Method of manufacturing austenitic stainless steel sheet cast piece
    1.
    发明授权
    Method of manufacturing austenitic stainless steel sheet cast piece 有权
    生产奥氏体不锈钢板材的方法

    公开(公告)号:US07066237B2

    公开(公告)日:2006-06-27

    申请号:US10509404

    申请日:2003-03-27

    IPC分类号: B22D11/06

    摘要: Methods for casting an austenitic stainless steel thin strip casting through a continuous caster, e.g., a twin-drum type caster, in which the mold walls move synchronous with the casting to obtain a casting, wherein defects, e.g., salt-and-pepper unevenly glossy defects, on a steel sheet formed after cold rolling or cold forming are prevented. In particular, casting an austenitic stainless steel thin strip casting by regulating a pressing force P of mold wall faces against the casting in the range from more than 1.0 to less than 2.5 t/m, and preferably from more than 1.1 to not more than 1.6 t/m. The continuous caster used may be a twin-drum type continuous caster, with a drum radius R(m) and a pressing force P(t/m) of mold wall faces satisfying the relation 0.5≦(√{square root over (R)})×P≦2.0, and preferably 0.8≦(√{square root over (R)})×P≦1.2.

    摘要翻译: 通过连续铸造机铸造奥氏体不锈钢薄带铸造方法,例如双辊式铸造机,其中模具壁与铸件同步移动以获得铸件,其中缺陷例如盐和胡椒不均匀 防止了在冷轧或冷成型后形成的钢板上的光泽缺陷。 特别地,通过将​​模具壁面的压力P调节在大于1.0至小于2.5t / m 2,优选大于1.1至不大于1.6的范围内,铸造奥氏体不锈钢薄带铸件 t / m。 所使用的连续脚轮可以是双鼓式连续脚轮,其鼓半径R(m)和模具壁面的按压力P(t / m)满足关系0.5 <=(√{平方根超过(R )xP <= 2.0,优选0.8 <=(√{平方根超过(R)xP <= 1.2。

    Method of manufacturing austenitic stainless steel sheet cast piece
    2.
    发明申请
    Method of manufacturing austenitic stainless steel sheet cast piece 有权
    生产奥氏体不锈钢板材的方法

    公开(公告)号:US20050217822A1

    公开(公告)日:2005-10-06

    申请号:US10509404

    申请日:2003-03-27

    摘要: Methods for casting an austenitic stainless steel thin strip casting through a continuous caster, e.g., a twin-drum type caster, in which the mold walls move synchronous with the casting to obtain a casting, wherein defects, e.g., salt-and-pepper unevenly glossy defects, on a steel sheet formed after cold rolling or cold forming are prevented. In particular, casting an austenitic stainless steel thin strip casting by regulating a pressing force P of mold wall faces against the casting in the range from more than 1.0 to less than 2.5 t/m, and preferably from more than 1.1 to not more than 1.6 t/m. The continuous caster used may be a twin-drum type continuous caster, with a drum radius R(m) and a pressing force P(t/m) of mold wall faces satisfying the relation 0.5≦({square root}{square root over (R)})×P≦2.0, and preferably 0.8≦({square root}{square root over (R)})×P≦1.2.

    摘要翻译: 通过连续铸造机铸造奥氏体不锈钢薄带铸造方法,例如双辊式铸造机,其中模具壁与铸件同步移动以获得铸件,其中缺陷例如盐和胡椒不均匀 防止了在冷轧或冷成型后形成的钢板上的光泽缺陷。 特别地,通过将​​模具壁面的压力P调节在大于1.0至小于2.5t / m 2,优选大于1.1至不大于1.6的范围内,铸造奥氏体不锈钢薄带铸件 t / m。 所使用的连续脚轮可以是双鼓式连续脚轮,其鼓半径R(m)和模具壁面的按压力P(t / m)满足关系0.5 <=({平方根} {平方根 (R)xP <= 2.0,优选0.8 <=({平方根} {平方根超过(R)×P <= 1.2。

