Abstract:
The thiol-containing composition for an optical material of the present invention includes a compound (A) represented by General Formula (a), and a compound (B) composed of at least one selected from a compound (b2-1) represented by General Formula (b2-1), a compound (b3-1) represented by General Formula (b3-1), a compound (b3-2) represented by General Formula (b3-2), and a compound (b4-2) represented by General Formula (b4-2), in which, in high-performance liquid chromatography measurement, the total peak area ratio of the compound included in the compound (B) is 0.1% to 60.0% with respect to the peak area 100 of the compound (A).
Abstract:
A xylylenediisocyanate composition including xylylenediisocyanate and a compound represented by Chemical Formula (1) below, wherein 0.6 ppm or more and 60 ppm or less of the compound represented by Chemical Formula (1) below is contained:
Abstract:
Provided are a film in which the balance between hydrophilicity and abrasion resistance is superior, decrease in hydrophilicity by water is minimal, and the weather resistance is also superior; as well as a polymer and a polymer composition that can yield such a film. The film of the invention is prepared from a specific copolymer (i) having a sulfonic acid-containing group, an epoxy group, and a specific alkoxysilyl group in a molecule, or from a composition including the copolymer (i).
Abstract:
A process for producing cyanonorbornene of the present invention includes Step 1 of preparing a mixture solution including 0.5% by weight to 28% by weight of methyl bicyclononadiene, with respect to a total amount of 100% by weight of dicyclopentadiene, acrylonitrile, and the methyl bicyclononadiene, in a container, and Step 2 of reacting the bicyclopentadiene with the acrylonitrile in the presence of the methyl bicyclononadiene, in the mixture solution.
Abstract:
The polymerizable composition for an optical material of the present invention contains (A) at least one kind of isocyanate having two or more isocyanato groups, which contains aromatic isocyanate, (B) at least one kind of alcohol having two or more hydroxyl groups, (C) an acidic phosphoric acid ester represented by the following Formula (1), and (D) a benzotriazole-based compound, in which a ratio of secondary hydroxyl groups to the total molar number of primary and secondary hydroxyl groups contained in the alcohol (B) is equal to or greater than 50%, and the benzotriazole-based compound (D) is contained in an amount of 1 part by weight to 11 parts by weight with respect to a total of 100 parts by weight of the isocyanate (A) and the alcohol (B).
Abstract:
A xylylene diisocyanate composition contains a xylylene diisocyanate and a chloromethylbenzyl isocyanate. The content ratio of the chloromethylbenzyl isocyanate is 0.2 ppm or more and below 600 ppm.
Abstract:
A manufacturing method of an isocyanate compound including obtaining a reaction solution containing an aldehyde compound by reacting a compound represented by Formula (a1) or (a2) with hydrogen and carbon monoxide in the presence of a metal compound of groups 8 to 10 and a phosphorus compound, neutralizing the reaction solution, purifying an aldehyde compound by distilling the neutralized reaction solution, reacting the aldehyde compound with ammonia and with hydrogen in the presence of a catalyst to obtain an amine compound; and reacting the amine compound with a carbonylating agent to obtain an isocyanate compound, wherein the phosphorus compound is represented by the Formula (R1O)3P, and the base compound is at least one selected from carbonate and hydrogen carbonate of metals of group I and carbonate and hydrogen carbonate of metals of group II, wherein the neutralizing the reaction solution is performed within a temperature range of 40° C. to 50° C.
Abstract:
A process for producing a pentaerythritol mercaptocarboxylic acid ester of the present invention includes: a step of reacting pentaerythritol with a mercaptocarboxylic acid, in which an absorbance of a 5 wt % aqueous solution of the pentaerythritol at a wavelength of 270 nm, which is measured using a quartz cell having an optical path length of 50 mm, is 0.07 or less.
Abstract:
A manufacturing method of an amine compound including obtaining a reaction solution containing an aldehyde compound by reacting a compound represented by Formula (a1) or (a2) with hydrogen and carbon monoxide in the presence of a metal compound of groups 8 to 10 and a phosphorus compound, neutralizing the reaction, purifying an aldehyde compound by distilling the neutralized reaction solution, and reacting the aldehyde compound with ammonia and with hydrogen in the presence of a catalyst to obtain an amine compound, wherein the phosphorus compound is represented by the Formula (R1O)3P, and the base compound is at least one selected from carbonate and hydrogen carbonate of metals of group I and carbonate and hydrogen carbonate of metals of group II, and wherein the neutralizing the reaction solution is performed within a temperature range of 40° C. to 50° C.
Abstract:
Provided is a polymerizable composition for an optical material including (A) isocyanates having two or more isocyanato groups, which include at least an isophorone diisocyanate, (B) at least one predetermined thiol having two or more mercapto groups, (C) an acidic phosphoric acid ester represented by General Formula (1), and (D) a tin compound represented by General Formula (2), in which the acidic phosphoric acid ester (C) is contained in an amount of 0.05 parts by weight to 0.9 parts by weight, with respect to a total of 100 parts by weight of the isocyanates (A) and the thiols (B), and the tin compound (D) is contained in such an amount that the content of tin is 0.05 parts by weight to 0.3 parts by weight, with respect to a total of 100 parts by weight of the isocyanates (A) and the thiols (B).