    IPC分类号: B32B9/00

    摘要: A cutting tool made of a surface-coated cubic boron nitride-based ultra-high-pressure sintered material, comprising a cutting insert main body formed by ultra-high-pressure sintering of a compact composed of titanium nitride, aluminum and/or aluminum oxide, and boron nitride, and a hard coating layer vapor deposited on the main body. The main body has a texture containing cubic boron nitride, titanium nitride and reaction product. The hard coating layer has a lower layer of nitride having a composition of [Ti1-X-YAlXSiY]N, where X is in a range from 0.40 to 0.60 and Y is in a range from 0.02 to 0.10 in an atomic ratio, and the upper layer comprises a thin layer A having the composition of [Ti1-X-YAlXSiY]N, where X is in a range from 0.40 to 0.60 in an atomic ratio and Y is in a range from 0.02 to 0.10, and a thin layer B consisting of a Ti nitride (TiN). The upper layer consists of the thin layer A and a thin layer B layered alternately.

    摘要翻译: 一种由表面涂覆的立方氮化硼基超高压烧结材料制成的切削工具,包括通过超高压烧结由氮化钛,铝和/或氧化铝构成的压块形成的切削刀片主体 和氮化硼,以及沉积在主体上的硬涂层蒸气。 主体具有立方氮化硼,氮化钛和反应产物的纹理。 硬涂层具有下层的氮化物,其组成为[Ti 1 -Y 1 O X 1 Si Y N] N,其中X为 在0.40〜0.60的范围内,Y在原子比为0.02〜0.10的范围内,上层包含具有[Ti 1 -YY< SUB X X Si Y N,其中X在原子比为0.40-0.60的范围内,Y在0.02至0.10的范围内,薄层B由 Ti氮化物(TiN)。 上层由薄层A和交替层叠的薄层B组成。

    Cutting tool made of surface-coated cubic boron nitride-based ultra-high-pressure sintered material
    2.
    发明授权
    Cutting tool made of surface-coated cubic boron nitride-based ultra-high-pressure sintered material 有权
    由表面立方氮化硼型超高压烧结材料制成的切削刀具

    公开(公告)号:US07939186B2

    公开(公告)日:2011-05-10

    申请号:US11753053

    申请日:2007-05-24

    IPC分类号: B23B27/14

    摘要: A cutting tool made of a surface-coated cubic boron nitride-based ultra-high-pressure sintered material, comprising a cutting insert main body formed by ultra-high-pressure sintering of a compact composed of titanium nitride, aluminum and/or aluminum oxide, and boron nitride, and a hard coating layer vapor deposited on the main body. The main body has a texture containing cubic boron nitride, titanium nitride and reaction product. The hard coating layer has a lower layer of nitride having a composition of [Ti1 -X-YAlXSiY]N, where X is in a range from 0.40 to 0.60 and Y is in a range from 0.02 to 0.10 in an atomic ratio, and the upper layer comprises a thin layer A having the composition of [Ti1-X-YAlXSiY]N, where X is in a range from 0.40 to 0.60 in an atomic ratio and Y is in a range from 0.02 to 0.10, and a thin layer B consisting of a Ti nitride (TiN). The upper layer consists of the thin layer A and a thin layer B layered alternately.

    摘要翻译: 一种由表面涂覆的立方氮化硼基超高压烧结材料制成的切削工具,包括通过超高压烧结由氮化钛,铝和/或氧化铝构成的压块形成的切削刀片主体 和氮化硼,以及沉积在主体上的硬涂层蒸气。 主体具有立方氮化硼,氮化钛和反应产物的纹理。 硬涂层具有[Ti1-X-YAlXSiY] N组成的下层氮化物,其中X在0.40〜0.60的范围内,Y在原子比为0.02〜0.10的范围内, 上层包括具有[Ti1-X-YAlXSiY] N组成的薄层A,其中X在原子比范围内在0.40至0.60的范围内,Y在0.02至0.10的范围内,薄层B 由Ti氮化物(TiN)组成。 上层由薄层A和交替层叠的薄层B组成。

    Production method of fine grain polycrystalline diamond compact
    3.
    发明申请
    Production method of fine grain polycrystalline diamond compact 有权
    精细晶粒多晶金刚石复合体的生产方法

