Rubber composition for tire and pneumatic tire using the same
    2.
    发明申请
    Rubber composition for tire and pneumatic tire using the same 有权
    用于轮胎的橡胶组合物和使用其的充气轮胎

    公开(公告)号:US20070100061A1

    公开(公告)日:2007-05-03

    申请号:US11585197

    申请日:2006-10-24

    IPC分类号: C08K5/00

    摘要: A rubber composition for a tire, in which a specific tackifier is compounded, and tackiness and various physical properties are improved, compared with compounding a petroleum resin or a terpene resin, is provided. The rubber composition for a tire comprising an alkyd resin and a pneumatic tire using the same. It is preferable that a material derived from a resource other than petroleum, particularly, a material derived from animal and/or vegetable, and more particularly, a material derived from an animal oil and/or a vegetable oil is contained in the alkyd resin, and it is preferable that unsaturated polybasic acid is contained in the alkyd resin.

    摘要翻译: 与混合石油树脂或萜烯树脂相比,提供了一种轮胎的橡胶组合物,其中特定的增粘剂配混,粘合性和各种物理性能得到改善。 包含醇酸树脂的轮胎用橡胶组合物和使用其的充气轮胎。 优选在醇酸树脂中含有源自石油以外的资源的材料,特别是源自动物和/或植物的材料,更具体地,衍生自动物油和/或植物油的材料, 优选在醇酸树脂中含有不饱和多元酸。

    Preparation process of oil extended rubber for tire, oil extended rubber for tire, and rubber composition and tire using the same
    3.
    发明授权
    Preparation process of oil extended rubber for tire, oil extended rubber for tire, and rubber composition and tire using the same 有权
    用于轮胎的油延伸橡胶,轮胎用油延伸橡胶,橡胶组合物和使用其的轮胎的制备方法

    公开(公告)号:US08044118B2

    公开(公告)日:2011-10-25

    申请号:US11723680

    申请日:2007-03-21

    IPC分类号: C08C1/14 B60C1/00

    摘要: The present invention provides a process for preparing an oil extended rubber, in which an effect on environments can be taken into consideration, provision for the future decrease of petroleum supply can be satisfied, and further, strength is excellent without molecular breakage, an oil extended rubber obtained by the preparation process, and a tire using the oil extended rubber. A process for preparing an oil extended rubber, comprising (a) a step of preparing an oil-in-water type emulsion by emulsifying a vegetable oil having an iodine value of not less than 135 with a surfactant, (b) a step of mixing said emulsion and a modified natural rubber latex, and then aging the mixture, and (c) a step of coagulating the mixture obtained in the step (b) to obtain a lump of a rubber, an oil extended rubber obtained by the preparation process, and a rubber composition for a tire and a tire which use the oil extended rubber.

    摘要翻译: 本发明提供了一种制备延油橡胶的方法,其中可以考虑对环境的影响,可以满足将来石油供应减少的要求,而且在没有分子破裂的情况下,强度优异,油扩展 通过制备方法获得的橡胶,以及使用延油橡胶的轮胎。 一种制备延油橡胶的方法,包括(a)通过用表面活性剂乳化碘值不小于135的植物油来制备水包油型乳液的步骤,(b)混合步骤 所述乳液和改性天然橡胶胶乳,然后使所述混合物老化,和(c)使步骤(b)中获得的混合物凝固的步骤获得橡胶块,通过制备方法获得的延油橡胶, 以及使用该油延伸橡胶的轮胎和轮胎用橡胶组合物。

    Preparation process of oil extended rubber for tire, oil extended rubber for tire, and rubber composition and tire using the same
    5.
    发明申请
    Preparation process of oil extended rubber for tire, oil extended rubber for tire, and rubber composition and tire using the same 有权
    用于轮胎的油延伸橡胶,轮胎用油延伸橡胶,橡胶组合物和使用其的轮胎的制备方法

    公开(公告)号:US20070232745A1

    公开(公告)日:2007-10-04

    申请号:US11723680

    申请日:2007-03-21

    IPC分类号: B60C1/00

    摘要: The present invention provides a process for preparing an oil extended rubber, in which an effect on environments can be taken into consideration, provision for the future decrease of petroleum supply can be satisfied, and further, strength is excellent without molecular breakage, an oil extended rubber obtained by the preparation process, and a tire using the oil extended rubber. A process for preparing an oil extended rubber, comprising (a) a step of preparing an oil-in-water type emulsion by emulsifying a vegetable oil having an iodine value of not less than 135 with a surfactant, (b) a step of mixing said emulsion and a modified natural rubber latex, and then aging the mixture, and (c) a step of coagulating the mixture obtained in the step (b) to obtain a lump of a rubber, an oil extended rubber obtained by the preparation process, and a rubber composition for a tire and a tire which use the oil extended rubber.

