Polyolefin composition for rotomolding
    4.
    发明授权
    Polyolefin composition for rotomolding 有权
    用于滚塑的聚烯烃组合物

    公开(公告)号:US07332543B2

    公开(公告)日:2008-02-19

    申请号:US10469601

    申请日:2002-03-01

    IPC分类号: C08L23/00 C08L23/04

    摘要: A polymer composition suitable for rotomoulding comprising I) An ethylene homopolymer or copolymer with at least one other C3-10 ? olefin, having a melt flow rate of 0.5 to 30, a molecular weight distribution (Mw/Mn) of less than 4, an Mw of 50,000 to 110,000, a density of 0.940 g/cm3 to 0.970 g/cm3 and a melting point of 100 to 145° C.; or I) a propylene homopolymer or copolymer with at least one other C2-10 ? olefin, having a melt flow rate of 0.5 to 30, a molecular weight distribution (Mw/Mn) of less than 4, an Mw of 150,000 to 300,000, and a melting point of 100 to 170° C.; and II) an ethylene homo or copolymer with at least one other C3-10 ?-olefin, having a melt flow rate of within 40% of the melt flow rate of component (I), a molecular weight distribution of (Mw/Mn) of less than 4, an Mw of within 30% of the Mw of component (I), a density of 0.880 g/cm3 to 0.940 g/cm3 said density being at least 0.010 g/cm3 less than the density of component (I) and a melting point of at least 5° C. less than that of component (I); or II) a propylene homo or copolymer with at least one other C2-10 ?-olefin having a melt flow rate of within 40% of the melt flow rate of component (I), a molecular weight distribution of (Mw/Mn) of less than 4, an Mw of within 30% of the Mw of component (I), and a melting point of at least 10° C. less than that of component (I).

    摘要翻译: 适用于滚塑的聚合物组合物,其包含I)乙烯均聚物或与至少一种其它C 3-10的共聚物 烯烃,熔体流动速率为0.5〜30,分子量分布(Mw / Mn)小于4,Mw为50,000〜110,000,密度为0.940g / cm3〜0.970g / cm3,熔点为 100〜145℃。 或I)具有至少一个其它C 2-10的丙烯均聚物或共聚物 烯烃,熔体流动速率为0.5〜30,分子量分布(Mw / Mn)小于4,Mw为15万〜300,000,熔点为100〜170℃。 和II)与至少一种其它C3-10α-烯烃的乙烯均聚物或共聚物,其熔体流动速率在组分(I)的熔体流动速率的40%以内,分子量分布(Mw / Mn) 小于4,组分(I)的Mw的30%以内的Mw,密度为0.880g / cm 3至0.940g / cm 3,所述密度比组分(I)的密度小至少0.010g / cm 3, 并且比组分(I)的熔点低至少5℃的熔点; 或II)与至少一种其它C2-10α-烯烃的丙烯均聚物或共聚物,其熔体流动速率在组分(I)的熔体流动速率的40%以内,分子量分布(Mw / Mn)为 小于4,组分(I)的Mw的30%以内的Mw,并且熔点至少比组分(I)的熔点低10℃。