Abstract:
A method according to the present disclosure may includes preparing a urea solution by dissolving urea in distilled water, adding phosphoric acid to the urea solution, adding pulp to the solution in which urea and phosphoric acid are dissolved, heating the solution such that the urea and the phosphoric acid each react with the pulp and preparing nanocellulose by washing the pulp which is completely reacted, and then grinding the pulp, in which a weight of the phosphoric acid is 10 to 50% based on a weight of the pulp.
Abstract:
A method for manufacturing a transparent composite material including preparing a film coated with a transparent resin, unidirectionally aligning glass fiber filaments and manufacturing a glass fiber plate by embedding the unidirectionally aligned glass fiber filaments in the transparent resin, wherein the transparent resin includes Si—O—Si bond and one of methyl, ethyl and phenyl.
Abstract:
Discussed is an adhesive containing a solid content, wherein the solid content can include cellulose, and carboxy methyl cellulose endowed with a carboxy methyl group.
Abstract:
The method for producing a nanocellulose support comprises coating a container with surface-treated nanocellulose solution, forming a nanocellulose film by drying the coated nanocellulose solution, and modifying the surface properties of the nanocellulose film by means of electron beam irradiation. According to an embodiment, the production of nanocellulose supports using the drying method allows substrates of various shapes to be coated and has simple processes, thus allowing mass production and production of over-sized supports.
Abstract:
A colorless composite material according to an embodiment includes glass fibers, and inorganic-organic hybrid resin having inorganic bonds and organic bonds, wherein the inorganic bonds are M-O-M bonds and M denotes a metallic element, wherein the metallic element is one of Ti, Zr and Al.