Abstract:
A polymer powder includes a polyamide, wherein a melting point determined in differential scanning calorimetry is 190° C. or higher, a difference between the melting point and a melting onset temperature, which is defined in differential scanning calorimetry as a lowest temperature among temperatures at each of which a first temperature differential value of Heat Flow (W/g) observed between a peak top temperature of an endothermic peak, observed when 10 mg of powder is heated at a rate of 20° C./min from 30° C. in a nitrogen atmosphere, and a temperature point of −50° C. from the peak top, becomes −0.2 (W/g.° C.), is less than 30° C., and a D50 particle size is 1 μm or more and 100 μm or less.
Abstract:
A polyarylene sulfide resin particulate has a mean particle diameter from more than 1 μm to 100 the uniformity is 4 or less, the melt viscosity measured at temperature of 300° C. and shear rate of 1216 sec−1 is 150 to 500 Pa·s, and the recrystallization temperature, defined as temperature of the heat generation peak at the time of crystallization when cooled from 340° C. to 50° C. at 20° C./min using a differential scanning calorimeter, is 150 to 210° C. The polyarylene sulfide resin particulate is suitable as a material powder for producing a three-dimensional molding by a powder sintering three-dimensional printer can be provided efficiently.
Abstract:
A polymer powder includes a polyamide, wherein a melting point determined in differential scanning calorimetry is 190° C. or higher, a difference between the melting point and a melting onset temperature, which is defined in differential scanning calorimetry as a lowest temperature among temperatures at each of which a first temperature differential value of Heat Flow (W/g) observed between a peak top temperature of an endothermic peak, observed when 10 mg of powder is heated at a rate of 20° C./min from 30° C. in a nitrogen atmosphere, and a temperature point of −50° C. from the peak top, becomes −0.2 (W/g.° C.), is less than 30° C., and a D50 particle size is 1 μm or more and 100 μm or less.
Abstract:
A polyester resin powder mixture has a small average particle size, excellent powder flowability, and high strength after molding. The polyester resin powder mixture is obtained by blending 0.1-5 parts by weight of silica microparticles having an average particle size of 20-500 nm in 100 parts by weight of a polyester resin powder having an average particle size that is over 1 μm and is less than or equal to 100 μm, and that has a uniformity of 4 or less.
Abstract:
A polyarylene sulfide resin powder/grain composition in which 100 weight parts of polyarylene sulfide resin powder/grain material whose average particle diameter exceeds 1 μm and is less than or equal to 100 μm and whose uniformity degree is less than or equal to 4 has been blended with 0.1 to 5 weight parts of an inorganic fine particle having an average particle diameter greater than or equal to 20 nm and less than or equal to 500 nm.
Abstract:
A polyarylene sulfide resin powder/grain composition in which 100 weight parts of polyarylene sulfide resin powder/grain material whose average particle diameter exceeds 1 μm and is less than or equal to 100 μm and whose uniformity degree is less than or equal to 4 has been blended with 0.1 to 5 weight parts of an inorganic fine particle having an average particle diameter greater than or equal to 20 nm and less than or equal to 500 nm.
Abstract:
A resin powder mixture which contains a polyarylene sulfide resin powder having a gas generation amount of 0.25 wt % or less, a melt flow rate of 5-75 g/10 min and an average particle diameter of 1-100 μm.
Abstract:
A method of producing polybutylene terephthalate resin shaped moldings includes supplying a 3D printer with a polybutylene terephthalate resin powder mixture that contains 100 parts by weight of a polybutylene terephthalate resin powder material having a mean diameter of more than 1 μm and 100 μm or less, a uniformity coefficient of 4 or less, and a terminal carboxyl group quantity of 35 eq/t or more and 50 eq/t or less, and 0.1 to 5 parts by weight of inorganic particles having a mean diameter of 20 to 500 nm.
Abstract:
A method of producing polybutylene terephthalate resin shaped moldings includes supplying a 3D printer with a polybutylene terephthalate resin powder mixture that contains 100 parts by weight of a polybutylene terephthalate resin powder material having a mean diameter of more than 1 μm and 100 μm or less, a uniformity coefficient of 4 or less, and a terminal carboxyl group quantity of 35 eq/t or more and 50 eq/t or less, and 0.1 to 5 parts by weight of inorganic particles having a mean diameter of 20 to 500 nm.
Abstract:
A polyarylene sulfide resin powder granular article mixture enabling production of a highly heat-resistant and high-ductility three-dimensional molded article has: 5-25 parts by weight of fluorine resin powder granular article with respect to 100 parts by weight of polyarylene sulfide resin powder granular article; an average particle size of greater than 1 μm to 100 μm or less; an angle of repose of 43 degrees or less; and a homogeneity of 4 or less.