摘要:
A wire for electric railways comprises a copper alloy which consists essentially, by weight percent, of 0.1 to 1.0% Cr, 0.01 to 0.3% Zr, 0.05 to 0.15% Sn, and 10 ppm or less O, and if required, further contains 0.01 to 0.1% Si, or 0.01 to 0.1% Si and 0.001 to 0.05% Mg, with the balance being Cu and inevitable impurities.
摘要:
A wire for electric railways comprises a copper alloy which consists essentially, by weight percent, of 0.1 to 1.0% Cr, 0.01 to 0.3% Zr, and 10 ppm or less O, and if required, further contains at least one element selected from the group consisting of 0.01 to 0.1% Si and 0.001 to 0.05% Mg, with the balance being Cu and inevitable impurities. The wire is manufactured by hot working a copper alloy billet having the above composition, immediately quenching the hot worked billet to prepare an element wire, cold working the element wire at least once, and subjecting the cold worked element wire to aging treatment.
摘要:
There is disclosed an engine valve of titanium alloy having a stem portion made of a cold-worked titanium alloy containing 2% to 4% by weight of aluminum, 1.5% to 3.5% by weight of vanadium and balance titanium. The engine valve suitable for use as an intake valve has a head portion made of a cast titanium alloy containing 2% to 7% by weight of aluminum, 3% to 20% by weight of vanadium and balance titanium. Moreover, an exhaust engine valve has a head portion made of a cast titanium alloy containing 5% to 10% by weight of aluminum and balance titanium.
摘要:
A zinc cast alloy is disclosed which contains, by weight, 15-60% Al, 0.05-3% Cu, 0.5-7% Si, 0.01-0.8% Mn, optionally 0.005-0.12% P and/or Na, balance Zn and incidental impurities. The alloy has a high damping characteristic, concurrently with good intergranular corrosion resistance and high resistance to both room and elevated temperatures. To achieve values of more than 1.times.10.sup.-3 (internal friction of Q.sup.-1), 20 .mu.m (corrosion depth) or less, 10 kg/mm.sup.2 or more (0.2% yield strength) at room temperature, and 20 kg/mm.sup.2 or more at elevated temperature of 100.degree. C., the alloy has to be subjected to a solution-heat treatment in the range of 300.degree.-400.degree. C., followed by a rapid cooling, preferably a water quench.
摘要翻译:公开了一种锌铸合金,其含有15-60%Al,0.05-3%Cu,0.5-7%Si,0.01-0.8%Mn,任选0.005-0.12%P和/或Na,余量Zn和 附带杂质。 该合金具有较高的阻尼特性,同时具有良好的耐晶间腐蚀性和对室温和高温的高耐受性。 为了实现在室温下大于1×10 -3(Q-1的内摩擦),20μm(腐蚀深度)或更小,10kg / mm 2或更高(0.2%屈服强度)的值和20kg / mm 2或 在100℃的升温下更多的是,合金必须在300-400℃的范围内进行溶解热处理,然后快速冷却,优选水淬。
摘要:
A continuous casting furnace for manufacturing an elongated cast product, for example, of copper or its alloy includes a housing defining a chamber. A crucible is accommodated within the chamber for holding a casting material. A heater is mounted on the crucible for melting the casting material. A generally vertically-disposed elongated casting nozzle hermetically extends into the chamber. One of the casting nozzle and the crucible is movable toward the other for immersing a lower end of the casting nozzle in the molten casting material in the crucible. The housing is connected to an inert gas source for introducing inert gas into the chamber when the casting material in the crucible is melted. When the lower end of the casting nozzle is immersed in the molten casting material, the molten casting material is moved along the casting nozzle by the pressure of the inert gas in the chamber. A cooling device is associated with the casting nozzle for solidifying the molten casting material when it is passed through the casting nozzle, thereby forming the elongated cast product.
摘要:
A fuel rod for a light water reactor comprises a cladding tube which comprises a zirconium alloy having a composition including 0.6 to 2.0% by weight of Nb, 0.5 to 1.5% by weight of Sn, 0.05 to 0.3% by weight of Fe, and the balance being Zr and incidental impurities; uranium oxide fuel pellets packed in the cladding tube; and end plugs comprising a zirconium alloy and closing both ends of the cladding tube. The cladding tube is sealed by TIG welding with the end plugs. Grain boundaries in each heat affected zone of the cladding tube, which are adjacent to a bead formed by TIG welding, have structural compositions including 4 to 30% by weight of Nb, and 0.9 to 20% by weight of Fe.
摘要:
A fuel rod for a light water reactor comprises a cladding tube which comprises a zirconium alloy having a composition including 0.6 to 2.0% by weight of Nb, 0.5 to 1.5% by weight of Sn, 0.05 to 0.3% by weight of Fe, and the balance being Zr and incidental impurities; uranium oxide fuel pellets packed in the cladding tube; and end plugs closing both ends of the cladding tube. The cladding tube is sealed by TIG welding with the end plugs. Precipitates having grain diameters of 0.01 to 0.5 .mu.m and comprise intermetallic compounds containing Zr, Nb and Fe are present at grain boundaries in the structure of heat affected zones of the cladding tube, the heat affected zone being adjacent to a bead formed by TIG welding.
摘要:
A copper based alloy consists essentially, by weight %, of 15 to 35% Zn, 7 to 14% Ni, 0.1 to 2% or less Mn, 0.01 to 0.5% Fe, 0.0005 to 0.1% P, at least one or two elements selected from the group consisting of 0.001 to 0.9% Si, 0.0003 to 0.02% Pb, and 0.0003 to 0.01% C, the total content of the selected at least two elements being limited to a range of 0.0006 to 0.9%, and the balance of Cu and inevitable impurities. The copper based alloy has excellent blankability as well as good corrosion resistance and high strength.
摘要:
A wear resistant copper alloy composition which includes: ______________________________________ Component (% by weight) ______________________________________ Zn 20 to 40 Al 2 to 11 at least one iron family metal 1 to 5 selected from Fe, Ni, and Co Ti 0.1 to 4 Component X, which is at least one Mn = 0.01 to less than 0.1 of Mn or S, in the amounts S = 0.0005 to 0.01 indicated Cu (with unavoidable impurities) balance. ______________________________________ The copper alloy, which contains as an optional component Mg (from 0.01 to 0.5% by weight), is particularly suitable for manufacturing synchronizer rings in automatic transmissions for internal combustion engines.
摘要:
In a Cu-alloy mold for use in centrifugal casting of Ti or Ti-alloys, the mold body is made of a Cu alloy satisfying the following relationship:Ts+0.3.rho..gtoreq.70where Ts is the tensile strength (kg/mm.sup.2), and .rho. is the electrical conductance (% IACS). A cavity disposed in the mold body has a volume which is at most 30% of the volume of the mold body. Also disclosed is a method for centrifugally casting Ti or Ti-alloy by the use of the above-described mold.