公开(公告)号:US12098271B2
公开(公告)日:2024-09-24
申请号:US17117846
申请日:2020-12-10
Applicant: Samsung Display Co., Ltd.
Inventor: Tetsuya Fujiwara , Hideo Umeda , Katsuhiro Yamamoto , Keisuke Morita
IPC: C08L33/08 , C08F220/18 , C08F220/20 , C08G83/00 , C09J7/30
CPC classification number: C08L33/08 , C08F220/1811 , C08F220/20 , C08G83/007 , C09J7/30 , C08L2205/02 , C08L2205/03 , C09J2203/318 , C09J2203/326 , C09J2301/416 , C09J2433/00
Abstract: A resin composition includes a first (meth)acrylic resin having a weight average molecular weight of about 500 or less, a second (meth)acrylic resin having a weight average molecular weight of about 6,000 or more, a radical polymerization initiator, and a polyrotaxane compound, where the resin composition has a viscosity in a range of about 1.0 mPa·s to about 100 mPa·s at 25° C.
-
公开(公告)号:US12168739B2
公开(公告)日:2024-12-17
申请号:US17813924
申请日:2022-07-20
Applicant: SAMSUNG DISPLAY CO., LTD.
Inventor: Tetsuya Fujiwara
IPC: G02B1/14 , C09J7/22 , C09J133/10 , C09J175/04 , G06F1/16
Abstract: A method of manufacturing an adhesive member includes providing, for a substrate, a resin composition having a viscosity of about 5 cP to about 50 cP, as measured according to JISK2283 method, at about 25° C. The resin composition is exposed to a first light to form a preliminary adhesive member having a curing rate of about 80% to about 98%. The preliminary adhesive member is exposed to a second light having a light integral/dose that is more than that of the first light to form an adhesive member. The preliminary adhesive member may have a loss tangent (tan δ) of about 0.2 to about 0.6 and may have a glass transition temperature of about −70° C. to −30° C. Accordingly, the preliminary adhesive member and adhesive member formed by the method of manufacturing an adhesive member may exhibit increased reliability.
-
公开(公告)号:US11898066B2
公开(公告)日:2024-02-13
申请号:US17859494
申请日:2022-07-07
Applicant: Samsung Display Co., Ltd.
Inventor: Tetsuya Fujiwara
IPC: C09D175/06 , C09J7/38 , C09J175/06
CPC classification number: C09J175/06 , C09J7/385 , C09J2203/318
Abstract: An adhesive member includes a polymer derived from a resin composition. The resin composition includes at least one (meth)acrylate monomer, at least one urethane (meth)acrylate oligomer, and at least one photoinitiator. The adhesive member has a glass transition temperature in a range of about −70° C. to about −30° C., a 180° peel force of about 800 gf/25 mm or greater at a temperature of 25° C., and a deformation recovery rate in a range of about 75% to about 100% at temperatures of −20° C. and 60° C. The deformation recovery rate satisfies the following equation: X2=[1−(X1/25)]×100%, where X1 denotes a shear strain measured 600 seconds after removing a shear stress applied in a way such that the adhesive member has a shear strain of 25% at the temperatures of −20° C. and 60° C., and X2 denotes the deformation recovery rate.
-
公开(公告)号:US12084598B2
公开(公告)日:2024-09-10
申请号:US17381107
申请日:2021-07-20
Applicant: Samsung Display Co., Ltd.
Inventor: Tetsuya Fujiwara
CPC classification number: C09J4/06 , B32B7/12 , B32B17/10 , B32B27/06 , C09J133/066 , G06F3/0412 , G09F9/301 , B32B2457/20 , C09J4/06 , C08F290/067
Abstract: A resin composition including at least one of a monofunctional (meth)acrylate having an imide ring structure or a monomer having a 2-pyrrolidone skeleton and a radical curable group in an amount of about 0.1 weight percent to about 5 weight percent based on the total weight of the resin composition, wherein the resin composition has a viscosity of about 5 millipascal seconds to less than about 50 millipascal seconds at 25° C., and wherein a glass transition temperature of the resin composition after being cured satisfies a value of about −50° C. to less than about 0°C.
-
公开(公告)号:US12071500B2
公开(公告)日:2024-08-27
申请号:US17383772
申请日:2021-07-23
Applicant: Samsung Display Co., Ltd.
Inventor: Tetsuya Fujiwara
IPC: C08F255/10 , C08F2/50 , C09J4/06 , G02F1/1333
CPC classification number: C08F255/10 , C08F2/50 , C09J4/06 , G02F1/133311 , C09K2323/05 , C09K2323/057 , C09K2323/059 , G02F2202/28 , C08F290/067 , C08F220/20 , C08F220/1811 , C08F220/36 , C08F279/02 , C08F220/20 , C08F220/1811 , C08F220/36
Abstract: A resin composition may include a (meth)acrylate (A) comprising a hydroxy group and having a molecular weight of about 500 or less, and a polymer (B) comprising polyisoprene or polybutadiene as a main skeleton, having at least one radical reactive group in one molecule, and having a molecular weight in a range of about 2,000 to about 35,000, wherein the resin composition has a glass transition temperature in a range of about −50° C. to about 0° C. after the resin composition is cured, and the resin composition has a viscosity in a range of about 5 mPa·s to about 50 mPa·s at a temperature in a range of about 30° C. to about 50° C.
-
公开(公告)号:US20230159801A1
公开(公告)日:2023-05-25
申请号:US17813924
申请日:2022-07-20
Applicant: Samsung Display Co., Ltd.
Inventor: Tetsuya Fujiwara
IPC: C09J133/10 , C09J7/22 , C09J175/04 , G02B1/14
CPC classification number: C09J133/10 , C09J7/22 , C09J175/04 , G02B1/14 , C09J2203/326 , C09J2301/416 , C09J2301/408 , G06F1/1652
Abstract: A method of manufacturing an adhesive member includes providing, for a substrate, a resin composition having a viscosity of about 5 cP to about 50 cP, as measured according to JISK2283 method, at about 25° C. The resin composition is exposed to a first light to form a preliminary adhesive member having a curing rate of about 80% to about 98%. The preliminary adhesive member is exposed to a second light having a light integral/dose that is more than that of the first light to form an adhesive member. The preliminary adhesive member may have a loss tangent (tan δ) of about 0.2 to about 0.6 and may have a glass transition temperature of about −70° C. to −30° C. Accordingly, the preliminary adhesive member and adhesive member formed by the method of manufacturing an adhesive member may exhibit increased reliability.
-
-
-
-
-