摘要:
The surface of a continuous web, the fibrous portion of which consists of papermaking fibres, is coated with a coating powder. The web is allowed to move between electrodes, which are in different potentials. A coating powder of inorganic material and polymeric binder material is applied on the surface of the web by utilizing the difference in the electric potential. The coated surface of the web is then finished. The coating powder comprises 10.1-99.5 wt.-% of inorganic material. A dry surface treated sheet material is thus formed.
摘要:
A film is formed on a planar surface by applying a granular layer on the planar surface by using electrostatic forces, and then finishing the granular layer to form the film. A converting line may be rebuilt to have devices employing this method. A multilayer sheet-like product comprising a film layer may be produced.
摘要:
The surface of a web is coated with a dry coating powder. The coating powder has inorganic material and polymeric binder material. The polymeric binder material is selected in such a manner that when increasing the temperature above the glass transition temperature the ratio G″/G′ is at the most equal to the ratio G″/G′ in the glass transition temperature.
摘要:
A method and assemby is disclosed for manufacturing a two-layer coated paper web, the method comprising the steps of applying a coating furnish layer to at least one surface of said paper web, drying the applied coating furnish layer to a point allowing a next coating layer to be applied thereon. Onto the first coating layer is applied a second coating layer that is dried. The application of successive coating layers is continued until the desired coat thickness is attained. The coating layers are applied using a metering film transfer method operating without leveling of the applied coating layer by doctoring, whereby in at least one of said coating layers is used a furnish having a solids content of not less than 62%.
摘要:
A web of paper or paperboard is manufactured by first forming a base web that is dried on the press section of papermaking machine. The base web is further dried on the dryer section of the papermaking machine and a base web speed differential, or draw, is set between the press section and the first dryer cylinder group of the dryer section, whereupon at least one surface of the web is surface sized. The draw is set to 3% maximum, and a surface size furnish is applied having a solids content of at least 15% of the total amount of size components and liquid in the furnish.
摘要:
A paper machine for the manufacture of LWC printing paper which is coated once has a headbox (100), a gap former (200), a press section (300) having at least one extended nip press, a pre-dryer section (400) in which a web (W) is dried applying at least cylinder drying (R1-R7), a precalender (500) in which the web (W) is pre-calendered, at least one portion which is formed of a coating station (600) and an after-dryer section (700) and in which the web (W) is coated on both sides applying a film coating method or a non-contact coating method and dried applying at least contact-free drying (710), an end calender (800) in which the web (W) is calendered, and a reel-up (900) in which the web (W) is reeled. The pre-calender (500) is a calender which is provided with at least one nip (NE1, NE2) and in which both surfaces of the web are in contact with a calendering backup surface having a surface temperature of at least 200° C., advantageously at least 250° C., the total length of the nip or nips of the pre-calender is in a range of 15-600 mm, advantageously in a range of 30-600 mm, the linear load of each nip is in a range of 50-500 kN/m, advantageously in a range of 100-400 kN/m, and the moisture content of the web before the first nip of the pre-calender (500) is in a range of 5-20%, advantageously in a range of 6-15%.
摘要:
A method is disclosed for manufacturing a surface sized web of paper or paperboard, the method comprising the step of applying to at least one side of the web an aqueous furnish of size. According to the method, the solids content of the size furnish being applied is at least 15% and the size frunish is applied to one side of the web by an amount not greater than 5 g/m2 as aqueous furnish of size applied to the web.
摘要翻译:公开了一种用于制造表面尺寸的纸或纸板网的方法,该方法包括将纤维素的至少一侧施加到尺寸的含水配料的步骤。 根据该方法,所施加的尺寸配料的固体含量为至少15%,并且将尺寸不均匀度施加到纤维网的一侧,其量不得大于5g / m 2,作为施加的尺寸的含水配料 到网络