Method for continuous production of biodegradable aliphatic/aromatic polyester copolymer
    1.
    发明授权
    Method for continuous production of biodegradable aliphatic/aromatic polyester copolymer 有权
    连续生产生物降解脂肪/芳族聚酯共聚物的方法

    公开(公告)号:US09416224B2

    公开(公告)日:2016-08-16

    申请号:US14651800

    申请日:2013-07-18

    摘要: A continuous preparation method of a biodegradable aliphatic/aromatic polyester copolymer includes: performing a first esterification reaction of an aliphatic dihydroxy compound with an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product from the first esterification reaction; continuously performing a first polycondensation reaction of a reaction product from the second esterification reaction to obtain a prepolymer; continuously performing a second polycondensation reaction of the prepolymer to obtain a second polycondensation reaction product having an intrinsic viscosity from about 0.9 dl/g to about 1.0 dl/g; and continuously performing a third polycondensation reaction of the second polycondensation reaction product to prepare the biodegradable aliphatic/aromatic polyester copolymer, wherein the performing of the first esterification reaction or the continuously performing of the second esterification reaction includes adding an aromatic carboxylic acid. The biodegradable aliphatic/aromatic polyester copolymer prepared by control of the intrinsic viscosity of the second polycondensation reaction product may be improved in processibility, film formability, tensile/tearing strength, and blending ability with another polymer resin. Use of a less amount of the aliphatic dihydroxy compound as a starting material may reduce manufacturing costs.

    摘要翻译: 生物降解性脂肪族/芳香族聚酯共聚物的连续制备方法包括:在185℃以下的温度下进行脂族二羟基化合物与脂肪族二羧酸的第一次酯化反应; 连续进行来自第一酯化反应的反应产物的第二次酯化反应; 连续进行来自第二酯化反应的反应产物的第一次缩聚反应,得到预聚物; 连续进行预聚物的第二缩聚反应,得到特性粘度为约0.9dl / g至约1.0dl / g的第二缩聚反应产物; 并连续进行第二缩聚反应产物的第三缩聚反应,制备生物降解性脂肪族/芳香族聚酯共聚物,其中进行第一酯化反应或连续进行第二酯化反应包括加入芳族羧酸。 通过控制第二缩聚反应产物的特性粘度而制备的可生物降解的脂族/芳族聚酯共聚物可以提高加工性,成膜性,拉伸/撕裂强度和与另一种聚合物树脂的共混能力。 使用少量的脂肪族二羟基化合物作为原料可能降低制造成本。

    Method for continuous production of biodegradable aliphatic/aromatic polyester copolymer
    2.
    发明授权
    Method for continuous production of biodegradable aliphatic/aromatic polyester copolymer 有权
    连续生产生物降解脂肪/芳族聚酯共聚物的方法

    公开(公告)号:US09403938B2

    公开(公告)日:2016-08-02

    申请号:US14651489

    申请日:2013-07-18

    摘要: A continuous preparation method of a biodegradable aliphatic/aromatic polyester copolymer includes: performing a first esterification reaction of an aliphatic dihydroxy compound with an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product from the first esterification reaction; continuously performing a first polycondensation reaction of a reaction product from the second esterification reaction to obtain a prepolymer; continuously performing a second polycondensation reaction of the prepolymer to obtain a second polycondensation reaction product having a melting index from about 15 g/10 min to about 25 g/10 min; and continuously performing a third polycondensation reaction of the second polycondensation reaction product to prepare the biodegradable aliphatic/aromatic polyester copolymer, wherein the performing of the first esterification reaction or the continuously performing of the second esterification reaction includes adding an aromatic carboxylic acid.

    摘要翻译: 生物降解性脂肪族/芳香族聚酯共聚物的连续制备方法包括:在185℃以下的温度下进行脂族二羟基化合物与脂肪族二羧酸的第一次酯化反应; 连续进行来自第一酯化反应的反应产物的第二次酯化反应; 连续进行来自第二酯化反应的反应产物的第一次缩聚反应,得到预聚物; 连续进行预聚物的第二缩聚反应,得到熔融指数为约15g / 10min至约25g / 10min的第二缩聚反应产物; 并连续进行第二缩聚反应产物的第三缩聚反应,制备生物降解性脂肪族/芳香族聚酯共聚物,其中进行第一酯化反应或连续进行第二酯化反应包括加入芳族羧酸。

    Method for continuously preparing biodegradable aliphatic/aromatic polyester copolymer

    公开(公告)号:US09637589B2

    公开(公告)日:2017-05-02

    申请号:US14423641

    申请日:2013-05-20

    摘要: Provided is a method of continuous preparation of a biodegradable aliphatic/aromatic polyester copolymer, the method including: performing a first esterification reaction of an aliphatic dihydroxy compound and an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product obtained by the first esterification reaction; obtaining a pre-polymer by continuously performing a first polycondensation reaction of a reaction product obtained by the second esterification reaction; and continuously performing polycondensation reaction of the pre-polymer, wherein an aromatic carboxylic acid is added to a reactor in which the first esterification reaction or the second esterification reaction is performed, to prepare the biodegradable aliphatic/aromatic polyester copolymer. According to the method of continuous preparation of the biodegradable aliphatic/aromatic polyester copolymer as described above, the amount of the aliphatic dihydroxy compound used, which is a starting material, is reduced and accordingly, manufacturing costs are reduced.

