公开(公告)号:US20110003139A1
公开(公告)日:2011-01-06
申请号:US12864419
申请日:2009-01-14
申请人: Masatada Numano , Nozomu Kawabe , Yukihiro Oishi , Nobuyuki Mori , Nobuyuki Okuda , Ryuichi Inoue
发明人: Masatada Numano , Nozomu Kawabe , Yukihiro Oishi , Nobuyuki Mori , Nobuyuki Okuda , Ryuichi Inoue
CPC分类号: C22F1/06 , B22D11/007 , B22D19/04 , B22D21/007 , C22C23/02 , C22C32/0063 , Y10T428/25
摘要: The invention offers a magnesium alloy sheet material having excellent plastic processibility and rigidity and a magnesium alloy formed body having excellent rigidity. The sheet material has magnesium alloy that forms the matrix containing hard particles. The region from the surface of the sheet material to a position away from the surface by 40% of the thickness of the sheet material is defined as the surface region, and the remaining region as the center region. Hard particles existing in the center region have a maximum diameter of more than 20 μm and less than 50 μm, and hard particles existing in the surface region have a maximum diameter of 20 μm or less. Because the hard particles existing at the surface side are fine particles, they are less likely to become the starting point of cracking or another defect at the time of plastic processing. Because the hard particles existing in the center region are coarse, they can increase the rigidity of the sheet material.
摘要翻译: 本发明提供具有优异的塑性加工性和刚性的镁合金板材和具有优异刚性的镁合金成形体。 片材具有形成含有硬质粒子的基体的镁合金。 从片材的表面到离开表面的位置的片材的厚度的40%的区域被定义为表面区域,其余区域被定义为中心区域。 存在于中心区域的硬质粒子的最大直径大于20μm且小于50μm,存在于表面区域的硬质粒子的最大直径为20μm以下。 由于存在于表面侧的硬质粒子是微细的粒子,因此在塑性加工时不太可能成为开裂的起点或其他缺陷。 由于存在于中心区域的硬质粒子较粗糙,因此能够提高片材的刚性。
-
公开(公告)号:US20110268986A1
公开(公告)日:2011-11-03
申请号:US13142360
申请日:2009-11-17
申请人: Masatada Numano , Ryuichi Inoue , Nobuyuki Okuda , Nozomu Kawabe , Koji Mori , Nobuyuki Mori , Yukihiro Oishi , Takahiko Kitamura
发明人: Masatada Numano , Ryuichi Inoue , Nobuyuki Okuda , Nozomu Kawabe , Koji Mori , Nobuyuki Mori , Yukihiro Oishi , Takahiko Kitamura
CPC分类号: H05K5/04 , Y10T29/49908 , Y10T156/10 , Y10T156/1002 , Y10T428/12611
摘要: The method of producing a magnesium alloy joined part has the following steps: a joining step of joining a reinforcing material made of metal to a plate material made of magnesium alloy without allowing an organic material to remain at the joined portion and a plastic-working step of performing plastic working on the plate material to which the reinforcing material is joined. A desirable means of joining the reinforcing material to the plate material can be to use an inorganic adhesive. Because the magnesium alloy joined part is formed by a structure in which the reinforcing material is joined to the plate material, in comparison with the case where the reinforcing material is formed by machining or the like, the magnesium alloy structural member can be obtained with high production efficiency.
摘要翻译: 镁合金接合部的制造方法具有以下步骤:将由金属制成的增强材料与镁合金制的板材接合而不使有机材料残留在接合部的接合工序和塑性加工工序 对加强材料接合的板材进行塑性加工。 将增强材料接合到板材的期望的方法可以是使用无机粘合剂。 由于镁合金接合部分是通过加强材料与板材接合的结构形成的,与通过机加工等形成增强材料的情况相比,可以获得高的镁合金结构件 生产效率。
-
公开(公告)号:US20110217514A1
公开(公告)日:2011-09-08
申请号:US12377916
申请日:2007-07-10
申请人: Nobuyuki Okuda , Masatoshi Majima , Shoichiro Sakai , Shinji Inazawa , Nobuyuki Mori , Ryuichi Inoue , Yukihiro Oishi , Nozomu Kawabe , Masatada Numano
发明人: Nobuyuki Okuda , Masatoshi Majima , Shoichiro Sakai , Shinji Inazawa , Nobuyuki Mori , Ryuichi Inoue , Yukihiro Oishi , Nozomu Kawabe , Masatada Numano
CPC分类号: C23C22/83 , C22C23/02 , C22F1/06 , C23C22/18 , C23C22/364 , C23C22/37 , C25D11/30 , Y10T428/24364
摘要: There is provided a magnesium alloy member having mechanical properties and corrosion resistance and a method of manufacturing the magnesium alloy member.A magnesium alloy member has a base material made of a magnesium alloy, and an anticorrosive film formed on the base material. The base material is a rolled magnesium alloy including 5 to 11% by mass of Al. By using a base material including a large amount of Al, a magnesium alloy member having excellent mechanical properties and high corrosion resistance can be produced. In addition, by using a rolled material, the number of surface defects at the time of casting is small, and the frequency of compensation processes such as undercoating and puttying can be reduced.
