Abstract:
A method of producing polybutylene terephthalate resin shaped moldings includes supplying a 3D printer with a polybutylene terephthalate resin powder mixture that contains 100 parts by weight of a polybutylene terephthalate resin powder material having a mean diameter of more than 1 μm and 100 μm or less, a uniformity coefficient of 4 or less, and a terminal carboxyl group quantity of 35 eq/t or more and 50 eq/t or less, and 0.1 to 5 parts by weight of inorganic particles having a mean diameter of 20 to 500 nm.
Abstract:
A method of producing polybutylene terephthalate resin shaped moldings includes supplying a 3D printer with a polybutylene terephthalate resin powder mixture that contains 100 parts by weight of a polybutylene terephthalate resin powder material having a mean diameter of more than 1 μm and 100 μm or less, a uniformity coefficient of 4 or less, and a terminal carboxyl group quantity of 35 eq/t or more and 50 eq/t or less, and 0.1 to 5 parts by weight of inorganic particles having a mean diameter of 20 to 500 nm.
Abstract:
A polyarylene sulfide resin powder/grain composition in which 100 weight parts of polyarylene sulfide resin powder/grain material whose average particle diameter exceeds 1 μm and is less than or equal to 100 μm and whose uniformity degree is less than or equal to 4 has been blended with 0.1 to 5 weight parts of an inorganic fine particle having an average particle diameter greater than or equal to 20 nm and less than or equal to 500 nm.
Abstract:
A production method includes a process (I) of heating a cyclic polyarylene sulfide composition under reduced pressure and a process (II) of heating and polymerizing a cyclic polyarylene sulfide composition. This simple method allows for production of a polyarylene sulfide of the higher molecular weight and can produce a polyarylene sulfide having a narrow molecular weight distribution, low gas generation and high industrial usability. Additionally, pelletization after the process (I) can produce a cyclic polyarylene sulfide pellet having ease of conveyance, excellent molding processability, less gas generation amount and high industrial usability.
Abstract:
A production method includes a process (I) of heating a cyclic polyarylene sulfide composition under reduced pressure and a process (II) of heating and polymerizing a cyclic polyarylene sulfide composition. This simple method allows for production of a polyarylene sulfide of the higher molecular weight and can produce a polyarylene sulfide having a narrow molecular weight distribution, low gas generation and high industrial usability. Additionally, pelletization after the process (I) can produce a cyclic polyarylene sulfide pellet having ease of conveyance, excellent molding processability, less gas generation amount and high industrial usability.
Abstract:
A polyester resin powder mixture has a small average particle size, excellent powder flowability, and high strength after molding. The polyester resin powder mixture is obtained by blending 0.1-5 parts by weight of silica microparticles having an average particle size of 20-500 nm in 100 parts by weight of a polyester resin powder having an average particle size that is over 1 μm and is less than or equal to 100 μm, and that has a uniformity of 4 or less.
Abstract:
A polyarylene sulfide resin powder/grain composition in which 100 weight parts of polyarylene sulfide resin powder/grain material whose average particle diameter exceeds 1 μm and is less than or equal to 100 μm and whose uniformity degree is less than or equal to 4 has been blended with 0.1 to 5 weight parts of an inorganic fine particle having an average particle diameter greater than or equal to 20 nm and less than or equal to 500 nm.