    Method for preparing biodegradable polyester resin

    公开(公告)号:US09617378B2

    公开(公告)日:2017-04-11

    申请号:US14915711

    申请日:2014-08-25

    CPC分类号: C08G63/88 C08G63/16 C08G63/78

    摘要: A method of preparing a biodegradable polyester resin is provided. The method of preparing a biodegradable polyester resin includes: (a) synthesizing the biodegradable polyester resin having a reheating crystallization initiation temperature (Tch1), a reheating crystallization peak temperature (Tch), and a reheating crystallization end temperature (Tch2); and (b) crystallizing the biodegradable polyester resin synthesized in step (a) by cooling the resin from a temperature of T1 to a temperature of T2 and then maintaining the resin at a temperature of T2 for a time of tc. Thus, the biodegradable polyester resin with improved solidification rate may be obtained.

    METHOD FOR PREPARING BIODEGRADABLE POLYESTER RESIN
    5.
    发明申请
    METHOD FOR PREPARING BIODEGRADABLE POLYESTER RESIN 有权
    制备可生物降解聚酯树脂的方法

    公开(公告)号:US20160222158A1

    公开(公告)日:2016-08-04

    申请号:US14915711

    申请日:2014-08-25

    IPC分类号: C08G63/88 C08G63/16 C08G63/78

    CPC分类号: C08G63/88 C08G63/16 C08G63/78

    摘要: A method of preparing a biodegradable polyester resin is provided. The method of preparing a biodegradable polyester resin includes: (a) synthesizing the biodegradable polyester resin having a reheating crystallization initiation temperature (Tch1), a reheating crystallization peak temperature (Tch), and a reheating crystallization end temperature (Tch2); and (b) crystallizing the biodegradable polyester resin synthesized in step (a) by cooling the resin from a temperature of T1 to a temperature of T2 and then maintaining the resin at a temperature of T2 for a time of tc. Thus, the biodegradable polyester resin with improved solidification rate may be obtained.

    摘要翻译: 提供了一种制备可生物降解的聚酯树脂的方法。 制备可生物降解的聚酯树脂的方法包括:(a)合成具有再加热结晶起始温度(Tch1),再加热结晶峰温度(Tch)和再加热结晶结束温度(Tch2)的生物降解性聚酯树脂; 和(b)通过将树脂从T1的温度冷却至T2的温度,然后将树脂保持在T2的温度下,使步骤(a)中合成的可生物降解的聚酯树脂结晶tc。 因此,可以获得凝固速率提高的生物降解性聚酯树脂。

    TRANSPARENT BIODEGRADABLE POLYMER
    8.
    发明申请

    公开(公告)号:US20170101504A1

    公开(公告)日:2017-04-13

    申请号:US15317164

    申请日:2015-05-22

    IPC分类号: C08G63/672

    CPC分类号: C08G63/672

    摘要: The present invention is characterized by introducing isosorbide to a monomer configuration for securing the transparency of a biodegradable polymer as well as providing material having excellent heat resistance and flexibility, As a monomer, a component derived from isosorbide which has a rigid structure is contained by 10-50 mol % of a total diol component, thereby bringing a heat resistance enhancing effect, and enhancing transparency by interfering with crystal formation, and allowing for providing a polymer having excellent flexibility. Thus, the present invention may enable securing stability in usage especially in the packaging area, and enable the heightening of the range of usage and utilization thereof.

    Method for continuous production of biodegradable aliphatic/aromatic polyester copolymer
    9.
    发明授权
    Method for continuous production of biodegradable aliphatic/aromatic polyester copolymer 有权
    连续生产生物降解脂肪/芳族聚酯共聚物的方法

    公开(公告)号:US09447233B2

    公开(公告)日:2016-09-20

    申请号:US14651663

    申请日:2013-07-18

    摘要: A continuous preparation method of a biodegradable aliphatic/aromatic polyester copolymer includes: performing a first esterification reaction of an aliphatic dihydroxy compound with an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product from the first esterification reaction; continuously performing a first polycondensation reaction of a reaction product from the second esterification reaction to obtain a prepolymer having a weight average molecular weight of about 6,900 to about 14,000; continuously performing a second polycondensation reaction of the prepolymer to obtain a second polycondensation reaction product; and continuously performing a third polycondensation reaction of the second polycondensation reaction product to prepare the biodegradable aliphatic/aromatic polyester copolymer, wherein the performing of the first esterification reaction or the continuously performing of the second esterification reaction includes adding an aromatic carboxylic acid. The biodegradable aliphatic/aromatic polyester copolymer prepared by the continuous method may be improved in processibility, film formability, tensile/tearing strength, and blending ability with another polymer resin. Use of a less amount of the aliphatic dihydroxy compound as a starting material may reduce manufacturing costs.

    摘要翻译: 生物降解性脂肪族/芳香族聚酯共聚物的连续制备方法包括:在185℃以下的温度下进行脂族二羟基化合物与脂肪族二羧酸的第一次酯化反应; 连续进行来自第一酯化反应的反应产物的第二次酯化反应; 连续地进行来自第二酯化反应的反应产物的第一缩聚反应,得到重均分子量为约6,900至约14,000的预聚物; 连续进行预聚物的第二次缩聚反应得到第二缩聚反应产物; 并连续进行第二缩聚反应产物的第三缩聚反应,制备生物降解性脂肪族/芳香族聚酯共聚物,其中进行第一酯化反应或连续进行第二酯化反应包括加入芳族羧酸。 通过连续法制备的可生物降解的脂肪族/芳香族聚酯共聚物可以提高加工性,成膜性,拉伸/撕裂强度和与另一种聚合物树脂的共混能力。 使用少量的脂肪族二羟基化合物作为原料可能降低制造成本。