Abstract:
Provided is a solid electrolyte which contains a composition expressed by 3LiOH·Li2SO4. The solid electrolyte has a lithium ion conductivity of 0.1×10−6 S/cm or more at 25° C. and an activation energy of 0.6 eV or more.
Abstract:
Provided is an all-solid lithium battery including: a low-angle oriented positive electrode plate that is a lithium complex oxide sintered plate having a porosity of 10 to 50%; a negative electrode plate containing Ti and capable of intercalating and deintercalating lithium ions at 0.4 V or higher (vs. Li/Li+); and a solid electrolyte having a melting point lower than the melting point or pyrolytic temperature of the oriented positive electrode plate or the negative electrode plate, wherein at least 30% of pores in the oriented positive electrode plate is filled with the solid electrolyte in an observation of a cross-section perpendicular to a main face of the oriented positive electrode plate.
Abstract:
A method of manufacturing a composite sintered body includes a step (Step S11) of molding mixed powder in which Al2O3, SiC, and MgO are mixed, into a green body having a predetermined shape and a step (Step S12) of generating a composite sintered body by sintering the green body. Then, in Step S11, the ratio of SiC to the mixed powder is not lower than 4.0 weight percentage and not higher than 13.0 weight percentage. Further, the purity of Al2O3 in Step S11 is not lower than 99.9%. It is thereby possible to suppress the abnormal grain growth of Al2O3 and suitably manufacture a composite sintered body having high relative dielectric constant and withstand voltage, and low tan δ.
Abstract:
A sintered compact includes an alumina phase as a primary phase, and further includes an amorphous phase containing Si and Mn and a cordierite phase. The sintered compact has a porosity of higher than or equal to 1.1% and less than or equal to 5.0%. Preferably, I1/(I1+I2) is greater than or equal to 0.20 and less than or equal to 0.45, where I1 is the strength of the main peak of cordierite obtained by an XRD method, and I2 is the strength of the main peak of alumina.
Abstract:
A MgO-based ceramic film according to the present invention contains crystalline phases of MgO and MgAl2O4, and Al is dissolved in the MgO to form a solid-solution. The ceramic film exhibits a diffraction peak representing the (200) plane of MgO at an angle 2θ of more than 42.92° in CuKα XRD measurement. A shoulder preferably appears on the higher angle side of the peak representing the (200) plane of MgO. The mass ratio MgO/Al2O3 of MgO to Al2O3 converted from Mg and Al in terms of oxides is preferably higher than 2.33.
Abstract:
A thermal spray coating according to the present invention contains mainly magnesium, aluminum, oxygen, and nitrogen and has, as a main phase, a crystal phase of a MgO—AlN solid solution in which aluminum nitride is dissolved with magnesium oxide. The thermal spray coating is obtained by thermal spray of powder of a ceramic material containing mainly magnesium, aluminum, oxygen, and nitrogen and having, as a main phase, a crystal phase of a MgO—AlN solid solution in which aluminum nitride is dissolved with magnesium oxide.
Abstract:
A manufacturing method of a sintered ceramic body mixes barium silicate with aluminum oxide, a glass material, and an additive oxide to prepare a material mixture, molds the material mixture and fires the molded object. The barium silicate is monoclinic and has an average particle diameter in a range of 0.3 μm to 1 μm and a specific surface area in a range of 5 m2/g to 20 m2/g. The aluminum oxide has an average particle diameter in a range of 0.4 μm to 10 μm, a specific surface area in a range of 0.8 m2/g to 8 m2/g. A volume ratio of the aluminum oxide to the barium silicate is in a range of 10% by volume to 25% by volume.
Abstract:
The composite sintered body includes Al2O3, and MgAl2O4. The content of Al2O3 in the composite sintered body is not less than 95.5% by weight. The average sintered grain size of Al2O3 in the composite sintered body is not less than 2 μm and not greater than 4 μm. The standard deviation of sintered grain size distribution of Al2O3 in the composite sintered body is not greater than 0.35. The bulk density of the composite sintered body is not less than 3.94 g/cm3 and not greater than 3.98 g/cm3. In the composite sintered body, the ratio of amount of crystal phase of MgAl2O4 to that of Al2O3 is not less than 0.003 and not greater than 0.01.
Abstract:
A cordierite-based sintered body according to the present invention contains cordierite as a main component and silicon nitride or silicon carbide. The cordierite-based sintered body preferably has a thermal expansion coefficient less than 2.4 ppm/° C. at 40° C. to 400° C., an open porosity of 0.5% or less, and an average grain size of 1 μm or less.