜以形成固化层的步骤,其中形成具有与涂料组合物不同的折射率的多层结构:(A)具有特定结构的含氟聚合物,在分子中具有聚环氧烷基团, (B)分子量为600以下的硅烷偶联剂进行表面处理的非表面改性无机微粒或无机微粒,(C)分子中不含氟原子的固化性粘合剂,以及 (D)成分,[成分(A)+成分(B)] / [成分(C)]的质量比为1/199〜60/40。

    METHOD FOR PRODUCING ANTIREFLECTION FILM, ANTIREFLECTION FILM, AND COATING COMPOSITION
    9.
    发明申请
    METHOD FOR PRODUCING ANTIREFLECTION FILM, ANTIREFLECTION FILM, AND COATING COMPOSITION 有权
    生产抗反射膜,抗反射膜和涂层组合物的方法

    公开(公告)号:US20120270021A1

    公开(公告)日:2012-10-25

    申请号:US13451214

    申请日:2012-04-19

    摘要: The method for producing an antireflection film is provided. The method includes, a step of coating a coating composition including the following components (A) to (D) on a base material to form a coating film, a step of volatilizing the solvent from the coating film for drying the coating film, and a step of curing the coating film to form a cured layer, in which a multilayer structure having different refractive indices from the coating composition is formed: (A) a fluorine-containing polymer with a specific structure, having a polyalkylene oxide group in the molecule, (B) non-surface-modified inorganic fine particles, or inorganic fine particles that are surface-treated with a silane coupling agent having a molecular weight of 600 or less, (C) a curable binder having no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.

    摘要翻译: 提供了制造抗反射膜的方法。 该方法包括:将下述成分(A)〜(D)的涂料组合物涂布在基材上形成涂膜的工序,使涂膜干燥后的溶剂挥发的工序,以及 固化涂膜以形成固化层的步骤,其中形成具有与涂料组合物不同的折射率的多层结构:(A)具有特定结构的含氟聚合物,在分子中具有聚环氧烷基团, (B)分子量为600以下的硅烷偶联剂进行表面处理的非表面改性无机微粒或无机微粒,(C)分子中不含氟原子的固化性粘合剂,以及 (D)成分,[成分(A)+成分(B)] / [成分(C)]的质量比为1/199〜60/40。

    PRODUCTION METHOD OF ANTIREFLECTION FILM, ANTIREFLECTION FILM AND COATING COMPOSITION
    10.
    发明申请
    PRODUCTION METHOD OF ANTIREFLECTION FILM, ANTIREFLECTION FILM AND COATING COMPOSITION 审中-公开
    抗反射膜的制备方法,抗反射膜和涂层组合物

    公开(公告)号:US20120207990A1

    公开(公告)日:2012-08-16

    申请号:US13396135

    申请日:2012-02-14

    IPC分类号: B32B7/02 C09D135/02 B05D5/06

    摘要: A production method of an antireflection film comprises, in order, a step of applying a coating composition obtained by mixing the following components (A) to (D) on a base material to form a coating film, a step of drying the coating film to volatilize the solvent therefrom, and a step of curing the coating film to form a cured layer, wherein a multilayer structure having different refractive indexes is formed from the coating composition: (A) a compound having at least one structure selected from a fluorine-containing hydrocarbon structure and a polysiloxane structure and at least one isocyanate group; (B) an inorganic fine particle; (C) a curable binder containing no fluorine atom in the molecule; and (D) a solvent; provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.

    摘要翻译: 防反射膜的制造方法依次包括将通过将下列组分(A)至(D)混合在基材上而获得的涂料组合物涂覆在基材上以形成涂膜的步骤,将涂膜干燥至 使溶剂挥发,并且使涂膜固化形成固化层的步骤,其中由涂料组合物形成具有不同折射率的多层结构体:(A)具有至少一种选自氟 烃结构和聚硅氧烷结构和至少一个异氰酸酯基团; (B)无机细粒; (C)分子中不含氟原子的可固化粘合剂; 和(D)溶剂; 条件是[成分(A)+成分(B)] / [成分(C)]的质量比为1/199〜60/40。