Abstract:
Disclosed are a method for producing a laminate including a step of laminating a resin impregnated fiber reinforced composition layer on a metal member, wherein the method includes a step of forming a resin coating on the metal member and a step of laminating a resin impregnated fiber reinforced composition layer containing a resin impregnated fiber reinforced composition containing (I) 20 to 80% by mass of a polymer having a melting point and/or a glass transition temperature of 50 to 300° C., and (C) 20 to 80% by mass of a reinforcing fiber (provided that the sum of the component (I) and the component (C) is taken as 100% by mass) via the above resin coating; and a laminate obtained by the method.
Abstract:
The purpose of the present invention is to provide a polar-group-containing propylene-type wax having excellent properties including a low melting point. A modified propylene-(α-olefin) copolymer (A) according to the present invention is produced by grafting at least one compound selected from an unsaturated carboxylic acid, a derivative of the unsaturated carboxylic acid and an unsaturated sulfonic acid salt onto a propylene-(α-olefin) copolymer (A1) and has an acid value of 1 to 100 KOHmg/g, wherein the propylene-(α-olefin) copolymer (A1) comprises 60 to 95 mol % of a propylene-derived constituent unit (a) and 5 to 40 mol % of a constituent unit (b) derived from an α-olefin having 4 or more carbon atoms, and satisfies the specific requirements (i) to (iii).
Abstract:
Disclosed are: a reinforcing fiber bundle with excellent mechanical property and handling property, which contains a propylene-based resin (A), a propylene-based resin (B) comprising at least a carboxylic acid salt bonded to the polymer chain, and a reinforcing fiber (C) wherein the propylene-based resin (A) comprises more than 70% by mass but not more than 100% by mass of a component (A-1) having a weight average molecular weight of 150,000 or more, the amount of the propylene-based resin (B) is 3 to 50 parts by mass per 100 parts by mass of the propylene-based resin (A), and the total content rate of the propylene-based resin (A) and the propylene-based resin (B) is 0.3 to 5% by mass in the whole reinforcing fiber bundle; and a molding material comprising the reinforcing fiber bundle and a matrix resin.