    公开(公告)号:US20110241266A1

    公开(公告)日:2011-10-06

    申请号:US13064470

    申请日:2011-03-28

    IPC分类号: C04B35/64

    摘要: [Problem] This invention aims to provide a production method of a fine grain polycrystalline diamond compact which is suitable for finishing cutting tool materials and/or ultra-precision machining tool materials. In the method, a freeze-drying process for preventing the growth of secondary particle formation is unnecessary, and an aid does not need to be mixed in advance.[Means for Resolution] Disclosed is a following production method of a fine grain polycrystalline diamond compact. Each of carbonate and a C—H based organic compound which is a solid at room temperature, is sandwiched between diamond powder layers to stack them up in layers in a Ta capsule. Particle size of the diamond powder is 4 μm or less in average; and the organic compound is preferably one or more selected from among polyethylene, polypropylene and polystyrene. The layers in the capsule are sintered under the conditions of a pressure of 7.7 GPa or higher and a temperature of 2000° C. or higher.In the method, diamond powder as a raw material for sintering is prepared without any freeze-drying process; also the pre-mixture of an aid and an oxalic acid dihydrate which is a hazardous material, is not required.

    摘要翻译: 本发明旨在提供一种适用于精加工刀具材料和/或超精密加工工具材料的细晶粒多晶金刚石复合体的制造方法。 在该方法中,不需要用于防止二次粒子形成生长的冷冻干燥过程,并且不需要预先混合。 [解决方法]公开了以下的细晶粒多晶金刚石复合体的制造方法。 碳酸盐和C-H基有机化合物在室温下为固体,被夹在金刚石粉末层之间,以便在Ta胶囊中层叠。 金刚石粉末的粒径平均为4μm以下; 有机化合物优选为聚乙烯,聚丙烯,聚苯乙烯等中的1种以上。 胶囊中的层在7.7GPa以上的压力和2000℃以上的温度的条件下烧结。 在该方法中,制备作为烧结原料的金刚石粉末,无需任何冷冻干燥工艺; 也不需要辅助剂和作为有害物质的草酸二水合物的预混合物。

    METHOD FOR PRODUCING SINTERED CUBIC BORON NITRIDE COMPACT
    5.
    发明申请
    METHOD FOR PRODUCING SINTERED CUBIC BORON NITRIDE COMPACT 有权
    生产烧结陶瓷氮化物复合材料的方法

    公开(公告)号:US20110192093A1

    公开(公告)日:2011-08-11

    申请号:US13022834

    申请日:2011-02-08

    IPC分类号: B01J3/06 C04B35/5831 B24D3/00

    摘要: A method for producing a highly uniform and highly dense sintered cubic boron nitride compact having high hardness by sintering at a milder condition without a binder, is provided. The method includes deflocculating secondary particles in cubic boron nitride starting powders by dispersing the starting powders in a solution of a deflocculant; molding the green compact after removing the solution of the deflocculant from the starting powders; and then sintering the green compact in the presence of a supercritical fluid source in a supercritical state by pressing and heating the green compact together with the supercritical fluid source. The supercritical fluid source can be one or more selected from a group consisted of polyvinylidene chloride, polyvinyl chloride, polyethylene, polypropylene, polystyrene, a polyester and an ABS resin. In the sintering, the pressure is 5 GPa or higher, and the temperature is 1400° C. or higher. According to the method, a highly uniform and highly dense sintered cubic boron nitride sintered compact having high hardness, can be obtained.

    摘要翻译: 提供了一种通过在较温和的条件下烧结而不用粘合剂来制造具有高硬度的高均匀高密度烧结立方氮化硼压块的方法。 该方法包括通过将起始粉末分散在抗絮凝剂溶液中来使立方氮化硼起始粉末中的二次粒子脱絮凝; 在从起始粉末中除去抗絮凝剂的溶液之后,模压生坯; 然后在超临界状态的超临界流体源的存在下,通过与超临界流体源一起压制和加热生坯,来烧结生坯。 超临界流体源可以是选自聚偏二氯乙烯,聚氯乙烯,聚乙烯,聚丙烯,聚苯乙烯,聚酯和ABS树脂中的一种或多种。 烧结时的压力为5GPa以上,温度为1400℃以上。 根据该方法,可以获得具有高硬度的高度均匀且高密度的烧结立方氮化硼烧结体。

