Mineral wool, insulating product and production method
    1.
    发明授权
    Mineral wool, insulating product and production method 有权
    矿棉,绝缘产品及生产方法

    公开(公告)号:US08877102B2

    公开(公告)日:2014-11-04

    申请号:US11910325

    申请日:2006-03-31

    摘要: The invention relates to thermally-stable mineral wool which can dissolve in a physiological medium, comprising fibres containing the following constituents, expressed in percentage by weight, namely: 35-60 % SiO2, preferably 39-55 %; 12-27% Al2O3, preferably 16-25%; 0-35% CaO, preferably 3-25%; 0-30% MgO, preferably 0-15%; 0-17% Na2O, preferably 6-12%; 0-17% K2O, preferably 3-12%; 10-17% R2O (Na2O+K2O), preferably 12-17%; 0-5% P2O5, preferably 0-2%; 0-20% Fe2O3; 0-8% B2O3, preferably 0-4%; and 0-3% TiO2, and at least one phosphorous compound that can react with said fibres at a temperature of less than 1000° C. in order to form a coating on the surface thereof. The invention is characterised in that the phosphorous content of said compound, as expressed in phosphorus atom weight, varies between 0.0005%, in particular more than 0.01%, and 1%, in particular less than 0.5%, of the total weight of the fibres. The invention is also characterised in that a phosphorus compound is a molecule in which the phosphorus atom(s) are bound to at least one carbon atom either directly or by means of an oxygen atom.

    摘要翻译: 本发明涉及能够溶解在生理介质中的热稳定矿棉,其包含以重量百分比表示的含有以下组分的纤维,即:35-60%SiO 2,优选39-55%; 12-27%Al2O3,优选16-25%; 0-35%CaO,优选3-25%; 0-30%MgO,优选0-15%; 0-17%Na 2 O,优选6-12%; 0-17%K2O,优选3-12%; 10-17%R 2 O(Na 2 O + K 2 O),优选12-17%; 0-5%P2O5,优选0-2%; 0-20%Fe2O3; 0-8%B2O3,优选0-4%; 和0-3%的TiO 2,以及至少一种能在低于1000℃的温度下与所述纤维反应的磷化合物,以在其表面上形成涂层。 本发明的特征在于,以磷原子重量表示的所述化合物的磷含量在纤维总重量的0.0005%,特别是大于0.01%和1%,特别是小于0.5%之间变化 。 本发明的特征还在于磷化合物是其中磷原子直接或通过氧原子结合至少一个碳原子的分子。