公开(公告)号:US20160121576A1
公开(公告)日:2016-05-05
申请号:US14927870
申请日:2015-10-30
Applicant: NITTO DENKO CORPORATION
Inventor: Shu SASAKI , Makoto SAITOU , Kiyoaki KODAMA , Masato FUJITA
CPC classification number: B32B5/18 , B32B3/30 , B32B5/022 , B32B5/22 , B32B5/245 , B32B5/26 , B32B7/06 , B32B7/12 , B32B15/046 , B32B15/08 , B32B15/12 , B32B15/14 , B32B15/18 , B32B15/20 , B32B27/12 , B32B27/281 , B32B27/304 , B32B27/32 , B32B27/322 , B32B27/36 , B32B27/365 , B32B29/02 , B32B2262/106 , B32B2264/108 , B32B2266/02 , B32B2266/0214 , B32B2266/0228 , B32B2266/025 , B32B2266/0257 , B32B2266/0264 , B32B2266/0278 , B32B2266/0292 , B32B2266/06 , B32B2266/08 , B32B2266/104 , B32B2270/00 , B32B2307/202 , B32B2307/212 , B32B2307/514 , B32B2307/56 , B32B2307/72 , B32B2307/748 , B32B2405/00 , B32B2457/208
Abstract: An electroconductive pressure-sensitive adhesive cushioning member includes an electroconductive resin foam layer, an electroconductive composite layer, and an electroconductive intermediate layer disposed between the electroconductive resin foam layer and the electroconductive composite layer. The electroconductive composite layer includes an electroconductive base layer and an electroconductive attachment layer disposed on a surface of the electroconductive base layer and having an attachment surface to be attached to an obstacle. Thus, the electroconductive cushioning member is excellent in conductivity, an electromagnetic waves shieling property, and a cushioning property.
Abstract translation: 导电压敏粘合剂缓冲构件包括导电树脂发泡层,导电复合层和设置在导电树脂泡沫层和导电复合层之间的导电中间层。 导电性复合层包括导电性基底层和导电性附着层,该导电性基底层和导电性附着层配置在导电性基底层的表面上,具有附着在障碍物上的附着面。 因此,导电性缓冲部件的导电性,电磁波隔离性和缓冲性优异。
-
公开(公告)号:US20130224434A1
公开(公告)日:2013-08-29
申请号:US13777606
申请日:2013-02-26
Applicant: NITTO DENKO CORPORATION
Inventor: Itsuhiro HATANAKA , Makoto SAITOU , Kazumichi KATO
IPC: C08L23/12
CPC classification number: C08L23/12 , C08L23/10 , C08L2201/02 , C08L2203/14 , C09J7/26 , C09J2201/606 , Y10T428/24273 , Y10T428/24331 , C08L23/16
Abstract: Disclosed is a resin foam sheet which has a low apparent density, is thin and flexible, and can be wound satisfactorily stably. The resin foam sheet has an apparent density of 0.02 to 0.30 g/cm3, a tensile strength of 0.5 to 3.0 MPa, a thickness of 0.20 to 0.70 mm, a length of 5 m or more, and a width of 300 mm or more and has openings on both sides. The resin foam sheet preferably has a value of 30% or less determined according to following Expression (1): (Thickness tolerance)/(Median thickness)×100 (1)
Abstract translation: 公开了一种表观密度低,薄而柔软的树脂发泡片,并且可以令人满意地稳定地卷绕。 树脂发泡体片的表观密度为0.02〜0.30g / cm 3,拉伸强度为0.5〜3.0MPa,厚度为0.20〜0.70mm,长度为5μm以上,宽度为300mm以上, 双方有开口。 树脂发泡体片材优选为根据下述式(1)确定的30%以下的值:(厚度公差)/(中值厚度)×100(1)
-