摘要:
The present invention provides a lubricant composition for hot metal working which is capable of inhibiting generation of flaws on the surface of materials to be provided for hot metal working, and provides a method of hot metal working. The invention provides a lubricant composition for hot metal working comprising a plurality of glass frits respectively having different softening point from each other.
摘要:
The present invention provides a lubricant composition for hot metal working which is capable of inhibiting generation of flaws on the surface of materials to be provided for hot metal working, and provides a method of hot metal working. The invention provides a lubricant composition for hot metal working comprising a plurality of glass frits respectively having different softening point from each other.
摘要:
The present invention is to provide a method for producing duplex stainless steel seamless pipe in which a duplex stainless steel billet can be inhibited from generating an oxide scale on the surface thereof during heating and the generation of outer surface flaw can also be prevented. The billet is heated in the a heating furnace for 1.5 hours or more and 4.0 hours or less at a heating temperature of 1250° C. or more and 1320° C. or less while regulating the average concentration of sulfur dioxide (SO2) gas in the atmosphere within the furnace to 0.01 volume % or less.
摘要:
The present invention is to provide a method for producing duplex stainless steel seamless pipe in which a duplex stainless steel billet can be inhibited from generating an oxide scale on the surface thereof during heating and the generation of outer surface flaw can also be prevented. The billet is heated in the a heating furnace for 1.5 hours or more and 4.0 hours or less at a heating temperature of 1250° C. or more and 1320° C. or less while regulating the average concentration of sulfur dioxide (SO2) gas in the atmosphere within the furnace to 0.01 volume % or less.
摘要:
A piercing and rolling plug has a film composed of oxides such as Fe3O4 and FeO and Fe (metal) as being formed on the surface of the base metal by electric arc spraying using an iron wire whose main component is Fe and, owing to this film, a plug excellent in heat-shielding and seizure-preventing effects can be realized and the lifetime of the plug can be prolonged. Further, in regenerating this plug, a film can be re-formed via the steps of shot blasting of the as-used plug in piercing and rolling and electric arc spraying in that order; thus, it is possible to regenerate the plug at low cost and in a short period of time.
摘要翻译:穿孔滚动塞具有由氧化物如Fe 3 O 4和FeO和Fe(金属)构成的膜,其通过使用主要成分为Fe的铁丝通过电弧喷涂形成在母材表面上,并且由于该膜 能够实现优良的隔热防止效果的塞子,延长塞子的使用寿命。 此外,在再生该插头时,可以通过以下步骤重新形成薄膜:依次进行穿孔和滚压以及电弧喷涂中使用的插头的喷丸处理; 因此,可以在低成本和短时间内再生插头。
摘要:
A piercing and rolling plug has a film composed of oxides such as Fe3O4 and FeO and Fe (metal) as being formed on the surface of the base metal by electric arc spraying using an iron wire whose main component is Fe and, owing to this film, a plug excellent in heat-shielding and seizure-preventing effects can be realized and the lifetime of the plug can be prolonged. Further, in regenerating this plug, a film can be re-formed via the steps of shot blasting of the as-used plug in piercing and rolling and electric arc spraying in that order; thus, it is possible to regenerate the plug at low cost and in a short period of time.
摘要翻译:穿孔滚动塞具有由氧化物如Fe 3 O 4和FeO和Fe(金属)构成的膜,其通过使用主要成分为Fe的铁丝通过电弧喷涂形成在母材表面上,并且由于该膜 能够实现优良的隔热防止效果的塞子,延长塞子的使用寿命。 此外,在再生该插头时,可以通过以下步骤重新形成薄膜:依次进行穿孔和滚压以及电弧喷涂中使用的插头的喷丸处理; 因此,可以在低成本和短时间内再生插头。
摘要:
A piercing mill includes a plurality of inclined rolls, a plug, a pusher, and an undriven guide roll. The pusher pushes a round billet from the rear end at least until the round billet advances for a prescribed distance after contacting the inclined rolls. The guide roll is between the inclined rolls and the pusher and includes a roll shaft and a roll surface, with the roll shaft arranged obliquely with respect to a pass line PL. The sectional shape of the roll surface is a concave arch shape. The round billet is rotated by the guide roll and the friction force generated when the round billet contacts the inclined rolls is reduced. Consequently, the wear of the inclined rolls can be restrained if the round billet is pierced and rolled while it is pushed in between the inclined rolls using the pusher.
摘要:
A piercing mill includes a plurality of inclined rolls, a plug, a pusher, and an undriven guide roll. The pusher pushes a round billet from the rear end at least until the round billet advances for a prescribed distance after contacting the inclined rolls. The guide roll is between the inclined rolls and the pusher and includes a roll shaft and a roll surface, with the roll shaft arranged obliquely with respect to a pass line PL. The sectional shape of the roll surface is a concave arch shape. The round billet is rotated by the guide roll and the friction force generated when the round billet contacts the inclined rolls is reduced. Consequently, the wear of the inclined rolls can be restrained if the round billet is pierced and rolled while it is pushed in between the inclined rolls using the pusher.
摘要:
a billet made of high Cr-high Ni alloy, which contains, by mass percent, 20 to 30% of Cr, 30 to 50% of Ni, and at least one element selected from Mo and W with a value “Mo+0.5W” of 1.5% or more is heated under conditions satisfying the following formula (1), and then the billet is pierced and rolled using an inclined roll type piercing mill with a roll gouge circumferential speed of 2.28 m/sec or higher. This prevents melted rash on the inner surface and lengthens the plug life. T≦1575−4.45×Vf−104.7×{−ln(th/ro)} (1) wherein T indicates a heating temperature (° C.) of the billet, Vf indicates the roll gouge circumferential speed (m/sec), ro indicates a radius (mm) of a billet at an entry-side, and th indicates a radial thickness (mm) of a pipe after piercing.
摘要:
a billet made of high Cr-high Ni alloy, which contains, by mass percent, 20 to 30% of Cr, 30 to 50% of Ni, and at least one element selected from Mo and W with a value “Mo+0.5W” of 1.5% or more is heated under conditions satisfying the following formula (1), and then the billet is pierced and rolled using an inclined roll type piercing mill with a roll gouge circumferential speed of 2.28 m/sec or higher. This prevents melted rash on the inner surface and lengthens the plug life. T≦1575−4.45×Vf−104.7×{−ln(th/ro)} (1) wherein T indicates a heating temperature (° C.) of the billet, Vf indicates the roll gouge circumferential speed (m/sec), ro indicates a radius (mm) of a billet at an entry-side, and th indicates a radial thickness (mm) of a pipe after piercing.