Information recording medium and method of manufacturing glass substrate for the information recording medium, and glass substrate for the information recording medium, manufactured using the method
    1.
    发明申请
    Information recording medium and method of manufacturing glass substrate for the information recording medium, and glass substrate for the information recording medium, manufactured using the method 审中-公开
    用于信息记录介质的信息记录介质和制造玻璃基板的方法以及使用该方法制造的用于信息记录介质的玻璃基板

    公开(公告)号:US20050074635A1

    公开(公告)日:2005-04-07

    申请号:US10392248

    申请日:2003-03-19

    IPC分类号: G11B5/64 G11B5/84 G11B5/66

    摘要: There is provided an information recording medium and a method of manufacturing a glass substrate for information recording media as well as a glass substrate manufactured using the method, according to which the take-off height (TOH) of a HDD for example can be made low. The surface shape in a predetermined region of an information recording medium is measured using an optical interferometer or an atomic force microscope. The measured surface shaped is subjected to line analysis along the circumferential direction of the information recording medium. A calculation is made of the product PSD×f of PSD corresponding to a predetermined wavelength ν and the reciprocal of the predetermined wavelength ν. The maximum value of the calculated PSD is controlled to not more than a predetermined value. As a result, the TOH can be made low by reducing waviness which hinders the magnetic head of a HDD or the like from stably flying.

    摘要翻译: 提供了一种信息记录介质和用于信息记录介质的玻璃基板的制造方法以及使用该方法制造的玻璃基板,根据该方法,例如可以使HDD的起飞高度(TOH)低 。 使用光学干涉仪或原子力显微镜测量信息记录介质的预定区域中的表面形状。 测量的表面形状沿着信息记录介质的圆周方向进行线分析。 对与预定波长nu对应的PSD的乘积PSDxf和预定波长nu的倒数进行计算。 将计算出的PSD的最大值控制在规定值以下。 结果,通过减少妨碍HDD等的磁头稳定地飞行的波纹,可以使TOH变低。

    Amorphous material processing method
    3.
    发明授权
    Amorphous material processing method 失效
    无定形材料加工方法

    公开(公告)号:US07727407B2

    公开(公告)日:2010-06-01

    申请号:US11131816

    申请日:2005-05-17

    IPC分类号: C03C25/66

    摘要: There are provided a method of processing an amorphous material which is capable of forming surface projections of uniform height in desired positions on the amorphous material, and a magnetic disk substrate using the amorphous material. A predetermined pressure is applied to selected parts of a surface of an amorphous material using fine particles having a hardness higher than that of the amorphous material to form high-density compressed layers, and a surface layer of the amorphous material is removed using a treatment agent that has a different removal capacity in the compressed layers and a remaining uncompressed layer, thus making the compressed layers project out. For example, the treatment agent may be an etching solution having a different etching rate in the compressed layers and the uncompressed layer.

    摘要翻译: 提供了一种处理非晶材料的方法,该非晶材料能够在非晶材料上的期望位置形成均匀高度的表面突起,以及使用该非晶材料的磁盘基板。 使用硬度高于无定形材料的细小颗粒将预定压力施加到非晶材料表面的选定部分,以形成高密度压缩层,并使用处理剂除去非晶材料的表面层 其在压缩层和剩余的未压缩层中具有不同的去除能力,从而使压缩层突出。 例如,处理剂可以是在压缩层和未压缩层中具有不同蚀刻速率的蚀刻溶液。

    Amorphous material processing method and glass substrate
    4.
    发明授权
    Amorphous material processing method and glass substrate 失效
    无定形材料加工方法和玻璃基板

    公开(公告)号:US06913702B2

    公开(公告)日:2005-07-05

    申请号:US09949692

    申请日:2001-09-10

    摘要: There are provided a method of processing an amorphous material which is capable of forming surface projections of uniform height in desired positions on the amorphous material, and a magnetic disk substrate using the amorphous material. A predetermined pressure is applied to parts of a surface of an amorphous material to form high-density compressed layers, and a surface layer of the amorphous material is removed using a treatment agent that has a different removal capacity in the compressed layers and a remaining uncompressed layer, thus making the compressed layers project out. For example, the treatment agent may be an etching solution having a different etching rate in the compressed layers and the uncompressed layer.

