    摘要: A method for manufacturing an electric contact material is provided which can prevent it from being adhesively melted even when being exposed to high temperatures resulting from an arc induced by an electric current being turned on or off. Also an electric contact material which is manufactured by the method and a thermal fuse are provided.A surface layer portion of an alloy containing 1 to 15 mass % of Cu, 0.01 to 0.7 mass % of Ni, and the remainder of Ag and unavoidable impurities is supplied with an amount of oxygen exceeding the amount of oxygen required for internal oxidation of Cu to form an oxygen concentrated layer. This alloy can serve as an electric contact material.This electric contact material is formed into a movable electrode, which is in turn employed for a thermal fuse.

    摘要翻译: 提供了一种制造电接触材料的方法,即使当暴露于由导通或断开的电流引起的电弧引起的高温时,也可以防止其粘着熔化。 还提供了通过该方法制造的电接触材料和热熔丝。 将含有1〜15质量%的Cu,0.01〜0.7质量%的Ni,剩余的Ag和不可避免的杂质的合金的表层部分供给超过Cu内部氧化所需的氧量 以形成氧浓缩层。 该合金可以用作电接触材料。 该电接触材料形成为可动电极,该可动电极又用作热熔丝。

    Urethane foam reinforcing material
    6.
    发明授权
    Urethane foam reinforcing material 有权
    聚氨酯泡沫增强材料

    公开(公告)号:US07790643B2

    公开(公告)日:2010-09-07

    申请号:US12304565

    申请日:2007-06-14

    IPC分类号: D04H1/46

    摘要: A reinforcing material for urethane foam effectively protects a molded urethane foam body and suppresses fricatives with a metal spring, having high productivity and excellent handleability and being applicable to a molded urethane foam body with highly uneven shape at low cost. It is a reinforcing material for urethane foam wherein a nonwoven fabric A having single fiber linear density of 1.0 to 3.0 dtex and a nonwoven fabric B having single fiber linear density of 0.5 to 2.5 dtex are laminated by needlepunching process by inserting needles from a direction of the nonwoven fabric A with a needle density of 35 to 70 needles/cm2.

    摘要翻译: 用于聚氨酯泡沫的增强材料有效地保护模制的聚氨酯泡沫体并且用金属弹簧抑制摩擦擦,具有高生产率和优异的可操作性,并且可以以低成本应用于具有高度不均匀形状的模制聚氨酯泡沫体。 作为聚氨酯泡沫塑料的增强材料,其中单丝纤维线密度为1.0〜3.0dtex的无纺布A和单纤维线密度为0.5〜2.5dtex的无纺布B通过针刺方法层叠, 针密度为35〜70针/ cm 2的无纺布A。

    Sliding contact material comprising Ag-Ni based alloy having Ni metal particles dispersed and clad composite material, and Dc compact motor using the same
    7.
    发明授权
    Sliding contact material comprising Ag-Ni based alloy having Ni metal particles dispersed and clad composite material, and Dc compact motor using the same 有权
    滑动接触材料包括具有分散和复合材料的Ni金属颗粒的Ag-Ni基合金,以及使用其的Dc紧凑型电动机

    公开(公告)号:US06638334B2

    公开(公告)日:2003-10-28

    申请号:US10088082

    申请日:2002-07-01

    IPC分类号: C22C105

    摘要: The present invention is aimed at providing a sliding contact material that has an alloy composition containing no harmful substance like Cd, especially excellent contact resistance properties, electrical functions that are good and is not subject to secular change, and abrasion resistance practically bearing comparison with conventional sliding contact materials, and is aimed at lengthening the life of a motor by the use of a sliding contact material having excellent durability as a commutator for a small direct-current motor. The present invention is a sliding contact material of an Ag—Ni-based alloy that is used in sliding part electrically switching on and off by mechanical sliding action, and the material is a sliding contact material of Ni metal particle-dispersed-type Ag—Ni-based alloy that is produced in such a method that 0.7 to 3.0 wt. % Ni powder, an additive of Li2CO3 powder corresponding to 0.01 to 0.50 wt. % Li after being converted to metal and the balance of Ag powder are mixed and stirred to form a uniformly dispersed mixture, then the mixture is treated with forming and sintering processes.

    摘要翻译: 本发明的目的在于提供一种滑动接触材料,其具有不含Cd等有害物质的合金组成物,特别优异的接触电阻性能,良好的电化学功能,不会发生长期变化,并且耐磨性实际上与传统的 滑动接触材料,旨在通过使用具有优异的耐久性的滑动接触材料作为小型直流电动机的换向器来延长电动机的寿命。 本发明是一种用于通过机械滑动动作电气接通和断开的滑动部分中的Ag-Ni基合金的滑动接触材料,并且该材料是Ni金属颗粒分散型Ag-Ni基合金的滑动接触材料, Ni基合金,其以0.7〜3.0重量% %Ni粉末,相当于0.01〜0.50重量%的Li2CO3粉末添加剂。 将Li转化成金属后,将Ag粉末的余量混合搅拌,形成均匀分散的混合物,然后用成型和烧结工艺处理混合物。

    Method for recovering metal from target and method for manufacturing target
    10.
    发明授权
    Method for recovering metal from target and method for manufacturing target 有权
    从目标中回收金属的方法和制造目标的方法

    公开(公告)号:US08366800B2

    公开(公告)日:2013-02-05

    申请号:US13052668

    申请日:2011-03-21

    IPC分类号: C22B7/00 C22C1/02

    摘要: A target consisting essentially of a CoCrPt-based metal or a CoCrPtRu-based metal, and one or more metal oxides selected from the group consisting of SiO2, Cr2O3, CoO, TiO2 and Ta2O5, is heated in an upper crucible of a two-level crucible that includes the upper crucible with a through hole formed in a bottom surface, and a lower crucible disposed below the through hole. The target is heated at a temperature of from 1400 to 1790° C. if the target does not contain both TiO2 and Ta2O5. The target is heated at a temperature of from 1400 to 1630° C. if the target contains TiO2 but does not contain Ta2O5. The target is heated at a temperature of from 1400 to 1460° C. if the target contains Ta2O5. The metal thereby melted is caused to flow into the lower crucible, so that the metal is separated from the metal oxide.