摘要:
The present invention is aimed at providing a sliding contact material that has an alloy composition containing no harmful substance like Cd, especially excellent contact resistance properties, electrical functions that are good and is not subject to secular change, and abrasion resistance practically bearing comparison with conventional sliding contact materials, and is aimed at lengthening the life of a motor by the use of a sliding contact material having excellent durability as a commutator for a small direct-current motor. The present invention is a sliding contact material of an Ag—Ni-based alloy that is used in sliding part electrically switching on and off by mechanical sliding action, and the material is a sliding contact material of Ni metal particle-dispersed-type Ag—Ni-based alloy that is produced in such a method that 0.7 to 3.0 wt. % Ni powder, an additive of Li2CO3 powder corresponding to 0.01 to 0.50 wt. % Li after being converted to metal and the balance of Ag powder are mixed and stirred to form a uniformly dispersed mixture, then the mixture is treated with forming and sintering processes.
摘要:
The invention provides a material for sliding contacts that is suitable for a small-sized DC motor used in recent downsized CD players and is excellent in durability. A material for sliding contacts used in a commutator of a small-sized DC motor that consists essentially of 0.01 to 3.0% Ni by weight, 0.01 to 6.0% ZnO by weight and/or 0.01 to 3.0% MgO by weight, furthermore, in some cases, 0.01 to 5.0% Cu by weight, and the balance Ag, in which Ni metal particles, ZnO particles or MgO particles are dispersed in the matrix of Ag.
摘要:
The invention provides a material for sliding contacts that is suitable for a small-sized DC motor used in recent downsized CD players and is excellent in durability. A material for sliding contacts used in a commutator of a small-sized DC motor that consists essentially of 0.01 to 3.0% Ni by weight, 0.01 to 6.0% ZnO by weight and/or 0.01 to 3.0% MgO by weight, furthermore, in some cases, 0.01 to 5.0% Cu by weight, and the balance Ag, in which Ni metal particles, ZnO particles or MgO particles are dispersed in the matrix of Ag.
摘要:
Provided are a substrate on which carbon nanotubes each having one end connected to the substrate can be formed at a high synthetic rate and from which the carbon nanotubes are less likely to be peeled off. The substrate is a substrate for forming the carbon nanotubes and includes a buffer layer 13 formed on at least one of surfaces of a substrate main body 14 and containing aluminum atoms and fluorine atoms. The carbon nanotube complex includes the substrate and a plurality of carbon nanotubes 11 each having one end connected to a surface of the buffer layer 13.
摘要:
Provided is a toner in which faulty transfer under an extremely-low-temperature, low-humidity environment hardly occurs, including toner particles and a zeolite as an external additive, in which a ratio of the alminium atoms to a total of the silicon atoms and the aluminium atoms contained in the zeolite is 0.2 to 24.0%.
摘要:
The present invention provides an energy device including a carbon nanotube electrode which prevents a carbon nanotube from peeling from an electric conductor. The energy device includes rolled electrode bodies, wherein at least one of the electrode bodies is formed such that a carbon nanotube layer is formed on the electric conductor, and concave regions are formed in a stripe shape on the carbon nanotube layer so as to extend in a direction parallel to a roll axis.
摘要:
In order to print a marked-up region in a color appropriate for printing, a MFP includes a communicating portion to which print data is input, a marked-up region extract portion for extracting a marked-up region from the print data, a marked-up region converter for converting a color of the extracted marked-up region to a conversion color appropriate for printing, and a printer for printing the marked-up region extracted from the print data in the conversion color.
摘要:
A toner is provided which is excellent in development stability in both a low-temperature, low-humidity environment and a high-temperature, high-humidity environment over a long time period. The toner includes toner particles containing at least a binder resin and a colorant, and a fatty acid metal salt. The fatty acid metal salt has a volume-based median diameter (D50s) of 0.15 μm or more and 0.65 μm or less, and the liberation ratio of the fatty acid metal salt in the toner is 1.0% or more and 25.0% or less.
摘要:
The present invention provides an energy device including a carbon nanotube electrode which prevents a carbon nanotube from peeling from an electric conductor. The energy device includes rolled electrode bodies, wherein at least one of the electrode bodies is formed such that a carbon nanotube layer is formed on the electric conductor, and concave regions are formed in a stripe shape on the carbon nanotube layer so as to extend in a direction parallel to a roll axis.
摘要:
The present invention provides a nanostructure on an upper surface of which a small-diameter carbon nanotube (CNT) is formed and which improves an adhesive strength between a substrate and the CNT while controlling an orientation of the CNT, and a method for manufacturing the nanostructure. The nanostructure includes a substrate 101, a porous layer 102 formed on the substrate 101 to have a fine pore, a fine pore diameter control layer 103 formed on the porous layer 102, and a carbon nanotube 701 formed to extend from the fine pore defined by the fine pore diameter control layer 103, and one end of the carbon nanotube is fixed by the fine pore diameter control layer 103. It is preferable that the substrate 101 and the fine pore diameter control layer 103 be electrically conductive. It is preferable that the porous layer 102 be an anode oxide film. It is preferable that a melting point of the fine pore diameter control layer 103 be 600° C. or higher.