1.
公开(公告)号:US20170240761A1
公开(公告)日:2017-08-24
申请号:US15238112
申请日:2016-08-16
Applicant: GRAND TEK ADVANCE MATERIAL SCIENCE CO., LTD.
Inventor: Hsueh-Tso LIN , Rui-Gang HOU , Dick ZHONG
IPC: C09D127/14 , C08J7/04 , B05D7/00 , C09D5/00
CPC classification number: C09D127/14 , B05D3/0254 , B05D3/0406 , B05D7/50 , B05D7/542 , B05D2202/00 , B05D2401/21 , B05D2506/10 , C08J7/047 , C08J2327/14 , C08J2427/14 , C09D5/002
Abstract: A method of manufacturing a coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first PVF, 30-70 parts by weight of an assistance resin, 5-30 parts by weight of a curing agent, 100-120 parts by weight of a first latent solvent, 3-methoxy-3-methyl-1-butanol, and water. The first latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 60:10-20:40-60. The method also applies a finish paint on the primer paint, wherein the finish paint includes 100 parts by weight of a second PVF, 100-120 parts by weight of a second latent solvent, 3-methoxy-3-methyl-1-butanol, and water, wherein the second latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 50:10-20:30-60. The primer paint and the finish paint are baked and dried to form a coating.
-
公开(公告)号:US20170240760A1
公开(公告)日:2017-08-24
申请号:US15219756
申请日:2016-07-26
Applicant: GRAND TEK ADVANCE MATERIAL SCIENCE CO., LTD.
Inventor: Hsueh-Tso LIN , Rui-Gang HOU , Chih-Hung LIN , Dick ZHONG
IPC: C09D127/14 , C09D1/00 , B05D3/02 , C09D7/12 , C09D163/00 , C09D171/00 , C09D5/08
CPC classification number: C09D127/14 , B05D3/0254 , B05D7/14 , B05D7/148 , B05D7/546 , B05D2252/02 , B05D2504/00 , B05D2506/10 , B05D2601/24 , C09D1/00 , C09D5/08 , C09D7/48 , C08L63/00 , C08L75/06
Abstract: A method of manufacturing a bi-layered coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first polyvinyl fluoride, 20 to 50 parts by weight of an assistance resin, and 150 to 170 parts by weight of a first latent solvent, and wherein the assistance resin is polyester modified epoxy resin, polyester type polyurethane resin, phenoxy resin, or a combination thereof. The primer paint is baked and dried to form a primer coating. A finish paint is then applied onto the primer coating, wherein the finish paint includes 100 parts by weight of a second polyvinyl fluoride and 120 to 150 parts by weight of a second latent solvent. The finish paint is baked and dried to form a finish coating on the primer coating.
-
3.
公开(公告)号:US20170232470A1
公开(公告)日:2017-08-17
申请号:US15091097
申请日:2016-04-05
Applicant: GRAND TEK ADVANCE MATERIAL SCIENCE CO., LTD.
Inventor: Hsueh-Tso LIN , Rui-Gang HOU , Dick ZHONG
IPC: B05D3/02 , C09D5/16 , B05D7/00 , C09D127/16
CPC classification number: B05D3/0254 , B05D5/083 , B05D7/50 , B05D7/52 , C09D5/1668 , C09D5/1693 , C09D127/16 , C08K5/3492 , C08L33/14 , C08L83/04
Abstract: A baking-type aqueous organic silicon fluorine-containing polymer paint is provided, which includes an aqueous organic silicon fluorine-containing polymer dispersion and a curing agent. The curing agent includes aqueous amino resin, aqueous isocyanate resin, or a combination thereof. In addition, the paint may further include an assist resin such as aqueous polyester resin, aqueous acrylic acid resin, aqueous epoxy resin, aqueous phenoxy resin, or a combination thereof.
-
-