摘要翻译: 提供了具有机械性能和耐腐蚀性的镁合金构件以及镁合金构件的制造方法。 镁合金构件具有由镁合金制成的基材和形成在基材上的防腐蚀膜。 基材是含有5〜11质量%的Al的轧制镁合金。 通过使用含有大量Al的基材,可以制造具有优异的机械性能和高耐腐蚀性的镁合金构件。 此外,通过使用轧制材料,铸造时的表面缺陷的数量少,可以降低底涂和腻子等补偿处理的频率。
-
公开(公告)号:US20110203706A1
公开(公告)日:2011-08-25
申请号:US13125023
申请日:2009-09-29
申请人: Yukihiro Oishi , Nozomu Kawabe , Nobuyuki Okuda , Nobuyuki Mori , Masatada Numano , Koji Mori , Takahiko Kitamura , Ryuichi Inoue
发明人: Yukihiro Oishi , Nozomu Kawabe , Nobuyuki Okuda , Nobuyuki Mori , Masatada Numano , Koji Mori , Takahiko Kitamura , Ryuichi Inoue
IPC分类号: C22C23/02
摘要: A formed product of a magnesium alloy having excellent impact resistance and a magnesium alloy sheet suitable as a material for the formed product are provided. The formed product is produced by press-forming a magnesium alloy sheet having an Al content of 7% by mass to 12% by mass and has a flat portion that is not subjected to drawing deformation. In a metal texture in a cross section of the flat portion in the thickness direction, the number of coarse intermetallic compound (Mg17Al12) particles having a particle size of 5 μm or more present in a surface area region extending from a surface of the flat portion to a position one-third of the thickness from the surface in the thickness direction is five or less. The formed product has a texture in which the number of coarse precipitations d1 is small and in which fine precipitations d0 are dispersed. The formed product is less likely to be dented even when impacted because of dispersion strengthening owing to the fine precipitations and solid-solution strengthening owing to Al that sufficiently forms a solid solution.
摘要翻译: 提供了具有优异抗冲击性的镁合金的成型产品和适合成型产品的材料的镁合金板。 形成的产品通过压制形成Al含量为7质量%至12质量%的镁合金板而制成,并具有不受拉伸变形的平坦部分。 在平坦部分的厚度方向的横截面中的金属结构中,存在于从平坦部分的表面延伸的表面区域中具有5μm以上的粒子的粗大的金属间化合物(Mg17Al12)颗粒的数量 到厚度方向上的表面厚度的三分之一的位置为五分之一以下。 形成的产品具有其中粗沉淀物d1的数量少并且其中分散有细小沉淀物d0的织构。 即使由于由于充分形成固溶体的Al的细小沉淀和固溶强化而引起的分散强化,即使被冲击也难以形成凹陷。
-
公开(公告)号:US20110097573A1
公开(公告)日:2011-04-28
申请号:US12527530
申请日:2009-01-09
申请人: Nobuyuki Okuda , Ryuichi Inoue , Masatada Numano , Nobuyuki Mori , Yukihiro Oishi , Nozomu Kawabe
发明人: Nobuyuki Okuda , Ryuichi Inoue , Masatada Numano , Nobuyuki Mori , Yukihiro Oishi , Nozomu Kawabe
IPC分类号: B32B15/04
CPC分类号: B05D5/06 , B05D5/067 , B05D7/14 , B05D2202/20 , C22C23/02 , Y10T428/264 , Y10T428/265 , Y10T428/31678
摘要: The invention offers a magnesium alloy structural member having a high metallic texture. The magnesium alloy structural member is provided with a base material made of magnesium alloy and a covering layer formed on the base material. The base material is provided, in at least one part of its surface, with a surface-processed portion that is subjected to a fine asperity-forming processing so as to obtain a metallic texture. The covering layer is transparent. The structural member can effectively increase the metallic texture by having the surface-processed portion. Because the structural member is provided with the covering layer, it has excellent corrosion resistance. Because the covering layer is transparent, the metallic texture in the surface-processed portion is readily sensed. The asperity-forming processing is performed through hairline finish, diamond cut finish, and the like.
