摘要:
An earth-boring bit, and a method of increasing the durability of the same, which includes the step providing a pliable sheet of a hardfacing matrix material. The pliable sheet of hardfacing material has a nickel and chromium matrix combined with a first element. The first element is selected from a group consisting of spherical sintered tungsten carbide, spherical cast tungsten carbide, and metallic glass. The hardfacing matrix material sheet is placed on a preselected surface of the drill bit. The hardfacing matrix material sheet is then fusion bonded to the drill bit.
摘要:
Earth-boring rotary drill bits include bit bodies comprising a composite material including a plurality of hard phase regions or particles dispersed throughout a titanium or titanium-based alloy matrix material. The bits further include a cutting structure disposed on a face of the bit body. In some embodiments, the bit bodies may include a plurality of regions having differing material compositions. For example, the bit bodies may include a first region comprising a plurality of hard phase regions or particles dispersed throughout a titanium or titanium-based alloy matrix material, and a second region comprising a titanium or a titanium-based alloy material. Methods for forming such drill bits include at least partially sintering a plurality of hard particles and a plurality of particles comprising titanium or a titanium-based alloy material to form a bit body comprising a particle-matrix composite material. A shank may be attached directly to the bit body.
摘要:
Rotary drill bits for drilling subterranean formations include a bit body and at least one cutting structure disposed on a face thereof. The bit body includes a crown region comprising a particle-matrix composite material that includes a plurality of boron carbide particles dispersed throughout an aluminum or aluminum-based alloy matrix material. In some embodiments, the matrix material may include a continuous solid solution phase and a discontinuous precipitate phase. Methods of manufacturing rotary drill bits for drilling subterranean formations include infiltrating a plurality of boron carbide particles with a molten aluminum or aluminum-based material. In additional methods, a green powder component is provided that includes a plurality of particles each comprising boron carbide and a plurality of particles each comprising aluminum or an aluminum-based alloy material. The green powder component is at least partially sintered to provide a bit body, and a shank is attached to the bit body.
摘要:
The present invention relates to compositions and methods for forming a bit body for an earth-boring bit. The bit body may comprise hard particles, wherein the hard particles comprise at least one carbide, nitride, boride, and oxide and solid solutions thereof, and a binder binding together the hard particles. The binder may comprise at least one metal selected from cobalt, nickel, and iron, and, optionally, at least one melting point reducing constituent selected from a transition metal carbide in the range of 30 to 60 weight percent, boron up to 10 weight percent, silicon up to 20 weight percent, chromium up to 20 weight percent, and manganese up to 25 weight percent, wherein the weight percentages are based on the total weight of the binder. In addition, the hard particles may comprise at least one of (i) cast carbide (WC+W2C) particles, (ii) transition metal carbide particles selected from the carbides of titanium, chromium, vanadium, zirconium, hafnium, tantalum, molybdenum, niobium, and tungsten, and (iii) sintered cemented carbide particles.
摘要:
The present invention relates to compositions and methods for forming a bit body for an earth-boring bit. The bit body may comprise hard particles, wherein the hard particles comprise at least one carbide, nitride, boride, and oxide and solid solutions thereof, and a binder binding together the hard particles. The binder may comprise at least one metal selected from cobalt, nickel, and iron, and, optionally, at least one melting point reducing constituent selected from a transition metal carbide in the range of 30 to 60 weight percent, boron up to 10 weight percent, silicon up to 20 weight percent, chromium up to 20 weight percent, and manganese up to 25 weight percent, wherein the weight percentages are based on the total weight of the binder. In addition, the hard particles may comprise at least one of (i) cast carbide (WC+W2C) particles, (ii) transition metal carbide particles selected from the carbides of titanium, chromium, vanadium, zirconium, hafnium, tantalum, molybdenum, niobium, and tungsten, and (iii) sintered cemented carbide particles.
摘要:
Methods of forming bit bodies for earth-boring bits include assembling green components, brown components, or fully sintered components, and sintering the assembled components. Other methods include isostatically pressing a powder to form a green body substantially composed of a particle-matrix composite material, and sintering the green body to provide a bit body having a desired final density. Methods of forming earth-boring bits include providing a bit body substantially formed of a particle-matrix composite material and attaching a shank to the body. The body is provided by pressing a powder to form a green body and sintering the green body. Earth boring Earth-boring bits include a unitary structure substantially formed of a particle-matrix composite material. The unitary structure includes a first region configured to carry cutters and a second region that includes a threaded pin. Earth-boring bits include a shank attached directly to a body substantially formed of a particle-matrix composite material.
摘要:
Methods of forming earth-boring rotary drill bits include providing a bit body, providing a shank that is configured for attachment to a drill string, and attaching the shank to the bit body. Providing a bit body includes providing a green powder component having a first region having a first composition and a second region having a second, different composition, and at least partially sintering the green powder component. Other methods include providing a powder mixture, pressing the powder mixture to form a green component, and sintering the green component to a final density. A shank is provided that includes an aperture, and a feature is machined in a surface of the bit body. The aperture is aligned with the feature, and a retaining member is inserted through the aperture. An earth-boring bit includes a bit body comprising a particle-matrix composite material including a plurality of hard particles dispersed throughout a matrix material. A shank is attached to the bit body using a retaining member.
摘要:
A rotary drill bit includes a bit body substantially formed of a particle-matrix composite material having an exterior surface and an abrasive wear-resistant material disposed on at least a portion of the exterior surface of the bit body. Methods for applying an abrasive wear-resistant material to a surface of a drill bit are also provided.
摘要:
A method of making an earth-boring rotary drill bit including a bit body configured to carry one or more cutters for engaging a subterranean earth formation. The method includes providing a plurality of hard particles in a mold to define a particle precursor of the bit body. The method also includes infiltrating the particle precursor of the bit body with a molten matrix material comprising a shape memory alloy forming a hard particle-molten matrix material mixture, wherein the hard particles are randomly dispersed within the molten matrix material. The method further includes cooling the molten matrix material to solidify a matrix material and form the bit body comprising a particle-matrix composite material having the plurality of hard particles randomly dispersed throughout the matrix material.
摘要:
An earth-boring rotary drill bit includes a bit body configured to carry one or more cutters for engaging a subterranean earth formation, the bit body comprising a particle-matrix composite material having a plurality of hard particles dispersed throughout a matrix material, the matrix material comprising a shape memory alloy. The matrix material comprises a metal alloy configured to undergo a reversible phase transformation between an austenitic phase and a martensitic phase. The matrix material may include an Ni-based alloy, Cu-based alloy, Co-based alloy, Fe-based alloy or Ti-based alloy. The drill bit may be made by a method that includes: providing a plurality of hard particles in a mold to define a particle precursor of the bit body; infiltrating the particle precursor of the bit body with a molten matrix material comprising a shape memory alloy forming a particle-matrix mixture; and cooling the molten particle-matrix mixture to solidify the matrix material and forming a bit body having a particle-matrix composite material comprising a shape memory alloy.