OPTICAL FUNCTIONAL FILM, AND METHOD FOR MANUFACTURING LIQUID CRYSTAL DISPLAY DEVICE USING SAME
    1.
    发明申请
    OPTICAL FUNCTIONAL FILM, AND METHOD FOR MANUFACTURING LIQUID CRYSTAL DISPLAY DEVICE USING SAME 有权
    光学功能膜,以及使用其制造液晶显示装置的方法

    公开(公告)号:US20130126080A1

    公开(公告)日:2013-05-23

    申请号:US13813286

    申请日:2011-08-23

    IPC分类号: B32B7/06 B32B38/00

    摘要: Provided is an optical functional film in which air bubbles can be effectively prevented from forming during lamination, and preferably in which a carrier film does not tear readily. Also provided is a method for manufacturing a liquid crystal display device using this optical functional film. A belt-shaped optical functional film is used in order to cut away the optical functional film at predetermined intervals from the belt-shaped optical functional film to which a carrier film is bonded, with the carrier film remaining uncut; to subsequently turn over the carrier film by an edge-shaped member and peel away the optical functional film; and to laminate the exposed surface of the optical functional film to a sheet member while the optical functional film is being peeled away, wherein the optical functional film is characterized in that the flexural rigidity of the carrier film per unit length in the longitudinal direction is from 5.0×10−5 N·mm2 to 8.0×10−2 N·mm2, and the longitudinal modulus in the longitudinal direction is from 3000 MPa to 5000 MPa.

    摘要翻译: 提供了一种光学功能膜,其中可以有效地防止在层压期间形成气泡,并且优选其中载体膜不易撕裂。 还提供了使用该光学功能膜的液晶显示装置的制造方法。 使用带状光学功能膜,以便以预定间隔从与载体膜接合的带状光学功能膜切除光学功能膜,载体膜保持未切割; 随后通过边缘形构件翻转载体膜并剥离光学功能膜; 并且在光学功能膜被剥离的同时将光学功能膜的暴露表面层压到片状构件上,其中光学功能膜的特征在于,纵向方向上每单位长度的载体膜的抗弯刚度来自 5.0×10-5N·mm2〜8.0×10-2N·mm2,纵向的纵向模量为3000〜5000MPa。

    Optical functional film, and method for manufacturing liquid crystal display device using same
    2.
    发明授权
    Optical functional film, and method for manufacturing liquid crystal display device using same 有权
    光功能膜及使用该液晶显示装置的液晶显示装置的制造方法

    公开(公告)号:US08936692B2

    公开(公告)日:2015-01-20

    申请号:US13813286

    申请日:2011-08-23

    摘要: Provided is an optical functional film in which air bubbles can be effectively prevented from forming during lamination, and preferably in which a carrier film does not tear readily. Also provided is a method for manufacturing a liquid crystal display device using this optical functional film. A belt-shaped optical functional film is used in order to cut away the optical functional film at predetermined intervals from the belt-shaped optical functional film to which a carrier film is bonded, with the carrier film remaining uncut; to subsequently turn over the carrier film by an edge-shaped member and peel away the optical functional film; and to laminate the exposed surface of the optical functional film to a sheet member while the optical functional film is being peeled away, wherein the optical functional film is characterized in that the flexural rigidity of the carrier film per unit length in the longitudinal direction is from 5.0×10−5 N·mm2 to 8.0×10−2 N·mm2, and the longitudinal modulus in the longitudinal direction is from 3000 MPa to 5000 MPa.

    摘要翻译: 提供了一种光学功能膜,其中可以有效地防止在层压期间形成气泡,并且优选其中载体膜不易撕裂。 还提供了使用该光学功能膜的液晶显示装置的制造方法。 使用带状光学功能膜,以便以预定间隔从与载体膜接合的带状光学功能膜切除光学功能膜,载体膜保持未切割; 随后通过边缘形构件翻转载体膜并剥离光学功能膜; 并且在光学功能膜被剥离的同时将光学功能膜的暴露表面层压到片状构件上,其中光学功能膜的特征在于,纵向方向上每单位长度的载体膜的抗弯刚度来自 5.0×10-5N·mm2〜8.0×10-2N·mm2,纵向的纵向模量为3000〜5000MPa。

    Method for continuously manufacturing liquid crystal display panel and inspection method
    3.
    发明授权
    Method for continuously manufacturing liquid crystal display panel and inspection method 有权
    连续制造液晶显示面板的方法及检验方法

    公开(公告)号:US08540543B2

    公开(公告)日:2013-09-24

    申请号:US13242795

    申请日:2011-09-23

    IPC分类号: H01J9/24

    CPC分类号: G02F1/1309

    摘要: The invention is a method for continuously manufacturing a liquid crystal display panel. In the method, the manufacturing step and the inspection step are performed on a continuous feeder. The inspection step includes applying a line-shaped light beam from one side with respect to the feeder to the liquid crystal display panel being fed; and imaging a region irradiated with the line-shaped light beam in the liquid crystal display panel, wherein the imaging is continuously performed in a line pattern parallel to a width direction of the feeder and performed at a position that is on another side with respect to the feeder and tilted at a predetermined angle to a feed direction of the feeder or a direction opposite thereto with respect to a direction in which the line-shaped light beam is applied.

