Abstract: A polyethylene terephthalate (PET) copolyester and a manufacturing method thereof are provided, including the following steps. A dispersion slurry including a talcum powder is formulated. Terephthalic acid and ethylene glycol are mixed, and the dispersion slurry and a side group ester compound are introduced to perform a transesterification reaction and form bis-2-hydroxylethyl terephthalate. Afterwards, a prepolymerization reaction and a polycondensation reaction are carried out to form a polyethylene terephthalate copolyester.
-
公开(公告)号:US11732131B2
公开(公告)日:2023-08-22
申请号:US17885517
申请日:2022-08-10
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Han-Ching Hsu , Chen-Wei Chang
IPC: C08L75/06 , D01D5/08 , C08G18/42 , C08G18/12 , C08G18/28 , D01F6/70 , C08G18/76 , D01D1/04 , C08K5/3492 , C08G18/08 , D01F1/10
CPC classification number: C08L75/06 , C08G18/0895 , C08G18/12 , C08G18/2825 , C08G18/4202 , C08G18/4236 , C08G18/4238 , C08G18/7671 , C08K5/3492 , D01D1/04 , D01D5/08 , D01F6/70 , D01F1/10
Abstract: A thermoplastic polyurethane resin suitable for melt spinning is formed from a reaction mixture via a polymerization reaction. The reaction mixture includes an isocyanate component and a polyol component. The polyol component includes a first polyol that has a first number average molecular weight and a second polyol that has a second number average molecular weight. The first number average molecular weight is between 1,000 g/mol and 1,500 g/mol, and the second number average molecular weight is between 2,500 g/mol and 3,000 g/mol. One resin component formed by the first polyol via the polymerization reaction is defined as a low melting point segment and correspondingly has a first melting point between 170° C. and 185° C. Another resin component formed by the second polyol via the polymerization reaction is defined as a high melting point segment and correspondingly has a second melting point between 195° C. and 210° C.
-
公开(公告)号:US20240166807A1
公开(公告)日:2024-05-23
申请号:US18091412
申请日:2022-12-30
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Han-Ching Hsu , Chen-Wei Chang
Abstract: A polyethylene terephthalate (PET) copolyester and a manufacturing method thereof are provided. The manufacturing method includes the following steps. A dispersion slurry including a talcum powder is formulated, wherein the talcum powder has an average particle size of 1 μm to 50 μm and an average specific surface area of 7 m2/g to 20 m2/g. Next, a terephthalic acid and an ethylene glycol are mixed, and the dispersion slurry and a crystallization accelerator are introduced, so as to carry out a transesterification reaction and therefore form a bis-2-hydroxylethyl terephthalate (BHET). Afterwards, a prepolymerization reaction and a polycondensation reaction are carried out to form a polyethylene terephthalate (PET) copolyester.
-
公开(公告)号:US11773304B2
公开(公告)日:2023-10-03
申请号:US16727761
申请日:2019-12-26
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Han-Ching Hsu , Chen-Wei Chang
IPC: C09J175/08 , C09J7/30 , C08G18/12 , C08K5/00 , C08G18/48 , C08K5/13 , C08K5/521 , C08K5/3475 , C08K5/09
CPC classification number: C09J175/08 , C08G18/12 , C08G18/4841 , C08G18/4845 , C08K5/005 , C08K5/09 , C08K5/13 , C08K5/3475 , C08K5/521 , C09J7/30
Abstract: A polyurethane adhesive and a mixture used for manufacturing a plastic athletic track are provided. The polyurethane adhesive includes a urethane pre-polymer which is formed by a reaction between an isocyanate and a polyol. The polyol is selected from the group consisting of polyether polyol and polybutadiene polyol, and a number average molecular weight of the polyol is between 1,000 g/mole and 6,000 g/mole. Based on the total weight of the polyurethane adhesive, a content of the urethane pre-polymer is between 80 wt % and 99.5 wt %, and a viscosity of the polyurethane adhesive is between 1,000 cps and 3,000 cps under an environmental temperature of between 15° C. and 40° C.
-
-
-