    摘要翻译: 提供了一种处理非晶材料的方法,该非晶材料能够在非晶材料上的期望位置形成均匀高度的表面突起,以及使用该非晶材料的磁盘基板。 将预定的压力施加到非晶材料的表面的部分以形成高密度压缩层,并且使用在压缩层中具有不同去除能力的处理剂去除非晶材料的表面层,并且剩余的未压缩 层,从而使压缩层投射出来。 例如,处理剂可以是在压缩层和未压缩层中具有不同蚀刻速率的蚀刻溶液。

    Glass substrate for information recording media and manufacturing method thereof
    5.
    发明授权
    Glass substrate for information recording media and manufacturing method thereof 有权
    用于信息记录介质的玻璃基板及其制造方法

    公开(公告)号:US06715318B2

    公开(公告)日:2004-04-06

    申请号:US09973495

    申请日:2001-10-09

    IPC分类号: C03C1900

    摘要: There are provided a glass substrate for information recording media in which the undulations on the glass substrate surface are optimized, thus contributing to reduction of the flying height, and at the same time preventing the occurrence of head crashes and thermal asperity, and a method of manufacturing the glass substrate. At least one surface of a glass substrate is polished, and the polished at least one surface of the glass substrate is subjected to surface scrubbing using a sponge having an Asker C hardness of not less than 40 according to The Society of Rubber Industry, Japan SRIS 0101.

    摘要翻译: 提供一种用于信息记录介质的玻璃基板,其中玻璃基板表面上的起伏被优化,从而有助于降低飞行高度,并且同时防止头部碰撞和热不均匀的发生,以及一种方法 制造玻璃基板。 抛光玻璃基板的至少一个表面,并且使用Asker C硬度不小于40的海绵对玻璃基板的抛光的至少一个表面进行表面洗涤,根据The Society of Rubber Industry,Japan SRIS 0101。

    Method for cleaning glass substrate
    6.
    发明授权
    Method for cleaning glass substrate 有权
    玻璃基板清洗方法

    公开(公告)号:US06568995B1

    公开(公告)日:2003-05-27

    申请号:US09699339

    申请日:2000-10-31

    IPC分类号: B24B724

    摘要: After a polishing process of polishing a glass substrate with an abrasive containing lanthanoid oxides, the glass substrate is subjected to the first and second washing processes. In the first washing process, the polished substrate is washed with a washing solution containing acid and a reducing agent, wherein the acid includes at least nitric acid. In the second washing process, the washed substrate is treated with an aqueous solution of an alkaline detergent. The substrate is suitable for a recording medium.

    摘要翻译: 在用含有镧系元素氧化物的研磨剂对玻璃基板进行抛光处理之后,对玻璃基板进行第一次和第二次洗涤处理。 在第一洗涤过程中,用含酸和还原剂的洗涤溶液洗涤抛光的底物,其中酸至少包含硝酸。 在第二次洗涤过程中,用碱性洗涤剂的水溶液处理洗涤过的底物。 该基片适用于记录介质。

    Separating method for dark ceramics sintered body
    7.
    发明授权
    Separating method for dark ceramics sintered body 失效
    深色陶瓷烧结体的分离方法

    公开(公告)号:US08409401B2

    公开(公告)日:2013-04-02

    申请号:US11991870

    申请日:2006-09-11

    IPC分类号: B32B38/10

    摘要: There are provided an aqueous solution for separation of a dark ceramics sintered body, which can easily collect in a recyclable condition a glass from a glass with a dark ceramics sintered body, and a separating method therefor, and an aqueous solution for separation with which a dark ceramics sintered body, a conductive ceramics sintered body and a glass are separately collected from a glass with a dark ceramics sintered body formed with the dark ceramics sintered body and the conductive ceramics sintered body, and a separating method therefor. A treatment liquid (hydrofluoric acid, a mixture of ammonium fluoride and an acid, etc.) having an etching ability for at least one of a glass and a dark ceramic sintered body is prepared as an aqueous solution 20 for separation of the dark ceramics sintered body, then type A treatment liquid is charged in a container 11, and a glass with a dark ceramics sintered body 30 is placed in the container 11.

    摘要翻译: 提供一种用于分离深色陶瓷烧结体的水溶液,其可以容易地从具有深色陶瓷烧结体的玻璃中以可回收的状态收集玻璃,以及其分离方法,以及用于分离的水溶液 黑陶瓷烧结体,导电陶瓷烧结体和玻璃分别从具有暗陶瓷烧结体和导电陶瓷烧结体形成的深色陶瓷烧结体的玻璃中收集,以及其分离方法。 制备具有对于玻璃和深陶瓷烧结体中的至少一种具有蚀刻能力的处理液(氢氟酸,氟化铵和酸的混合物)作为用于分离黑色陶瓷烧结体的水溶液20 然后将A型处理液装入容器11中,将具有深色陶瓷烧结体30的玻璃放置在容器11中。