Low viscosity, ethylenically unsaturated polyurethanes containing
allophanate groups
    5.
    发明授权
    Low viscosity, ethylenically unsaturated polyurethanes containing allophanate groups 失效
    含有脲基甲酸酯基团的低粘度,烯属不饱和聚氨酯

    公开(公告)号:US5739251A

    公开(公告)日:1998-04-14

    申请号:US826262

    申请日:1997-03-27

    摘要: The present invention relates to ethylenically unsaturated polyurethanes which are substantially free from isocyanate groups and have a) a content of .beta.,.gamma.-ethylenically unsaturated ether groups (calculated as C.dbd.C, MW 24) incorporated through allophanate groups of 0.5 to 10% by weight, b) an allophanate group content (calculated as N.sub.2 C.sub.2 HO.sub.3, MW 101) of 1 to 20% by weight and c) a total content of ethylenically unsaturated groups of (calculated as C.dbd.C, MW 24) of 1 to 15% by weight. The present invention also relates to ethylenically unsaturated polyisocyanates which contain allophanate groups and have i) an NCO content of 5 to 25% by weight, ii) a content of .beta.,.gamma.-ethylenically unsaturated ether groups (calculated as C.dbd.C, MW 24) incorporated through allophanate groups of 0.5 to 15% by weight and iii) an allophanate group content (calculated as N.sub.2 C.sub.2 HO.sub.3, MW 101) of 1 to 30%. Finally, the present invention relates to one-component coating compositions containing the ethylenically unsaturated polyurethanes according to the invention.

    摘要翻译: 本发明涉及烯属不饱和聚氨酯,其基本上不含异氰酸酯基团,并且具有a)通过脲基甲酸酯基团通过0.5至10%的通过以下方式引入的β,γ-烯属不饱和醚基团的含量(以C = C,MW 24计算) 重量,b)脲基甲酸酯基含量(以N2C2HO3,MW101计算)为1〜20重量%,c)(计算为C = C,MW 24)的烯属不饱和基团的总含量为1〜15% 重量。 本发明还涉及含有脲基甲酸酯基并且i)NCO含量为5至25重量%的烯键式不饱和多异氰酸酯,ii)β,γ-烯属不饱和醚基团的含量(按C = C计算,MW 24 )通过0.5至15重量%的脲基甲酸酯基组合,和iii)脲基甲酸酯基含量(以N 2 C 2 HO 3,MW 101计算)为1至30%。 最后,本发明涉及含有根据本发明的烯属不饱和聚氨酯的单组分涂料组合物。

    REINFORCED UV-A CURABLE COMPOSITE COMPOSITIONS AND METHODS
    6.
    发明申请
    REINFORCED UV-A CURABLE COMPOSITE COMPOSITIONS AND METHODS 有权
    增强UV-A可固化复合材料组合物和方法

    公开(公告)号:US20100260941A1

    公开(公告)日:2010-10-14

    申请号:US12420112

    申请日:2009-04-08

    摘要: The present disclosure is directed to a process for forming a reinforced ultraviolet (UV) radiation-curable composite. The composite may be formed by applying reinforcing layers and resin layers to a substrate. The resin composition may include an aliphatic urethane acrylate oligomer, a polyfunctional acrylate monomer, and a photoinitiator. The composite formed on the substrate may be exposed to UV radiation to cure the composite on the substrate. The composite may be characterized in that it is cured within 10 minutes of exposure to UV radiation and does not exhibit oxygen inhibition effects, such as, for example, surface tack. The reinforced UV-curable composite may find utility, for example, as a rapid field repair patch in aerospace applications, among others.

    摘要翻译: 本公开涉及形成增强的紫外线(UV)可辐射固化复合材料的方法。 可以通过将增强层和树脂层施加到基底上来形成复合材料。 树脂组合物可以包括脂肪族聚氨酯丙烯酸酯低聚物,多官能丙烯酸酯单体和光引发剂。 形成在基底上的复合物可以暴露于UV辐射以固化基底上的复合物。 该复合材料的特征在于其在暴露于UV辐射的10分钟内固化,并且不显示出氧抑制作用,例如表面粘性。 增强的可UV固化复合材料可以用于例如航空航天应用中的快速现场修补补片。

    Low viscosity, ethylenically unsaturated polyurethanes containing
allophanate groups
    8.
    发明授权
    Low viscosity, ethylenically unsaturated polyurethanes containing allophanate groups 失效
    含有脲基甲酸酯基团的低粘度,烯属不饱和聚氨酯

    公开(公告)号:US5767220A

    公开(公告)日:1998-06-16

    申请号:US917797

    申请日:1997-08-25

    CPC分类号: C08G18/7837 C08G18/671

    摘要: The present invention relates to ethylenically unsaturated polyurethanes which are substantially free from isocyanate groups and have a) a total content of (meth)acryloyl groups (calculated as C=C, MW 24) of 1 to 20% by weight. b) an allophanate group content (calculated as N.sub.2 C.sub.2 HO.sub.3, MW 101) of 1 to 20% by weight and c) an isocyanurate group content (calculated as N.sub.3,C.sub.3,O.sub.3, MW 126) of up to 18% by weight, in which the allophanate and isocyanurate groups are prepared from aliphatic polyisocyanates. The present invention also relates to a one-component coating composition containing these ethylenically unsaturated polyurethanes.

    摘要翻译: 本发明涉及基本上不含异氰酸酯基并且具有(a)(i = C,MW 24计算)的(甲基)丙烯酰基的总含量为1〜20重量%的烯属不饱和聚氨酯。 b)脲基甲酸酯基含量(以N2C2HO3,MW101计算)为1〜20重量%,c)异氰脲酸酯基含量(以N 3,C 3,O 3,MW 126计)高达18重量%,其中 脲基甲酸酯和异氰脲酸酯基团由脂族多异氰酸酯制备。 本发明还涉及含有这些烯属不饱和聚氨酯的单组分涂料组合物。

    PROCESS FOR THE PRODUCTION OF SIZED AND/OR WET-STRENGTH PAPERS, PAPERBOARDS AND CARDBOARDS
    10.
    发明申请
    PROCESS FOR THE PRODUCTION OF SIZED AND/OR WET-STRENGTH PAPERS, PAPERBOARDS AND CARDBOARDS 有权
    生产尺寸和/或湿度强度纸,纸张和卡片的方法

    公开(公告)号:US20120160437A1

    公开(公告)日:2012-06-28

    申请号:US12975470

    申请日:2010-12-22

    IPC分类号: D21H17/57 D21H17/00

    CPC分类号: D21H21/16 D21H17/44

    摘要: The present invention relates to a process for the production of sized and/or wet-strength papers, paperboards or cardboards, wherein an aqueous radiation-curable dispersion containing water and at least one polymer, characterized in that the polymer contains cationic groups, is mixed with suspended wood pulp and/or chemical pulp and this mixture is sieved, pressed, thermally dried and then radiation-cured, characterized in that the dispersion is employed in amounts, based on its non-aqueous content in relation to the solid content of the wood pulp and/or chemical pulp, of from 0.001 to 10 wt. %, the papers, paperboards and cardboards produced by this process, and compositions comprising suspended wood pulp and/or chemical pulp and an aqueous radiation-curable dispersion containing at least one polymer, characterized in that the polymer contains cationic groups.