摘要:
An aromatic polyester consisting of 40-70 mol % of unit I derived from p-hydroxybenzoic acid, 1-8 mol % of unit II derived from m-hydroxybenzoic acid or isophthalic acid, 6-36 mol % of units III and IV derived from terephthalic acid and 2,6-naphthalene dicarboxylic acid, respectively, and 10-40 mol % of unit V derived from a symmetrical dihydroxy compound can be melt molded at a temperature of up to 330.degree. C. into an article having improved mechanical and thermal properties. An aromatic polyesteramide consisting of components I to V and unit VI having an anilino group is also provided. A filled composition is obtained by blending the polyester or polyesteramide with an inorganic filler. A magnetic resin composition is obtained by blending the polyester or polyesteramide with a magnetic powder.
摘要:
Copolyesteramides consisting of specific units can be injection molded at a low temperature into a part having a high heat distortion temperature. A filled composition is obtained by blending the copolyesteramide with an inorganic filler. A magnetic resin composition is obtained by blending the copolyesteramide with an magnetic powder.The copolyesteramide consists essentially of units , , , , and of the following formulae: ##STR1## wherein each of R.sup.1, R.sup.2, R.sup.3 and R.sup.4 is independently at least one divalent radical selected from the group consisting of para-phenylene, 2,6-naphthalene, and 4,4'-biphenylene,R.sup.5 is a para- or meta-phenylene radical,X.sup.1 is --NH--,X.sup.2 is --NH--, --O-- or ##STR2##
摘要:
An aromatic polyester consisting of 40-70 mol % of unit I derived from p-hydroxybenzoic acid, 1-8 mol % of unit II derived from m-hydroxybenzoic acid or isophthalic acid, 6-36 mol % of units III and IV derived from terephthalic acid and 2,6-naphthalene dicarboxylic acid, respectively, and 10-40 mol % of unit V derived from a symmetrical dihydroxy compound can be melt molded at a temperature of up to 330.degree. C. into an article having improved mechanical and thermal properties. An aromatic polyesteramide consisting of components I to V and unit VI having an anilino group is also provided. A filled composition is obtained by blending the polyester or polyesteramide with an inorganic filler. A magnetic resin composition is obtained by blending the polyester or polyesteramide with a magnetic powder.
摘要:
The improved resin composition comprises:(A) a melt-workable liquid-crystal polyester resin obtained by polymerizing components selected from the group consisting of a dicarboxylic acid represented by the general formula (a) HOOC--R.sub.1 --COOH, a diol represented by the general formula (b) HO--R.sup.2 --OH, and an oxycarboxylic acid represented by the general formula (c) HO--R.sup.3 --COOH;(B) a polycarbonate resin having a recurring unit represented by the general formula: ##STR1## (C) a polyolefin and/or an olefinic copolymer, and the polyolefin and/or olefinic copolymer (C) is contained in an amount of 1-15 parts by weight per 100 parts by weight of a resin consisting of 95-5 wt % of the liquid-crystal polyester resin (A) and 5-95 wt % of the polycarbonate resin(B). This resin composition is balanced between various physical properties including moldability, heat resistance, impact resistance, dimensional stability and stiffness.
摘要:
Thermoplastic resin compositions comprising polyarylate and polyamide resins as main components, and an epoxy resin of the following formula [1] in a predetermined amount are provided. ##STR1## The thermoplastic resin compositions of the invention have good impact strength along with good heat and solvent resistances and good moldability.
摘要:
Provided herein are an aromatic polyester having superior physical properties which is composed of the following units ##STR1## an aromatic polyester amide formed by introducing a prescribed amount of amide linkage into said aromatic polyester; filament thereof; and a composition formed by adding an inorganic filler or magnetic powder to said polymers.
摘要:
Thermoplastic resin compositions comprising polyarylate and polyamide resins as main components, polyethylene terephthalate and an epoxy resin of the following formula [1] in a predetermined amount are provided. ##STR1##The thermoplastic resin compositions of the invention have good impact strength along with good heat and solvent resistances and good moldability.
摘要:
An improved polyarylate resin is provided, which resin comprises the following units (I) to (IV) ##STR1## the units (I) being contained in an amount of from 3 to 30 mole %, the units (II) being contained in amount of not less than 30 mole %, the units (III) being contained in an amount of not less than 30 mole %, and the units (IV) being contained in an amount of not larger than 25 mole %, each based on the total moles of the units (I) to (IV). The polyarylate resin has good mechanical strength, heat resistance, resistance to color change, transparency, moldability and flame retardancy. A resin composition comprising the polyarylate resin, a polyamide and an epoxy resin is also provided.
摘要:
Thermoplastic resin compositions comprising polyarylate and polyamide resins as main components, polyethylene terephthalate and an epoxy resin of the following formula [1] in a predetermined amount are provided. ##STR1##The thermoplastic resin compositions of the invention have good impact strength along with good heat and solvent resistances and good moldability.
摘要:
An ultrasonic treatment apparatus comprises at least one hand piece, a plurality of probes, and an ultrasonic drive device. The hand piece has an ultrasonic oscillation device for generating ultrasonic vibration. Each probe is adapted to be attached to the hand piece and designed to transmit the ultrasonic vibration generated by the hand piece. The ultrasonic drive device is connected to the hand piece, for driving the ultrasonic oscillation device.