摘要翻译: 本发明提供具有高金属质感的镁合金结构件。 镁合金结构件具有由镁合金制成的基材和形成在基材上的覆盖层。 在其表面的至少一部分中,基材具有进行微细凹凸形成处理的表面处理部,以获得金属质感。 覆盖层是透明的。 结构构件可以通过具有表面处理部分来有效地增加金属质感。 由于结构件具有覆盖层,因此具有优异的耐腐蚀性。 由于覆盖层是透明的,因此容易感测到表面处理部分中的金属质感。 通过发丝加工,金刚石切割加工等进行凹凸成形加工。
-
公开(公告)号:US20110229733A1
公开(公告)日:2011-09-22
申请号:US13131179
申请日:2009-11-12
申请人: Masatada Numano , Ryuichi Inoue , Nobuyuki Okuda , Nozomu Kawabe , Koji Mori , Nobuyuki Mori , Yukihiro Oishi , Takahiko Kitamura
发明人: Masatada Numano , Ryuichi Inoue , Nobuyuki Okuda , Nozomu Kawabe , Koji Mori , Nobuyuki Mori , Yukihiro Oishi , Takahiko Kitamura
IPC分类号: B32B3/00
CPC分类号: C22C23/02 , B23K31/02 , B23K35/3602 , B23K2103/15 , C21D2251/00 , C22F1/00 , C22F1/06 , Y02P10/212 , Y10T428/12729
摘要: A plurality of magnesium alloy parts are joined to one another through an inorganic joining layer (an reinforcing material 2, a boss 3, and a pin 4 are joined to a base material 1). Concrete examples of the inorganic joining layer include a layer of an inorganic adhesive and a metal thin film formed on the magnesium alloy part at the time of hot cladding. Because the magnesium alloy parts are joined together through the inorganic joining layer, in comparison with the case where a reinforcing material and the like are formed by machining, waste of the material can be reduced. The use of the inorganic joining layer can produce a magnesium alloy structural member that does not generate hazardous smoke and soot even when it is melted for recycling.
摘要翻译: 多个镁合金部件通过无机接合层(增强材料2,凸台3,销4接合到基材1)彼此接合。 无机接合层的具体实例包括在热包层时在镁合金部件上形成的无机粘合剂层和金属薄膜。 由于通过无机接合层将镁合金部件接合在一起,与通过机械加工形成增强材料等的情况相比,可以减少材料的浪费。 无机接合层的使用可以产生即使在熔融再循环时也不产生危险烟雾和烟灰的镁合金结构件。
-
公开(公告)号:US20110165431A1
公开(公告)日:2011-07-07
申请号:US13063657
申请日:2009-07-16
申请人: Ryuichi Inoue , Nozomu Kawabe , Yukihiro Oishi , Nobuyuki Okuda , Nobuyuki Mori , Masatada Numano , Takahiko Kitamura , Koji Mori
发明人: Ryuichi Inoue , Nozomu Kawabe , Yukihiro Oishi , Nobuyuki Okuda , Nobuyuki Mori , Masatada Numano , Takahiko Kitamura , Koji Mori
IPC分类号: B21D5/00
CPC分类号: B21D5/00 , B21D22/02 , B21D22/20 , B21D51/52 , Y10T428/12382
摘要: The invention offers a pressed product (F) produced by press-forming a metal plate (1). The pressed product (F) has a peripheral surface that has a corner portion (12) connecting two surfaces in the peripheral surface. The corner portion (12) has an outside corner radius R that is equal to or smaller than the thickness “t” of the metal plate (1). That is, the pressed product (F) has the sharp corner portion (12).
摘要翻译: 本发明提供通过压制成形金属板(1)制成的压制品(F)。 压制品(F)具有外周面,该外周面具有连接外周面的两面的角部(12)。 角部(12)的外侧角半径R等于或小于金属板(1)的厚度“t”。 也就是说,被压制品(F)具有尖锐的拐角部分(12)。
-
公开(公告)号:US08852363B2
公开(公告)日:2014-10-07
申请号:US12864419
申请日:2009-01-14
申请人: Masatada Numano , Nozomu Kawabe , Yukihiro Oishi , Nobuyuki Mori , Nobuyuki Okuda , Ryuichi Inoue
发明人: Masatada Numano , Nozomu Kawabe , Yukihiro Oishi , Nobuyuki Mori , Nobuyuki Okuda , Ryuichi Inoue
CPC分类号: C22F1/06 , B22D11/007 , B22D19/04 , B22D21/007 , C22C23/02 , C22C32/0063 , Y10T428/25
摘要: The invention offers a magnesium alloy sheet material having excellent plastic processibility and rigidity and a magnesium alloy formed body having excellent rigidity. The sheet material has magnesium alloy that forms the matrix containing hard particles. The region from the surface of the sheet material to a position away from the surface by 40% of the thickness of the sheet material is defined as the surface region, and the remaining region as the center region. Hard particles existing in the center region have a maximum diameter of more than 20 μm and less than 50 μm, and hard particles existing in the surface region have a maximum diameter of 20 μm or less. Because the hard particles existing at the surface side are fine particles, they are less likely to become the starting point of cracking or another defect at the time of plastic processing. Because the hard particles existing in the center region are coarse, they can increase the rigidity of the sheet material.
