摘要:
With use of separated alloy powder (10) as a sintering material, it is possible to utilize characteristics of metals of different types (SUS steel and Cu, for example). Further, a boundary surface between regions constituted by different metals is at least partially alloyed. Thus, it is possible to enhance bonding strength between the regions, and possible to enhance strength of a sintered bearing.
摘要:
A sintered metal bearing is obtained by compression-molding of a raw-material powder containing at least a Cu powder, an SUS powder, and a pure Fe powder and thereafter sintering a compression-molded body at a predetermined temperature.
摘要:
Provided are a sintered metal material improved in sliding property and wear resistance with respect to an associated sliding member to be supported, and a sintered oil-impregnated bearing formed of this metal material. A bearing sleeve is formed by compacting a mixed metal powder composed of not less than 5 wt % and not more than 94.3 wt % of Cu powder, not less than 5 wt % and not more than 94.3 wt % of SUS powder, not less than 0.2 wt % and not more than 10 wt % of Sn powder, and not less than 0.5 wt % and not more than wt % of graphite, and then performing sintering on a compact of the mixed metal powder.
摘要:
A density of a bearing sleeve made of a sintered metal is set within a range of from 80% to 95% with respect to a true density, and a Young's modulus of the bearing sleeve is set to be equal to or more than 70 GPa. When the density of the bearing sleeve is increased and also the Young's modulus thereof is set to be equal to or more than 70 GPa in this manner, dimensional variation of an inner peripheral surface of the bearing sleeve can be suppressed to be equal to or less than 0.5 μm when a shaft member having an outer diameter of from 2 mm to 4 mm is to be supported.
摘要:
A maximum diameter (d) of each of surface openings formed in a bearing surface through melting of Sn metal powder as a binder is set within a range of 0 μm
摘要:
A sintered metal bearing is obtained by compression-molding of a raw-material powder containing at least a Cu powder, an SUS powder, and a pure Fe powder and thereafter sintering a compression-molded body at a predetermined temperature.
摘要:
A maximum diameter (d) of each of surface openings formed in a bearing surface through melting of Sn metal powder as a binder is set within a range of 0 μm
摘要:
A method for quenching a steel pipe by water cooling from an outer surface thereof, where pipe end portions are not subjected to water cooling, and at least part of a main body other than the pipe end portions is subjected to water cooling. A region(s) that is not subjected to direct water cooling over an entire circumference thereof can be along an axial direction at least in part of the main body other than the pipe end portions. The start and stop of water cooling can be intermittent at least in part of the quenching. During the water cooling of the pipe outer surface, an intensified water cooling can be performed in a temperature range in which the pipe outer surface temperature is higher than Ms point. Thereafter, the cooling can be switched to moderate cooling so that the outer surface is cooled down to Ms point or lower.
摘要:
To provide a thermal spray membrane contact material, contact member and contact part and an apparatus to which they are applied, showing excellent seizure resistance and wear resistance even under high surface pressure/low speed sliding, high speed/high temperature sliding, or high surface pressure/high speed sliding. In a bucket connecting apparatus connecting an arm and a bucket by a work implement connecting pin, the above-mentioned work implement connecting pin comprises a base material made of steel having an axis function and a contact surface formed of a thermal spray membrane contact material film-formed on the base material, said contact surface being placed at least on a supported surface site of the work implement connecting pin relative to a bracket and on a slipping contact surface with a work implement bushing, further, said thermal spray membrane contact material being composed of a Mo metal phase, or 10 vol % or more of a Mo metal phase and a metal phase and/or alloy phase containing one or more elements selected from the group consisting of Fe, Ni, Co, Cr, Cu and Zn.
摘要:
The present invention provides a device and a method for displaying appropriately on the display area for each processing unit such as an application according to the applied equipment. The CPU 12 processes display area acquisition requests from a plurality of processing units R1-Rn according to a display management program. The display management program decides whether use of the display area is allowed to each processing unit, considering the relationship of the plurality of display areas requested from each processing unit R1-Rn. Each processing unit R1-Rn executes display processing for the display area for which use is allowed. In this way, whether use is allowed is notified from the display management program to each processing unit R1-Rn after each processing unit R1-Rn sends the display area acquisition request. As a consequence, display in a plurality of areas by each processing unit R1-Rn can be controlled appropriately.