    摘要翻译: 本发明提供了一种制备延油橡胶的方法,其中可以考虑对环境的影响,可以满足将来石油供应减少的要求,而且在没有分子破裂的情况下,强度优异,油扩展 通过制备方法获得的橡胶,以及使用延油橡胶的轮胎。 一种制备延油橡胶的方法,包括(a)通过用表面活性剂乳化碘值不小于135的植物油来制备水包油型乳液的步骤,(b)混合步骤 所述乳液和改性天然橡胶胶乳,然后使所述混合物老化,和(c)使步骤(b)中获得的混合物凝固的步骤获得橡胶块,通过制备方法获得的延油橡胶, 以及使用该油延伸橡胶的轮胎和轮胎用橡胶组合物。

    RUBBER COMPOSITION FOR BREAKER AND PNEUMATIC TIRE
    9.
    发明申请
    RUBBER COMPOSITION FOR BREAKER AND PNEUMATIC TIRE 有权
    用于断路器和气动轮胎的橡胶组合物

    公开(公告)号:US20110294949A1

    公开(公告)日:2011-12-01

    申请号:US13117182

    申请日:2011-05-27

    IPC分类号: C08L7/00 C08K3/36 C08K3/04

    摘要: The present invention provides a rubber composition for a breaker, which achieves both good fuel economy and good breaking performance while simultaneously having excellent processability, and a pneumatic tire including a breaker produced using the rubber composition. The present invention relates to a rubber composition for a breaker, including: a rubber component that contains a modified natural rubber, the rubber having a phosphorus content of 200 ppm or less; and carbon black and/or a white filler, wherein the rubber composition contains 5% by mass or more of the modified natural rubber based on 100% by mass of the rubber component.

    摘要翻译: 本发明提供了一种用于断路器的橡胶组合物,其具有良好的燃料经济性和良好的断裂性能,同时具有优异的加工性能,以及包括使用该橡​​胶组合物制备的断路器的充气轮胎。 本发明涉及一种用于破碎机的橡胶组合物,包括:含有改性天然橡胶的橡胶组分,该磷含量为200ppm以下的橡胶; 和炭黑和/或白色填料,其中,基于100质量%的橡胶组分,橡胶组合物含有5质量%以上的改性天然橡胶。

    Rubber composition for breaker and pneumatic tire
    10.
    发明授权
    Rubber composition for breaker and pneumatic tire 有权
    断路器和充气轮胎的橡胶组合物

    公开(公告)号:US08633275B2

    公开(公告)日:2014-01-21

    申请号:US13117182

    申请日:2011-05-27

    IPC分类号: C08L9/00

    摘要: The present invention provides a rubber composition for a breaker, which achieves both good fuel economy and good breaking performance while simultaneously having excellent processability, and a pneumatic tire including a breaker produced using the rubber composition. The present invention relates to a rubber composition for a breaker, including: a rubber component that contains a modified natural rubber, the rubber having a phosphorus content of 200 ppm or less; and carbon black and/or a white filler, wherein the rubber composition contains 5% by mass or more of the modified natural rubber based on 100% by mass of the rubber component.

    摘要翻译: 本发明提供了一种用于断路器的橡胶组合物,其具有良好的燃料经济性和良好的断裂性能,同时具有优异的加工性能,以及包括使用该橡​​胶组合物制备的断路器的充气轮胎。 本发明涉及一种用于破碎机的橡胶组合物,包括:含有改性天然橡胶的橡胶组分,该磷含量为200ppm以下的橡胶; 和炭黑和/或白色填料,其中,基于100质量%的橡胶组分,橡胶组合物含有5质量%以上的改性天然橡胶。