    Image forming apparatus
    4.
    发明授权
    Image forming apparatus 有权
    图像形成装置

    公开(公告)号:US08867980B2

    公开(公告)日:2014-10-21

    申请号:US12689526

    申请日:2010-01-19

    申请人: Hiroshige Inoue

    发明人: Hiroshige Inoue

    IPC分类号: G03G15/00

    摘要: An image forming apparatus has a pair of registration rollers which are moved in the width direction so that a sheet side end position is within a predetermined range in the width direction based on sheet side end position information from a lateral registration detection sensor. In the case that an image-formed sheet is conveyed to a sheet processing portion without being reversed, the pair of registration rollers are moved so that the sheet side end position is within the first range, and in the case that an image-formed sheet is conveyed to the sheet processing portion, the pair of registration rollers are moved so that the sheet side end position is within the second range being different from the first range before reversing and within the first range after reversing.

    摘要翻译: 图像形成装置具有一对定位辊,其沿着宽度方向移动,使得纸张侧端部位置基于来自横向对准检测传感器的纸张侧端部位置信息,在宽度方向上处于预定范围内。 在图像形成的纸张没有被反转的情况下被输送到纸张处理部分的情况下,一对记录辊被移动,使得纸张侧端部位置处于第一范围内,并且在图像形成的纸张 被输送到片材处理部分,一对对准辊移动,使得片材侧端部位置在与反转之前的第一范围不同的第二范围内,并且在倒转之后的第一范围内。

    Image forming apparatus
    5.
    发明授权
    Image forming apparatus 有权
    图像形成装置

    公开(公告)号:US08600285B2

    公开(公告)日:2013-12-03

    申请号:US12906746

    申请日:2010-10-18

    IPC分类号: G03G15/00

    摘要: An image forming apparatus includes an image forming unit configured to form an image on a sheet, a fixing unit configured to fix the image formed by the image forming unit on the sheet, a cooling unit configured to cool the sheet having the image fixed thereon by the fixing unit, a curl amount changing unit configured to change an amount of curl of the sheet by bending the sheet having the image fixed thereon, and a path configured to guide the sheet having the image fixed thereon to the image forming unit, after the sheet is conveyed through the curl amount changing unit and the curl amount changing unit. The curl amount changing unit changes an amount of bending the sheet according to whether the sheet is stopped at the cooling unit or not.

    摘要翻译: 图像形成装置包括图像形成单元,被配置为在片材上形成图像;固定单元,被配置为将由图像形成单元形成的图像固定在片材上;冷却单元,被配置为将具有固定在其上的图像的片材 固定单元,卷曲量改变单元,被配置为通过弯曲具有固定在其上的图像的片材来改变片材的卷曲量;以及路径,被配置为将具有固定在其上的图像的片材引导到图像形成单元, 片材通过卷曲量改变单元和卷曲量改变单元传送。 卷曲量变更单元根据片材是否停止在冷却单元而改变片材的弯曲量。

    Austenitic stainless steel welding wire and welding structure
    9.
    发明授权
    Austenitic stainless steel welding wire and welding structure 有权
    奥氏体不锈钢焊丝和焊接结构

    公开(公告)号:US08710405B2

    公开(公告)日:2014-04-29

    申请号:US11404413

    申请日:2006-04-13

    IPC分类号: B23K35/34 B23K35/22

    CPC分类号: B23K35/26

    摘要: A welding wire for austenitic stainless steel welding contains, in percent by mass, C: 0.005 through 0.05%, Si: 0.1 through 1.0%, Mn: 1.0 through 3.5%, Cr: 25.0 through 28.0%, Ni: 16.0 through 23.9%, Mo: 1.6 through 3.0%, Cu: 0.1 through 0.5%, Al: 0.001 through 0.02%, and N: more than 0.30 through 0.50%, limiting O to 0.03% or less, P to 0.03% or less, and S to 0.005% or less, and having a ratio of a Cr equivalent to Ni equivalent (Cr equivalent/Ni equivalent) within a range between 0.85 and 1.2 and a PI value of 35 or more, the remainder being iron and unavoidable impurities.