    Method for producing sintered cubic boron nitride compact
    6.
    发明授权
    Method for producing sintered cubic boron nitride compact 有权
    立方氮化硼烧结体的制造方法

    公开(公告)号:US08657893B2

    公开(公告)日:2014-02-25

    申请号:US13022834

    申请日:2011-02-08

    摘要: A method for producing a highly uniform and highly dense sintered cubic boron nitride compact having high hardness by sintering at a milder condition without a binder, is provided. The method includes deflocculating secondary particles in cubic boron nitride starting powders by dispersing the starting powders in a solution of a deflocculant; molding the green compact after removing the solution of the deflocculant from the starting powders; and then sintering the green compact in the presence of a supercritical fluid source in a supercritical state by pressing and heating the green compact together with the supercritical fluid source. The supercritical fluid source can be one or more selected from a group consisted of polyvinylidene chloride, polyvinyl chloride, polyethylene, polypropylene, polystyrene, a polyester and an ABS resin. In the sintering, the pressure is 5 GPa or higher, and the temperature is 1400° C. or higher. According to the method, a highly uniform and highly dense sintered cubic boron nitride sintered compact having high hardness, can be obtained.

    摘要翻译: 提供了一种通过在较温和的条件下烧结而不用粘合剂来制造具有高硬度的高均匀高密度烧结立方氮化硼压块的方法。 该方法包括通过将起始粉末分散在抗絮凝剂溶液中来使立方氮化硼起始粉末中的二次粒子脱絮凝; 在从起始粉末中除去抗絮凝剂的溶液之后,模压生坯; 然后在超临界状态的超临界流体源的存在下,通过与超临界流体源一起压制和加热生坯,来烧结生坯。 超临界流体源可以是选自聚偏二氯乙烯,聚氯乙烯,聚乙烯,聚丙烯,聚苯乙烯,聚酯和ABS树脂中的一种或多种。 烧结时的压力为5GPa以上,温度为1400℃以上。 根据该方法,可以获得具有高硬度的高度均匀且高密度的烧结立方氮化硼烧结体。

    Production method of fine grain polycrystalline diamond compact
    8.
    发明授权
    Production method of fine grain polycrystalline diamond compact 有权
    精细晶粒多晶金刚石复合体的生产方法

    公开(公告)号:US08753562B2

    公开(公告)日:2014-06-17

    申请号:US13064470

    申请日:2011-03-28

    摘要: [Problem]This invention aims to provide a production method of a fine grain polycrystalline diamond compact which is suitable for finishing cutting tool materials and/or ultra-precision machining tool materials. In the method, a freeze-drying process for preventing the growth of secondary particle formation is unnecessary, and an aid does not need to be mixed in advance.[Means for Resolution]Disclosed is a following production method of a fine grain polycrystalline diamond compact. Each of carbonate and a C—H based organic compound which is a solid at room temperature, is sandwiched between diamond powder layers to stack them up in layers in a Ta capsule. Particle size of the diamond powder is 4 μm or less in average; and the organic compound is preferably one or more selected from among polyethylene, polypropylene and polystyrene. The layers in the capsule are sintered under the conditions of a pressure of 7.7 GPa or higher and a temperature of 2000° C. or higher.In the method, diamond powder as a raw material for sintering is prepared without any freeze-drying process; also the pre-mixture of an aid and an oxalic acid dihydrate which is a hazardous material, is not required.

    摘要翻译: 本发明旨在提供一种适用于精加工刀具材料和/或超精密加工工具材料的细晶粒多晶金刚石复合体的制造方法。 在该方法中,不需要用于防止二次粒子形成生长的冷冻干燥过程,并且不需要预先混合。 [解决方法]公开了以下的细晶粒多晶金刚石复合体的制造方法。 碳酸盐和C-H基有机化合物在室温下为固体,被夹在金刚石粉末层之间,以便在Ta胶囊中层叠。 金刚石粉末的粒径平均为4μm以下; 有机化合物优选为聚乙烯,聚丙烯,聚苯乙烯等中的1种以上。 胶囊中的层在7.7GPa以上的压力和2000℃以上的温度的条件下烧结。 在该方法中,制备作为烧结原料的金刚石粉末,无需任何冷冻干燥工艺; 也不需要辅助剂和作为有害物质的草酸二水合物的预混合物。