摘要:
A method for producing a lubricant base oil, the method comprising a first step of fractionating, from a hydrocarbon oil containing a base oil fraction and a heavy fraction that is heavier than the base oil fraction, the base oil fraction and the heavy fraction, and a second step of obtaining a dewaxed oil by isomerization and dewaxing of the base oil fraction fractionated in the first step, wherein a hydrocracked oil obtained by hydrocracking the heavy fraction fractionated in the first step is returned to the first step.
摘要:
A process for producing a Fischer-Tropsch synthesis catalyst according to the present invention comprises a step of calcining a carrier precursor containing silica calcined at a temperature T1 and a zirconium compound at a temperature T2 to obtain a carrier; and a step of calcining a catalyst precursor containing the carrier and a cobalt compound and/or a ruthenium compound at a temperature T3, wherein the content of the zirconium compound in the carrier precursor is 0.01 to 7% by mass in terms of zirconium oxide based on the total mass of the catalyst, and T1, T2, and T3 satisfy conditions represented by expressions (1) to (3): T1≧T3 (1) 250° C.≦T2≦450° C. (2) 250° C.≦T3≦450° C. (3).
摘要:
A method for producing a hydroisomerization catalyst according to the present invention includes: a first step of preparing a catalyst to be treated, which contains a support having a one-dimensional porous structure including a 10-membered ring and at least one metal selected from the group consisting of: group 8 to 10 metals of the periodic table, Mo, and W supported on the hydroisomerization catalyst; and a second step of producing a hydroisomerization catalyst having a carbon content of 0.4 to 2.5% by mass by subjecting the catalyst to be treated to a coking treatment by means of a carbon-containing compound.
摘要:
A method for producing a lubricant base oil that has a predetermined boiling point range, the method including a first step of bringing a feedstock containing a first hydrocarbon oil having a boiling point in the above boiling point range and a second hydrocarbon oil having a lower boiling point than the boiling point range into contact with a hydroisomerization catalyst, wherein the catalyst contains a support that includes a zeolite having a one-dimensional porous structure including a 10-membered ring and a binder, and platinum and/or palladium supported on the support.
摘要:
A method for producing a lubricant base oil which comprises a first step of carrying out isomerization dewaxing by contacting, in the presence of hydrogen, a hydrocarbon oil containing normal paraffin having a boiling point of 360° C. or higher, with a hydroisomerization catalyst under conditions such that a cracking rate defined in the following formula (1) is 10 mass % or less, and a second step of carrying out the above isomerization dewaxing by temporarily switching the above conditions to conditions such that the cracking rate is 13 mass % or more. Cracking rate (mass %)=[(C1−C2)/C1]×100 (1) wherein C1 represents the mass ratio of a fraction having a boiling point of 360° C. or higher in the above hydrocarbon oil, and C2 represents the mass ratio of the fraction having a boiling point of 360° C. or higher in the above hydrocarbon oil after the isomerization dewaxing.
摘要:
A method for producing a lubricant base oil, the method comprising a first step of fractionating, from a hydrocarbon oil containing a base oil fraction and a heavy fraction that is heavier than the base oil fraction, the base oil fraction and the heavy fraction, and a second step of obtaining a dewaxed oil by isomerization and dewaxing of the base oil fraction fractionated in the first step, wherein a hydrocracked oil obtained by hydrocracking the heavy fraction fractionated in the first step is returned to the first step.
摘要:
A method for producing a hydroisomerization catalyst according to the present invention includes: a first step of preparing a catalyst to be treated, which contains a support having a one-dimensional porous structure including a 10-membered ring and at least one metal selected from the group consisting of: group 8 to 10 metals of the periodic table, Mo, and W supported on the hydroisomerization catalyst; and a second step of producing a hydroisomerization catalyst having a carbon content of 0.4 to 2.5% by mass by subjecting the catalyst to be treated to a coking treatment by means of a carbon-containing compound.
摘要:
A Fischer-Tropsch synthesis catalyst containing 10 to 30% by mass, as a metal atom, of metallic cobalt and/or cobalt oxide, based on the mass of the catalyst, supported on a carrier containing silica, in which the carrier has an average pore diameter of 8 to 25 nm and the metallic cobalt and/or cobalt oxide has an average crystallite diameter of not less than the average pore diameter of the carrier and less than 35 nm.
摘要:
A method for producing a base oil for lubricant oils comprising: a first step of hydrocracking a stock oil having a content percentage of a heavy matter of 80% by mass or more so that a crack per mass of the heavy matter is 20 to 85% by mass, to obtain a hydrocracked oil comprising the heavy matter and a hydrocracked product thereof, a second step of fractionating the hydrocracked oil into a base oil fraction comprising the hydrocracked product and a heavy fraction comprising the heavy matter and being heavier than the base oil fraction, respectively, a third step of isomerization dewaxing the base oil fraction from the fractionation in the second step to obtain a dewaxed oil, wherein the heavy fraction from the fractionation in the second step is returned to the first step as a part of the stock oil.
摘要:
A method for producing a hydroisomerization catalyst includes a first step of preparing a support precursor by heating a mixture containing an ion-exchanged zeolite and a binder, the ion-exchanged zeolite being prepared by ion-exchanging an organic template-containing zeolite which contains an organic template and has a one-dimensional pore structure including a 10-membered ring in a solution containing ammonium ions and/or protons, at a temperature of 250 to 350° C. under N2 atmosphere, and a second step of preparing a hydroisomerization catalyst, which is prepared by calcining a catalyst precursor, the catalyst precursor being prepared based on the support precursor containing a platinum salt and/or a palladium salt, at a temperature of 350 to 400° C. in an atmosphere containing molecular oxygen, the hydroisomerization catalyst containing a support which includes a zeolite and carries platinum and/or palladium.