Zirconium oxide hydrate particles and method for producing the same
    4.
    发明授权
    Zirconium oxide hydrate particles and method for producing the same 失效
    氧化锆水合物颗粒及其制备方法

    公开(公告)号:US07829061B2

    公开(公告)日:2010-11-09

    申请号:US12167110

    申请日:2008-07-02

    IPC分类号: C01G25/02

    摘要: The zirconium oxide hydrate particles of the present invention are represented by the formula ZrO2.nH2O and have a mean primary particle size of 0.5 nm or more and 5 nm or less, and “n” in the formula represents a number greater than 2.5. Moreover, the method for producing of zirconium oxide hydrate particles of the present invention includes the step of preparing zirconium oxide hydrate particles by adding an aqueous zirconium salt solution to an aqueous alkaline solution while controlling the pH to 7.0 or more and 13.0 or less, and the step of subjecting the zirconium oxide hydrate particles to a hydrothermal treatment in the presence of water at a temperature of 50° C. or more and less than 110° C. for 3 hours or more.

    摘要翻译: 本发明的氧化锆水合物颗粒由式ZrO 2·nH 2 O表示,平均一次粒径为0.5nm以上且5nm以下,式中“n”表示大于2.5的数。 此外,本发明的氧化锆水合物颗粒的制造方法包括通过向碱性水溶液中添加锆盐水溶液,同时将pH控制在7.0以上且13.0以下,制备氧化锆水合物颗粒的工序,以及 在水存在下,在50℃以上且小于110℃的温度下对氧化锆水合物颗粒进行水热处理3小时以上的步骤。

    ZIRCONIUM OXIDE HYDRATE PARTICLES AND METHOD FOR PRODUCING THE SAME
    5.
    发明申请
    ZIRCONIUM OXIDE HYDRATE PARTICLES AND METHOD FOR PRODUCING THE SAME 失效
    氧化锆水合物颗粒及其生产方法

    公开(公告)号:US20090011239A1

    公开(公告)日:2009-01-08

    申请号:US12167110

    申请日:2008-07-02

    IPC分类号: C01G25/02 B32B5/16

    摘要: The zirconium oxide hydrate particles of the present invention are represented by the formula ZrO2.nH2O and have a mean primary particle size of 0.5 nm or more and 5 nm or less, and “n” in the formula represents a number greater than 2.5. Moreover, the method for producing of zirconium oxide hydrate particles of the present invention includes the step of preparing zirconium oxide hydrate particles by adding an aqueous zirconium salt solution to an aqueous alkaline solution while controlling the pH to 7.0 or more and 13.0 or less, and the step of subjecting the zirconium oxide hydrate particles to a hydrothermal treatment in the presence of water at a temperature of 50° C. or more and less than 110° C. for 3 hours or more.

    摘要翻译: 本发明的氧化锆水合物颗粒由式ZrO 2·nH 2 O表示,平均一次粒径为0.5nm以上且5nm以下,式中“n”表示大于2.5的数。 此外,本发明的氧化锆水合物颗粒的制造方法包括通过向碱性水溶液中添加锆盐水溶液,同时将pH控制在7.0以上且13.0以下,制备氧化锆水合物颗粒的工序,以及 在水存在下,在50℃以上且小于110℃的温度下对氧化锆水合物颗粒进行水热处理3小时以上的步骤。

    FUEL CELL ELECTROLYTE MEMBRANE, MEMBRANE ELECTRODE ASSEMBLY, AND FUEL CELL
    9.
    发明申请
    FUEL CELL ELECTROLYTE MEMBRANE, MEMBRANE ELECTRODE ASSEMBLY, AND FUEL CELL 审中-公开
    燃料电池膜,膜电极组件和燃料电池

    公开(公告)号:US20100266926A1

    公开(公告)日:2010-10-21

    申请号:US12063687

    申请日:2007-10-01

    IPC分类号: H01M8/10

    摘要: A proton-conductive composite electrolyte membrane, for a fuel cell, comprises a metal-oxide hydrate with proton conductivity and organic macromolecules in which an intermediate layer is formed between the metal-oxide hydrate and the first organic macromolecular electrolyte. The intermediate layer can enhance the adhesion at an interface between the metal-oxide hydrate and the organic macromolecule, and thereby the amount of methanol that penetrates along the interface can be reduced. Accordingly, the composite electrolyte membrane has both high proton conductivity and low methanol permeability, and a membrane electrode assembly that comprises the composite electrolyte membrane can produce a high output.

    摘要翻译: 用于燃料电池的质子传导复合电解质膜包括具有质子传导性的金属氧化物水合物和在金属氧化物水合物和第一有机高分子电解质之间形成中间层的有机大分子。 中间层可以提高金属氧化物水合物和有机高分子之间的界面处的粘附性,从而可以减少沿着界面渗透的甲醇的量。 因此,复合电解质膜具有高质子传导性和低甲醇渗透性,并且包含复合电解质膜的膜电极组件可以产生高输出。

    Fuel cell and membrane electrode assembly
    10.
    发明申请
    Fuel cell and membrane electrode assembly 审中-公开
    燃料电池和膜电极组件

    公开(公告)号:US20050214631A1

    公开(公告)日:2005-09-29

    申请号:US11063990

    申请日:2005-02-24

    摘要: A fuel cell anode for oxidizing fuel, a cathode for reducing oxygen and a solid polymer electrolyte membrane sandwiched between the anode and the cathode, wherein the cathode comprises a catalyst supporter having a catalyst metal and a material having a polymer proton conductivity and a material having water-repellency, the material having water-repellency being electric conductive. The material having water-repellency is a carbonaceous material such as graphite intercalation compound, activated charcoal, carbonaceous material having water-repellent function groups. The disclosure is also related to a membrane electrode assembly comprising an anode catalyst layer, a proton conductive polymer electrolyte membrane and a cathode catalyst layer, the anode catalyst layer, the membrane and the cathode catalyst layer being laminated and united, wherein the catalyst layers contain carbon supporting metal catalyst and a water-repellent material, the water-repellent material being electrically conductive.