Abstract:
A method of manufacturing a coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first PVF, 30-70 parts by weight of an assistance resin, 5-30 parts by weight of a curing agent, 100-120 parts by weight of a first latent solvent, 3-methoxy-3-methyl-1-butanol, and water. The first latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 60:10-20:40-60. The method also applies a finish paint on the primer paint, wherein the finish paint includes 100 parts by weight of a second PVF, 100-120 parts by weight of a second latent solvent, 3-methoxy-3-methyl-1-butanol, and water, wherein the second latent solvent, 3-methoxy-3-methyl-1-butanol, and water have a weight ratio of 50:10-20:30-60. The primer paint and the finish paint are baked and dried to form a coating.
Abstract:
An aqueous organic silicon fluoro-containing polymer dispersion is provided. The dispersion includes 100 parts by weight of poly(vinylidene difluoride-hexafluoropropylene), 10 to 30 parts by weight of organic silicon emulsion, and acrylate polymer. The acrylate polymer and the sum of the poly(vinylidene difluoride-hexafluoropropylene) and the organic silicon emulsion have a weight ratio of 30:100 to 50:100.
Abstract:
Polyphenylene ether resin composition includes 100 parts by weight of polyphenylene ether resin, 25 to 40 parts by weight of copolymer, and 0.01 to 0.02 parts by weight of initiator. The copolymer is (A) copolymer polymerized of (a) mono-functional monomer, (b1) bi-functional monomer, and (c) tri-functional monomer through radical polymerization, (B) copolymer polymerized of (a) mono-functional monomer and (b2) bi-functional monomer through radical polymerization, or (C) a combination thereof.
Abstract:
A method of manufacturing a bi-layered coating is provided, which includes applying a primer paint on a substrate, wherein the primer paint includes 100 parts by weight of a first polyvinyl fluoride, 20 to 50 parts by weight of an assistance resin, and 150 to 170 parts by weight of a first latent solvent, and wherein the assistance resin is polyester modified epoxy resin, polyester type polyurethane resin, phenoxy resin, or a combination thereof. The primer paint is baked and dried to form a primer coating. A finish paint is then applied onto the primer coating, wherein the finish paint includes 100 parts by weight of a second polyvinyl fluoride and 120 to 150 parts by weight of a second latent solvent. The finish paint is baked and dried to form a finish coating on the primer coating.
Abstract:
A baking-type aqueous organic silicon fluorine-containing polymer paint is provided, which includes an aqueous organic silicon fluorine-containing polymer dispersion and a curing agent. The curing agent includes aqueous amino resin, aqueous isocyanate resin, or a combination thereof. In addition, the paint may further include an assist resin such as aqueous polyester resin, aqueous acrylic acid resin, aqueous epoxy resin, aqueous phenoxy resin, or a combination thereof.
Abstract:
A ceramic paint is provided, which includes a mixture of a silica sol-gel, 20 to 60 parts by weight of filler, and 1 to 50 parts by weight of a fluorine-containing polymer, wherein the silica sol-gel is formed by reacting 100 parts by weight of silica sol, 50 to 100 parts by weight of organic silane, and 0.3 to 1 parts by weight of a catalyst.