摘要:
The alternate soaking apparatus for treatment of tissue materials has a plurality of chemical liquid containers, a treatment container for soaking and treating a tissue material, a plurality of liquid feed tubes for providing fluid communication between the corresponding chemical liquid containers and the treatment container to introduce the respective chemical liquids into the treatment container, a liquid discharge tube for discharging the chemical liquids in the treatment container, and control means for controllably opening and closing the liquid feed tubes and the liquid discharge tube to allow the plurality of chemical liquids to be contained in the treatment container individually and alternately. A tissue material is treated using the above alternate soaking apparatus under the condition that one of chemical liquids is an aqueous solution containing calcium, and another one of chemical liquids is an aqueous solution containing phosphoric acid, so as to form a calcium phosphate compound on the surface of and in the inside of the treated tissue material. The present invention allows a ligament material and to be automatically synthesized with a calcium phosphate-based compound in a shorter time-period by a limited number of members during the operation while securing an aseptic condition.
摘要:
Provision of a porous ceramic material which rapidly induces bone tissue formation and has practical strength.A porous ceramic material 11 having substantially unidirectionally oriented pores 12, a porosity of 40-90%, and an average open area of one pore of 0.05×10−3-50×10−3 mm2 both in a first sectional surface perpendicular to the pore 12 orientation direction and a second sectional surface parallel to the first sectional surface and 5 mm distant from the first sectional surface in the pore 12 Orientation direction. Using the material 11, when a cylindrical test piece (diameter 3 mm×height 5 mm, the pore 12 array direction as a height direction) made of the material is dipped in polyethylene glycol up to 1 mm from one end thereof, polyethylene glycol permeates through the whole test piece preferably within 30 seconds.
摘要翻译:提供一种快速诱导骨组织形成并具有实用强度的多孔陶瓷材料。 在垂直于孔12取向的第一截面中,具有基本上单向取向的孔12,孔隙率为40-90%,孔的平均开放面积为0.05×10 -3〜50×10 -3 mm 2的多孔陶瓷材料11 方向和平行于第一截面的第二截面,并且在孔12的方位方向上离开第一截面的距离为5mm。 使用材料11,当将由该材料制成的圆柱形试验片(直径3mm×高度5mm,作为高度方向的孔12排列方向)从其一端浸入到聚乙二醇中至多1mm时,聚乙二醇渗透通过 整个试片优选在30秒内。
摘要:
A method for producing a porous body comprising apatite/collagen composite fibers comprising the steps of gelling a dispersion comprising long apatite/collagen composite fibers having an average length of 10-75 mm, short apatite/collagen composite fibers having an average length of 0.05-1 mm, and a liquid; freezing and drying the resultant gel to form a porous body; and cross-linking collagen in the porous body.
摘要:
A porous composite comprising a porous layer containing a calcium phosphate ceramic, and a dense layer formed on part of the porous layer and having a smaller average pore size than that of the porous layer. The porous composite can be produced by (1) introducing a slurry containing a calcium phosphate ceramic/collagen composite and collagen into a molding die having a high thermal conductivity, (2) rapidly freezing and drying the slurry in the molding die, to form a porous body comprising a porous layer and a dense layer formed on the porous layer, (3) cross-linking collagen in the porous body, and (4) removing the dense layer except for a portion thereof on a surface coming into contact with a soft tissue when implanted in a human body, so that the porous layer is exposed.
摘要:
In the process of producing a porous body containing a fibrous apatite/collagen composite by gelating a dispersion comprising the fibrous apatite/collagen composite, collagen and water, freeze-drying the resultant gel to form a porous body, and cross-linking collagen in the porous body, a method for controlling the average pore diameter of the porous body by the solidification time of the gel in the freezing step.
摘要:
A method for producing a porous body comprising apatite/collagen composite fibers comprising the steps of gelling a dispersion comprising long apatite/collagen composite fibers having an average length of 10-75 mm, short apatite/collagen composite fibers having an average length of 0.05-1 mm, and a liquid; freezing and drying the resultant gel to form a porous body; and cross-linking collagen in the porous body.
摘要:
A porous composite comprising a porous layer containing a calcium phosphate ceramic, and a dense layer formed on part of the porous layer and having a smaller average pore size than that of the porous layer. The porous composite can be produced by (1) introducing a slurry containing a calcium phosphate ceramic/collagen composite and collagen into a molding die having a high thermal conductivity, (2) rapidly freezing and drying the slurry in the molding die, to form a porous body comprising a porous layer and a dense layer formed on the porous layer, (3) cross-linking collagen in the porous body, and (4) removing the dense layer except for a portion thereof on a surface coming into contact with a soft tissue when implanted in a human body, so that the porous layer is exposed.
摘要:
Provision of a porous ceramic material which rapidly induces bone tissue formation and has practical strength.A porous ceramic material 11 having substantially unidirectionally oriented pores 12, a porosity of 40-90%, and an average open area of one pore of 0.05×10−3-50×10−3 mm2 both in a first sectional surface perpendicular to the pore 12 orientation direction and a second sectional surface parallel to the first sectional surface and 5 mm distant from the first sectional surface in the pore 12 orientation direction. Using the material 11, when a cylindrical test piece (diameter 3 mm×height 5 mm, the pore 12 array direction as a height direction) made of the material is dipped in polyethylene glycol up to 1 mm from one end thereof, polyethylene glycol permeates through the whole test piece preferably within 30 seconds.
摘要:
In the process of producing a porous body containing a fibrous apatite/collagen composite by gelating a dispersion comprising said fibrous apatite/collagen composite, collagen and water, freeze-drying the resultant gel to form a porous body, and cross-linking collagen in said porous body, a method for controlling the average pore diameter of said porous body by the solidification time of said gel in said freezing step.
摘要:
Sustained release microparticles suitable for various types of drugs, or drug-containing sustained release microparticles capable of sustained release of drugs over a period of three days or more and capable of inhibiting initial burst release; a process for producing the same; and preparations containing the microparticles are disclosed. The drug-containing sustained release microparticles comprise a drug other than human growth hormone and a porous apatite derivative, and optionally include a water-soluble bivalent metal compound. The drug-containing sustained release microparticles can be produced by dispersing under agitation microparticles of a porous apatite derivative in an aqueous solution containing a drug so that the aqueous solution infiltrates into the porous apatite derivative; optionally adding an aqueous solution containing a water-soluble bivalent metal compound that may infiltrate into the porous apatite derivative; further adding additives such as a stabilizer to the mixture; and effecting lyophilization or vacuum drying.