CELLULOSE FIBER-DISPERSING RESIN COMPOSITE MATERIAL, FORMED BODY, AND COMPOSITE MEMBER

    公开(公告)号:US20210221988A1

    公开(公告)日:2021-07-22

    申请号:US17226581

    申请日:2021-04-09

    Abstract: A cellulose fiber-dispersing resin composite material, containing a cellulose fiber dispersed in a resin, in which a content of the cellulose fiber is 1% by mass or more and less than 70% by mass, and LL and LN satisfy the following [Expression 1], when a length weighted average fiber length of the cellulose fiber is taken as LL, and a number average fiber length of the cellulose fiber is taken as LN measured under the following measurement condition; a formed body using this composite material; and a composite member using this formed body. LL and LN are determined for a dissolution residue obtained by immersing the cellulose fiber-dispersing resin composite material in a solvent capable of dissolving the resin in the composite material, in accordance with Pulps-Determination of fiber length by automated optical analysis specified by ISO 16065 2001. 1.1

    FIBER-DISPERSED RESIN COMPOSITE MATERIAL, MOLDING, AND COMPOSITE MEMBER

    公开(公告)号:US20220162409A1

    公开(公告)日:2022-05-26

    申请号:US17670918

    申请日:2022-02-14

    Abstract: A fiber-dispersed resin composite material, containing fiber dispersed in a resin, wherein the content of the fiber in the fiber-dispersed resin composite material is 1 mass % or more and less than 70 mass %, and wherein the fiber-dispersed resin composite material has a maximum color difference A determined under conditions below of 0.05 or more and 6 or less:

    L*, a*, and b* values in CIE (L*a*b*) color space are measured on a straight line at 8 points with an interval of 1 cm by using a chromameter, and a color difference ΔE1 between measurement points linearly adjacent to each other is calculated by [Expression 1-1] below while a maximum value among 7 calculated values for the resulting color difference ΔE1 is set as the maximum color difference A, Δ ⁢ E ⁢ 1 = [ ( L i + 1 ⋆ - L i ⋆ ) 2 + ( a i + 1 * - a i * ) 2 + ( b i + 1 ⋆ - b i ⋆ ) 2 ] 0 . 5 [ Expression ⁢ ⁢ 1 ⁢ - ⁢ 1 ] where L*i, a*i, and b*i are the L*, a*, and b* values at i-th measurement point among the 8 measurement points, and i is an integer of 1 to 7 in [Expression 1-1].

    RESIN FORMED BODY AND RESIN COMPOSITION

    公开(公告)号:US20210198463A1

    公开(公告)日:2021-07-01

    申请号:US17201674

    申请日:2021-03-15

    Abstract: A resin formed body obtained from a resin composition that contains a polypropylene resin and a cellulose fiber, the polypropylene resin partially containing an acid modified polypropylene resin, wherein the resin formed body has a diffraction peak derived from a polypropylene α-crystal (040) plane at a position of a scattering vector s of 1.92±0.1 nm−1, a diffraction peak derived from a polypropylene β-crystal (300) plane at a position of a scattering vector s of 1.83±0.1 nm−1, and a diffraction peak derived from a cellulose Iβ type crystal (004) plane at a position of a scattering vector s of 3.86±0.1 nm−1, observed in a wide-angle X-ray diffraction measurement, and wherein an orientation degree of the cellulose fiber in the resin formed body is larger than 0.1 and less than 0.8.

    RESIN FORMED BODY AND RESIN COMPOSITION

    公开(公告)号:US20210198462A1

    公开(公告)日:2021-07-01

    申请号:US17199859

    申请日:2021-03-12

    Abstract: A resin formed body, having a diffraction peak at a position where a scattering vector s is 3.86±0.1 nm−1 in a wide-angle X-ray diffraction measurement, and having at least one melting peak each at respective regions of 129° C. or lower and 159° C. or higher in a differential scanning calorimetry, and with which a peak of tan δ is observed in a range of −40±10° C. in a dynamic viscoelastic measurement, and a resin composition suitable for preparing the same.