    摘要翻译: 本发明是连续制造液晶显示面板的方法。 在该方法中,制造步骤和检查步骤在连续进料器上进行。 所述检查步骤包括将相对于所述供给器的一侧的线状光束施加到被馈送的液晶显示面板; 并对在液晶显示面板中的线状光束照射的区域进行成像,其中以与馈送器的宽度方向平行的线图案连续进行成像,并且在相对于 进给器,并且相对于施加线状光束的方向以与给料器的进给方向或与其相反的方向倾斜预定角度。

    METHOD FOR CONTINUOUSLY MANUFACTURING LIQUID CRYSTAL DISPLAY PANEL AND INSPECTION METHOD
    4.
    发明申请
    METHOD FOR CONTINUOUSLY MANUFACTURING LIQUID CRYSTAL DISPLAY PANEL AND INSPECTION METHOD 有权
    连续制造液晶显示面板和检查方法的方法

    公开(公告)号:US20120238176A1

    公开(公告)日:2012-09-20

    申请号:US13242795

    申请日:2011-09-23

    IPC分类号: H01J9/24

    CPC分类号: G02F1/1309

    摘要: The invention is a method for continuously manufacturing a liquid crystal display panel. In the method, the manufacturing step and the inspection step are performed on a continuous feeder. The inspection step includes applying a line-shaped light beam from one side with respect to the feeder to the liquid crystal display panel being fed; and imaging a region irradiated with the line-shaped light beam in the liquid crystal display panel, wherein the imaging is continuously performed in a line pattern parallel to a width direction of the feeder and performed at a position that is on another side with respect to the feeder and tilted at a predetermined angle to a feed direction of the feeder or a direction opposite thereto with respect to a direction in which the line-shaped light beam is applied.

    摘要翻译: 本发明是连续制造液晶显示面板的方法。 在该方法中,制造步骤和检查步骤在连续进料器上进行。 所述检查步骤包括将相对于所述供给器的一侧的线状光束施加到被馈送的液晶显示面板; 并对在液晶显示面板中的线状光束照射的区域进行成像,其中以与馈送器的宽度方向平行的线图案连续进行成像,并且在相对于 进给器,并且相对于施加线状光束的方向以与给料器的进给方向或与其相反的方向倾斜预定角度。

    MATERIAL ROLL AND SYSTEM AND METHOD FOR MANUFACTURING OPTICAL DISPLAY DEVICE
    7.
    发明申请
    MATERIAL ROLL AND SYSTEM AND METHOD FOR MANUFACTURING OPTICAL DISPLAY DEVICE 有权
    用于制造光学显示装置的材料辊和系统和方法

    公开(公告)号:US20120031552A1

    公开(公告)日:2012-02-09

    申请号:US13028770

    申请日:2011-02-16

    IPC分类号: B32B7/06 B32B38/04 C09J7/02

    摘要: Provided are a system and a method for manufacturing an optical display device and a material roll, which can effectively prevent the production of defective optical display devices even in a process including drawing a long sheet material from a material roll and bonding an optical film to an optical display unit, and which is a roll of a laminate of a first base film, a first pressure-sensitive adhesive layer, an optical film, a second pressure-sensitive adhesive layer, and a second base film, which are wound in the roll in this order from the outside, and has a width corresponding to the length of any one side of a rectangular optical display unit, wherein the adhering strength A of the first base film-side interface of the first pressure-sensitive adhesive layer, the adhering strength B of the optical film-side interface of the first pressure-sensitive adhesive layer, the adhering strength C of the optical film-side interface of the second pressure-sensitive adhesive layer, and the adhering strength D of the second base film-side interface of the second pressure-sensitive adhesive layer satisfy the relations A

    摘要翻译: 提供一种用于制造光学显示装置和材料辊的系统和方法,其可以有效地防止有缺陷的光学显示装置的生产,即使在包括从材料辊拉长长片材并将光学膜粘合到 光学显示单元,并且是卷绕在辊中的第一基膜,第一粘合剂层,光学膜,第二压敏粘合剂层和第二基膜的层压体卷 并且具有对应于矩形光学显示单元的任一侧的长度的宽度,其中第一粘合剂层的第一基膜侧界面的粘附强度A,粘附 第一粘合剂层的光学膜侧界面的强度B,第二压敏粘合剂层的光学膜侧界面的粘合强度C和 第二粘合剂层的第二基膜侧界面的粘合强度D满足A

    System and method for bonding optical film to a liquid crystal display panel
    9.
    发明授权
    System and method for bonding optical film to a liquid crystal display panel 有权
    用于将光学膜粘合到液晶显示面板的系统和方法

    公开(公告)号:US08172631B2

    公开(公告)日:2012-05-08

    申请号:US13021294

    申请日:2011-02-04

    IPC分类号: H01J9/00 B32B41/00

    摘要: There are provided a system and a method for manufacturing a liquid crystal display element, which make it possible to perform a lamination process in a smaller installation space, and which are provided to perform a process including turning over and horizontally rotating a liquid crystal panel using a panel turning unit, feeding optical functional films from first and second continuous rolls, respectively, using film feeding lines arranged linearly in planar view, feeding the liquid crystal panel using a panel feeding line placed above the film feeding lines in an overlapping manner and shaped linearly in planar view, and bonding each of the optical functional films, which are fed from the first and second rolls, to the liquid crystal panel from below.

    摘要翻译: 提供了一种用于制造液晶显示元件的系统和方法,其使得可以在较小的安装空间中进行层压处理,并且其被设置用于执行包括使用以下方式翻转和水平旋转液晶面板的处理 面板转向单元,分别使用在平面图中线性布置的供电线从第一连续辊和第二连续辊供给光学功能膜,以重叠的方式使用放置在胶片供给线上方的面板供给线供给液晶面板并成形 将从第一和第二辊供给的每个光学功能膜从下方接合到液晶面板,