    摘要翻译: 奥氏体不锈钢焊接用焊丝以质量%计含有C:0.005〜0.05%,Si:0.1〜1.0%,Mn:1.0〜3.5%,Cr:25.0〜28.0%,Ni:16.0〜23.9% Mo:1.6〜3.0%,Cu:0.1〜0.5%,Al:0.001〜0.02%,N:大于0.30〜0.50%,将O限制在0.03%以下,P:0.03%以下,S:0.005以下 %以下,Cr相当于Ni当量(Cr当量/ Ni当量)在0.85〜1.2的范围内,PI值为35以上,剩余部分为铁和不可避免的杂质。

    AUSTENITE-TYPE STAINLESS STEEL HOT-ROLLING STEEL MATERIAL WITH EXCELLENT CORROSION RESISTANCE, PROOF-STRESS, AND LOW-TEMPERATURE TOUGHNESS AND PRODUCTION METHOD THEREOF
    10.
    发明申请
    AUSTENITE-TYPE STAINLESS STEEL HOT-ROLLING STEEL MATERIAL WITH EXCELLENT CORROSION RESISTANCE, PROOF-STRESS, AND LOW-TEMPERATURE TOUGHNESS AND PRODUCTION METHOD THEREOF 有权
    奥氏体不锈钢热轧钢材,具有优良的耐腐蚀性,耐应力和低温韧性及其生产方法

    公开(公告)号:US20120111457A1

    公开(公告)日:2012-05-10

    申请号:US13349866

    申请日:2012-01-13

    IPC分类号: C21D11/00 C22C38/58 C22C38/44

    摘要: An austenitic stainless steel hot-rolled steel material can be provided which has seawater resistance and strength superior to conventional steel. Low-temperature toughness can be maintained, which is preferable in a structural member of speedy craft. The steel material can include an austenitic stainless steel hot-rolled steel material which excels in the properties of corrosion resistance, proof stress, and low-temperature toughness. In such austenitic stainless steel hot-rolling steel material, e.g., PI [=Cr+3.3(Mo+0.5W)+16N] ranges from 35 to 40, δ cal [=2.9 (Cr+0.3Si +Mo+0.5W)−2.6 (Ni+0.3Mn+0.25Cu+35C+20N)−18] ranges from −6 to +2, and a 0.2% proof stress at room temperature is not less than 550 MPa, Charpy impact value measured using a V-notch test piece at −40° C. is not less than 100 J/cm2, and the pitting potential measured in a deaerated aqueous solution of 10% NaCl at 50° C. (Vc'100) is not less than 500 mV (as it relates to saturated Ag/AgCl).

    摘要翻译: 可以提供具有优于常规钢的耐海水性和强度的奥氏体不锈钢热轧钢材。 可以保持低温韧性,这在快速工艺的结构构件中是优选的。 钢材可以包括耐腐蚀性,耐应力性和低温韧性优异的奥氏体不锈钢热轧钢材。 在这种奥氏体不锈钢热轧钢材中,例如PI [= Cr + 3.3(Mo + 0.5W)+ 16N]为35〜40,δcal[= 2.9(Cr + 0.3Si + Mo + 0.5W) -2.6(Ni + 0.3Mn + 0.25Cu + 35C + 20N)-18]的范围为-6至+2,室温下的0.2%屈服应力不低于550MPa,夏比冲击值使用V- 在-40℃下的切口试验片不小于100J / cm 2,在50℃的10%NaCl的脱气水溶液(Vc'100)中测定的点蚀电位不小于500mV 它涉及饱和Ag / AgCl)。