Negative electrode for nonaqueous secondary battery
    1.
    发明授权
    Negative electrode for nonaqueous secondary battery 失效
    非水二次电池用负极

    公开(公告)号:US07838154B2

    公开(公告)日:2010-11-23

    申请号:US11174645

    申请日:2005-07-06

    IPC分类号: H01M4/80

    摘要: A negative electrode 10 for a nonaqueous secondary battery, has an active material layer 2 containing active material particles 2a. The active material layer 2 has a metallic material 4 deposited among the particles by electroplating. The negative electrode 10 has a large number of holes 5 open on at least one side thereof and extending through the thickness of the active material layer. The negative electrode 10 further has a pair of current collecting layers 3a and 3b adapted to be brought into contact with an electrolyte. The active material layer 2 is between the current collecting layers 3a and 3b. The holes 5 open on the negative electrode 10 preferably have an opening area ratio of 0.3% to 30%. At least one of the pair of the current collecting layers 3a and 3b preferably has a thickness of 0.3 to 10 μm.

    摘要翻译: 非水系二次电池用负极10具有含有活性物质粒子2a的活性物质层2。 活性物质层2具有通过电镀沉积在颗粒之间的金属材料4。 负极10具有在其至少一个侧面上开口并且延伸穿过活性材料层的厚度的大量孔5。 负极10还具有适于与电解液接触的一对集流层3a和3b。 活性物质层2位于集流层3a和3b之间。 在负极10上打开的孔5的开口面积比优选为0.3%〜30%。 一对集电层3a和3b中的至少一个优选具有0.3至10μm的厚度。

    Process of producing nonaqueous secondary battery
    7.
    发明申请
    Process of producing nonaqueous secondary battery 审中-公开
    生产非水二次电池的方法

    公开(公告)号:US20090070988A1

    公开(公告)日:2009-03-19

    申请号:US11920646

    申请日:2005-12-08

    IPC分类号: H01M10/04

    摘要: A process of producing a nonaqueous secondary battery comprising the steps of disposing a separator between a member containing a silicon-based material and a positive electrode, together with interposing a metallic lithium layer between the separator and the member to obtain an assembly, and aging the resulting assembly for a prescribed period of time to alloy lithium with the silicon-based material. Lithium alloying is preferably performed to a degree such that the amount of lithium in the silicon-based material is 5% to 50% based on the theoretical initial charge capacity of silicon. When the positive electrode has a lithium-containing active material for positive electrode, lithium alloying is preferably performed to a degree satisfying formula (1): 4.4A−B≧C, where A is the number of moles of silicon in the member containing the silicon-based material; B is the number of moles of lithium in the lithium-containing active material for positive electrode; and C is the number of moles of lithium to be alloyed.

    摘要翻译: 一种非水系二次电池的制造方法,其特征在于,包括以下步骤:在含硅基材料的构件和正极之间设置隔板,并在隔膜和构件之间插入金属锂层,得到组装体,并使其老化 在合适的时间内将锂合金与硅基材料合并。 锂合金化优选以使得硅基材料中的锂的量基于硅的理论初始充电容量为5%至50%的程度进行。 当正极具有用于正极的含锂活性材料时,锂合金化优选进行到满足公式(1)的程度:4.4AB> = C,其中A是含有硅的构件中的硅的摩尔数 的材料; B是正极用含锂活性物质中的锂的摩尔数; C是要合金化的锂的摩尔数。

    Negative electrode for nonaqueous secondary battery
    9.
    发明申请
    Negative electrode for nonaqueous secondary battery 失效
    非水二次电池用负极

    公开(公告)号:US20060051677A1

    公开(公告)日:2006-03-09

    申请号:US11174645

    申请日:2005-07-06

    IPC分类号: H01M4/80 H01M4/40

    摘要: A negative electrode 10 for a nonaqueous secondary battery, has an active material layer 2 containing active material particles 2a. The active material layer 2 has a metallic material 4 deposited among the particles by electroplating. The negative electrode 10 has a large number of holes 5 open on at least one side thereof and extending through the thickness of the active material layer. The negative electrode 10 further has a pair of current collecting layers 3a and 3b adapted to be brought into contact with an electrolyte. The active material layer 2 is between the current collecting layers 3a and 3b. The holes 5 open on the negative electrode 10 preferably have an opening area ratio of 0.3% to 30%. At least one of the pair of the current collecting layers 3a and 3b preferably has a thickness of 0.3 to 10 μm.

    摘要翻译: 非水系二次电池用负极10具有包含活性物质粒子2a的活性物质层2。 活性物质层2具有通过电镀沉积在颗粒之间的金属材料4。 负极10具有在其至少一个侧面上开口并且延伸穿过活性材料层的厚度的大量孔5。 负极10还具有适于与电解质接触的一对集流层3a和3b。 活性物质层2位于集流层3a和3b之间。 在负极10上打开的孔5的开口面积比优选为0.3%〜30%。 一对集电层3a和3b中的至少一个优选具有0.3至10μm的厚度。

    Negative electrode for nonaqueous secondary battery
    10.
    发明授权
    Negative electrode for nonaqueous secondary battery 有权
    非水二次电池用负极

    公开(公告)号:US08197966B2

    公开(公告)日:2012-06-12

    申请号:US12306973

    申请日:2007-04-18

    IPC分类号: H01M2/16

    摘要: A negative electrode 10 for a nonaqueous secondary battery has an active material layer 12 containing active material particles 12a. The particles 12a are coated at least partially with a metallic material 13 having low capability of lithium compound formation. The active material layer 12 has voids located between the metallic material-coated particles 12a with a void fraction of 15% to 45%. The metallic material 13 on the surface of the particles is preferably present throughout the thickness of the active material layer. The active material particles 12a are preferably of a silicon-based material. The active material layer 12 preferably contains 1% to 3% by weight of an electroconductive carbon material based on the weight of the active material particles 12a.

    摘要翻译: 非水系二次电池用负极10具有含有活性物质粒子12a的活性物质层12。 颗粒12a至少部分地被具有低的锂化合物形成能力的金属材料13涂覆。 活性物质层12具有位于金属材料涂覆颗粒12a之间的空隙,空隙率为15%至45%。 颗粒表面上的金属材料13优选存在于活性材料层的整个厚度上。 活性物质粒子12a优选为硅系材料。 基于活性物质颗粒12a的重量,活性物质层12优选含有1重量%至3重量%的导电碳材料。