Abstract:
The present invention aims to provide an electronic device housing that is able to maintain the antenna performance without deteriorating the radio communication performance, excellent in terms of the degree of warpage and dimensional accuracy, and mass productivity. The electronic device housing includes a fiber reinforcing member (a) and a fiber reinforcing member (b), wherein the fiber reinforcing member (a) contains a resin (a1) and a fiber (a2), the fiber (a2) being in the form of discontinuous fibers; the fiber reinforcing member (b) contains a resin (b1) and a fiber (b2), the fiber (b2) being in the form of continuous fibers; the projected area of the fiber reinforcing member (a) accounts for 60% or more of the total projected area, which accounts for 100%, of the housing projected onto the plane of the top face; and requirements (i) and/or (ii) given below are met: (i) the resin (a1) is a thermoplastic resin having a melting point of more than 265° C., and (ii) the resin (a1) is a thermoplastic resin having a water absorption rate of 0.4% or less.
Abstract:
The invention aims to provide an electronic device housing that can maintain the antenna performance without deteriorating the radio communication performance, ensures uniform characteristics as one molded electronic device housing in spite of consisting of a plurality of members, and show excellent features in terms of the degree of warpage and dimensional accuracy as well as small deformation in high temperature environments and high mass productivity. The electronic device housing consists mainly of a fiber reinforcing member (a) and a fiber reinforcing member (b), the fiber reinforcing member (a) containing a resin (a1) and a fiber (a2), the fiber reinforcing member (b) containing a resin (b1) and a fiber (b2), the fiber reinforcing member (a) and the fiber reinforcing member (b) being joined directly without the existence of another layer at the joining face between the fiber reinforcing member (a) and the fiber reinforcing member (b), and the fiber reinforcing member (a) and the fiber reinforcing member (b) fulfilling a specific relation in terms of linear expansion coefficient and/or bending elastic modulus.
Abstract:
The present invention is a method for producing a liquid crystalline polyester, which comprises reacting an aromatic hydroxycarboxylic acid, a diol containing 70 mol % or more of an aromatic diol having a structural unit (I) as shown below and an aromatic dicarboxylic acid with one another in the presence of an acylating agent and an aliphatic sulfonic acid represented by formula (A) shown below. (wherein Ar represents a bivalent aromatic group which is an aromatic hydrocarbon group and has a molecular weight of less than 200) Formula (A) R—SO3H (wherein R represents an alkyl group having 1 to 12 carbon atoms) According to the present invention, a liquid crystalline polyester, which can be molded into an article having excellent tensile strength and excellent creep properties and from which a gas is generated in a reduced amount, can be produced with high efficiency.