摘要:
A method for producing a base oil for lubricant oils comprising: a first step of hydrocracking a stock oil having a content percentage of a heavy matter of 80% by mass or more so that a crack per mass of the heavy matter is 20 to 85% by mass, to obtain a hydrocracked oil comprising the heavy matter and a hydrocracked product thereof, a second step of fractionating the hydrocracked oil into a base oil fraction comprising the hydrocracked product and a heavy fraction comprising the heavy matter and being heavier than the base oil fraction, respectively, a third step of isomerization dewaxing the base oil fraction from the fractionation in the second step to obtain a dewaxed oil, wherein the heavy fraction from the fractionation in the second step is returned to the first step as a part of the stock oil.
摘要:
A method for producing a hydroisomerization catalyst includes a first step of preparing a support precursor by heating a mixture containing an ion-exchanged zeolite and a binder, the ion-exchanged zeolite being prepared by ion-exchanging an organic template-containing zeolite which contains an organic template and has a one-dimensional pore structure including a 10-membered ring in a solution containing ammonium ions and/or protons, at a temperature of 250 to 350° C. under N2 atmosphere, and a second step of preparing a hydroisomerization catalyst, which is prepared by calcining a catalyst precursor, the catalyst precursor being prepared based on the support precursor containing a platinum salt and/or a palladium salt, at a temperature of 350 to 400° C. in an atmosphere containing molecular oxygen, the hydroisomerization catalyst containing a support which includes a zeolite and carries platinum and/or palladium.
摘要:
A method for producing a hydroisomerization catalyst includes a first step of preparing a support precursor by heating a mixture containing an ion-exchanged zeolite and a binder, the ion-exchanged zeolite being prepared by ion-exchanging an organic template-containing zeolite which contains an organic template and has a one-dimensional pore structure including a 10-membered ring in a solution containing ammonium ions and/or protons, at a temperature of 250 to 350° C. under N2 atmosphere, and a second step of preparing a hydroisomerization catalyst, which is prepared by calcining a catalyst precursor, the catalyst precursor being prepared based on the support precursor containing a platinum salt and/or a palladium salt, at a temperature of 350 to 400° C. in an atmosphere containing molecular oxygen, the hydroisomerization catalyst containing a support which includes a zeolite and carries platinum and/or palladium.