摘要:
A cold-rolled steel sheet includes, on a percent by mass basis: C: 0.0010% to 0.0030%, Si: 0.05% or less, Mn: 0.1% to 0.3%, P: 0.05% or less, S: 0.02% or less, Al: 0.02% to 0.10%, N: 0.005% or less, and Nb: 0.010% to 0.030% and the remainder composed of Fe and incidental impurities, wherein values in a rolling direction and a direction perpendicular to the rolling direction are within a range of 1.0 to 1.6, and a mean value Elm of elongations in the rolling direction, a direction at 45° with respect to the rolling direction, and the direction perpendicular to the rolling direction is 40% or more, where Elm=(ElL+2×ElD+ElC)/4 and ElL: elongation in the rolling direction, ElD: elongation in the direction at 45° with respect to the rolling direction, and ElC: elongation in the direction perpendicular to the rolling direction.
摘要:
A cold-rolled steel sheet includes, on a percent by mass basis: C: 0.0010% to 0.0030%, Si: 0.05% or less, Mn: 0.1% to 0.3%, P: 0.05% or less, S: 0.02% or less, Al: 0.02% to 0.10%, N: 0.005% or less, and Nb: 0.010% to 0.030% and the remainder composed of Fe and incidental impurities, wherein r values in a rolling direction and a direction perpendicular to the rolling direction are within a range of 1.0 to 1.6, and a mean value Elm of elongations in the rolling direction, a direction at 45° with respect to the rolling direction, and the direction perpendicular to the rolling direction is 40% or more, where Elm=(ElL+2×ElD+ElC)/4 ElL: elongation in the rolling direction, ElD: elongation in the direction at 45° with respect to the rolling direction, and ElC: elongation in the direction perpendicular to the rolling direction.
摘要:
A zinc-electroplated steel sheet comprises a steel sheet; a tin layer which is formed on the steel sheet, the tin layer having a deposition amount of 0.5 mg/m.sup.2 to less than 10 mg/m.sup.2 ; and a zinc-electroplating layer which is formed on the tin layer.A method for producing a zinc-electroplated steel sheet comprising the steps of: pickling a steel sheet with a pickling solution so as to deposit a tin of an amount of 0.5 mg/m.sup.2 to less than 10 mg/m.sup.2 on the steel sheet; and zinc-electroplating the pickled steel sheet.
摘要翻译:锌电镀钢板包括钢板; 形成在钢板上的锡层,锡层的沉积量为0.5mg / m 2至小于10mg / m 2; 以及形成在锡层上的锌电镀层。 一种锌电镀钢板的制造方法,其特征在于,包括以下步骤:在所述钢板上沉积含有0.5mg / m 2至小于10mg / m 2的锡的酸洗液, 和锌电镀酸洗钢板。
摘要:
A management system of CAD data is provided, which stores sets of the CAD data, and a set of mesh conditions under which a CAE model is created from each of the sets of the CAD data and a set of analysis conditions under which CAE analysis on the created CAE model is performed associated with each set of the CAD data. Moreover, the management system of CAD data, to perform the CAE analysis on one of the sets of the CAD data, reads from the storage unit the set of the CAD data, and the set of the mesh conditions and the set of the analysis conditions associated with the set of the CAD data, creates the CAE model from the set of the CAD data under the read set of the mesh conditions, and perform the CAE analysis on the created CAE model under the read set of the analysis conditions.
摘要:
A management system of CAD data is provided, which stores sets of the CAD data, and a set of mesh conditions under which a CAE model is created from each of the sets of the CAD data and a set of analysis conditions under which CAE analysis on the created CAE model is performed associated with each set of the CAD data. Moreover, the management system of CAD data, to perform the CAE analysis on one of the sets of the CAD data, reads from the storage unit the set of the CAD data, and the set of the mesh conditions and the set of the analysis conditions associated with the set of the CAD data, creates the CAE model from the set of the CAD data under the read set of the mesh conditions, and perform the CAE analysis on the created CAE model under the read set of the analysis conditions.
摘要:
A method for producing a zinc-electroplated steel sheet comprising the steps of: pickling a steel sheet with a pickling solution so as to deposit a tin of an amount of 0.5 mg/m.sup.2 to less than 10 mg/m.sup.2 on the steel sheet; and zinc-electroplating the pickled steel sheet.
摘要翻译:一种锌电镀钢板的制造方法,其特征在于,包括以下步骤:在所述钢板上沉积含有0.5mg / m 2至小于10mg / m 2的锡的酸洗液, 和锌电镀酸洗钢板。