摘要:
Process for producing activated carbon, preferably high surface area activated carbon, from inexpensive cellulosic precursors, such as paper, by pretreating the cellulosic precursor with an activating agent, such as phosphoric acid, followed by carbonization in an inert atmosphere at an elevated temperature to produce activated carbon. The activated carbon can be further activated to increase its surface area by heating it in an oxidizing atmosphere at an elevated temperature to yield activated carbon having a surface area of at least 100 m.sup.2 /g.
摘要:
A room temperature setting carbonaceous cement comprising a solid carbonaceous material, a catalyst, a liquid carbonizable component, and copper particles, which when treated with the catalyst will provide a carbon yield of at least 40% for the liquid component at an elevated baking temperature and possess increased flexural strength at elevated temperatures and reduced electrical resistance.
摘要:
A room temperature setting carbonaceous cement comprising a solid carbonaceous material, a catalyst and a liquid carbonizable component, and a boron containing or phosphorus containing material, which when treated with the catalyst will possess increased oxidation resistance at elevated temperatures.
摘要:
A room temperature setting carbonaceous cement comprising a solid carbonaceous material, a catalyst and a liquid carbonizable component which when treated with the catalyst will provide a carbon yield of at least 40% at an elevated baking temperature and possess a flexural strength which is above at least 750 psi at room temperature and at said elevated temperature.
摘要:
A method for intercalating graphite flakes which requires less intercalation solution and avoids a washing step, thus producing economy in material and production costs, and avoiding production of contaminated waste water which requires costly disposal steps.
摘要:
A stable blister free flexible graphite is formed in accordance with the present invention by performing two chemical reactions including a first step of high temperature heat treatment which converts the active carbon surface from hydrophilic to hydrophobic and generates active surface sites and a second step of exposing the heat treated graphite to a stabilizing reagent for stabilizing the active sites generated by the first step of high temperature heat treatment.
摘要:
A process for forming pinhole free ultra-thin flexible sheet material from natural graphite comprising treating low ash natural graphite particles with an oxidizing agent to intercalate the graphite, introducing the particles after they are dried to less than 2% by weight water into a furnace preheated to at least 2000.degree. F. to cause rapid expansion to a specific volume of at least 800 cc/gm and compressing the expanded graphite to below 8 mils in thickness with a density of less than 1.3 g/cc.
摘要:
A thermal interface and a thermal interface as part of a thermal management system that comprises a heat source, and a cooling module. The heat source has an external surface; the thermal interface is a flexible graphite sheet article having two parallel planar surfaces, with the first planar surface of the thermal interface being in operative contact with the external surface of the heat source and the second planar surface being in contact with the cooling module. The graphite sheet contains oil.
摘要:
An article, such as a seal ring, suitable for reduction of chatter when used in stuffing boxes with reciprocating stems. The article has an amorphous carbon phase at the surface of the article with the amorphous carbon phase extending into the article from the surface.
摘要:
A binder which comprises pitch and the condensation product of (A) a ketone or dione selected from the group consisting of C.sub.3 to C.sub.13 aliphatic linear, branched or cyclic ketones and diones having at least one active hydrogen on each carbon atom adjacent to a ##STR1## group, compounds of the formula: ##STR2## wherein a and b are integers having a values of 0 to 6, and the C.sub.1 to C.sub.4 alkyl substituted derivatives thereof; and (B) at least one compound selected from the group consisting of C.sub.5 to C.sub.11 aldehydes, said aldehydes having an aromatic ring containing 4 to 6 carbon atoms and 0 to 1 oxygen atoms, wherein said condensation product has a Heat of Reaction Value of less than about 155 cal/g. Said binders being useful in the production of graphite electrodes having superior physical and electrical properties.