摘要翻译: 本发明提供具有优异的塑性加工性和刚性的镁合金板材和具有优异刚性的镁合金成形体。 片材具有形成含有硬质粒子的基体的镁合金。 从片材的表面到离开表面的位置的片材的厚度的40%的区域被定义为表面区域,其余区域被定义为中心区域。 存在于中心区域的硬质粒子的最大直径大于20μm且小于50μm,存在于表面区域的硬质粒子的最大直径为20μm以下。 由于存在于表面侧的硬质粒子是微细的粒子,因此在塑性加工时不太可能成为开裂的起点或其他缺陷。 由于存在于中心区域的硬质粒子较粗糙,因此能够提高片材的刚性。
-
公开(公告)号:US08820614B2
公开(公告)日:2014-09-02
申请号:US13352029
申请日:2012-01-17
申请人: Masatada Numano , Ryuichi Inoue , Nobuyuki Okuda , Nozomu Kawabe , Koji Mori , Nobuyuki Mori , Yukihiro Oishi , Takahiko Kitamura
发明人: Masatada Numano , Ryuichi Inoue , Nobuyuki Okuda , Nozomu Kawabe , Koji Mori , Nobuyuki Mori , Yukihiro Oishi , Takahiko Kitamura
CPC分类号: H05K5/04 , Y10T29/49908 , Y10T156/10 , Y10T156/1002 , Y10T428/12611
摘要: The method of producing a magnesium alloy joined part has the following steps: a joining step of joining a reinforcing material made of metal to a plate material made of magnesium alloy without allowing an organic material to remain at the joined portion and a plastic-working step of performing plastic working on the plate material to which the reinforcing material is joined. A desirable means of joining the reinforcing material to the plate material can be to use an inorganic adhesive. Because the magnesium alloy joined part is formed by a structure in which the reinforcing material is joined to the plate material, in comparison with the case where the reinforcing material is formed by machining or the like, the magnesium alloy structural member can be obtained with high production efficiency.
摘要翻译: 镁合金接合部的制造方法具有以下步骤:将由金属制成的增强材料与镁合金制的板材接合而不使有机材料残留在接合部的接合工序和塑性加工工序 对加强材料接合的板材进行塑性加工。 将增强材料接合到板材的期望的方法可以是使用无机粘合剂。 由于镁合金接合部分是通过加强材料与板材接合的结构形成的,与通过机加工等形成增强材料的情况相比,可以获得高的镁合金结构件 生产效率。
-
公开(公告)号:US08501301B2
公开(公告)日:2013-08-06
申请号:US12377916
申请日:2007-07-10
申请人: Nobuyuki Okuda , Masatoshi Majima , Shoichiro Sakai , Shinji Inazawa , Nobuyuki Mori , Ryuichi Inoue , Yukihiro Oishi , Nozomu Kawabe , Masatada Numano
发明人: Nobuyuki Okuda , Masatoshi Majima , Shoichiro Sakai , Shinji Inazawa , Nobuyuki Mori , Ryuichi Inoue , Yukihiro Oishi , Nozomu Kawabe , Masatada Numano
CPC分类号: C23C22/83 , C22C23/02 , C22F1/06 , C23C22/18 , C23C22/364 , C23C22/37 , C25D11/30 , Y10T428/24364
摘要: A magnesium alloy member having mechanical properties and corrosion resistance and a method of manufacturing the magnesium alloy member are provided. A magnesium alloy member has a base material made of a magnesium alloy, and an anticorrosive film formed on the base material. The base material is a rolled magnesium alloy including 5 to 11% by mass of Al. By using a base material including a large amount of Al, a magnesium alloy member having excellent mechanical properties and high corrosion resistance can be produced. In addition, by using a rolled material, the number of surface defects at the time of casting is small, and the frequency of compensation processes such as undercoating and puttying can be reduced.
摘要翻译: 提供具有机械性能和耐腐蚀性的镁合金构件以及镁合金构件的制造方法。 镁合金构件具有由镁合金制成的基材和形成在基材上的防腐蚀膜。 基材是含有5〜11质量%的Al的轧制镁合金。 通过使用含有大量Al的基材,可以制造具有优异的机械性能和高耐腐蚀性的镁合金构件。 此外,通过使用轧制材料,铸造时的表面缺陷的数量少,可以降低底涂和腻子等补偿处理的频率。
-
-
-
-
-
-
-
-
-