LAYERED FILM AND LAYERED MEMBER
    3.
    发明申请

    公开(公告)号:US20220299681A1

    公开(公告)日:2022-09-22

    申请号:US17629944

    申请日:2020-07-22

    IPC分类号: G02B1/14 G02B1/11

    摘要: Provided is a laminated film that can be molded into a complicated shape. A laminated film comprising a transparent support substrate; an uncured hard coat layer formed on at least one surface of the transparent support substrate; and an uncured optical interference layer formed on the uncured hard coat layer, wherein the uncured hard coat layer comprises an active energy ray-curable composition for forming a hard coat layer, the uncured optical interference layer comprises an active energy ray-curable composition for forming a optical interference layer, a thickness of the transparent support substrate is 50 μm or more and 600 μm or less, a luminous reflectance including regular reflected light measured from an uncured optical interference layer side is 0.1% or more and 4.0% or less, and a stretch ratio at 160° C. is 50% or more.

    METHOD FOR MANUFACTURING LAYERED FILM, AND METHOD FOR MANUFACTURING LAYERED MEMBER

    公开(公告)号:US20220288914A1

    公开(公告)日:2022-09-15

    申请号:US17629927

    申请日:2020-07-22

    IPC分类号: B32B37/24 B32B37/10 B32B38/00

    摘要: Provided is a method for manufacturing a laminated film that can be molded into a complicated shape. A method for manufacturing a laminated film comprising: a step of forming an uncured hard coat layer by applying an active energy-ray curable composition for forming a hard coat layer to one side of a first support substrate having a thickness of 50 μm or more and 600 μm or less, and then drying the composition; a step of forming an uncured optical interference layer by applying an active energy-ray curable composition for forming a optical interference layer on one surface of a second support substrate so that the thickness of the uncured optical interference layer is between 15 nm or more and 200 nm or less, and then drying the composition; and a lamination step of laminating a surface of the uncured hard coat layer opposite the first support substrate and a surface of the uncured optical interference layer opposite the second support substrate to obtain a laminated film, wherein a stretch ratio of the laminated film at 160° C. is 50% or more.